This datasheet includes:

  VESTODUR® X9400 nc (nf) | PBT-GF10 | Evonik Industries AG
Product Texts
VESTODUR® X9400 nc


Resin: ISO 7792-PBT,MHR, A12-04, GF10

 

VESTODUR® X9400 is a 10 % glass fiber reinforced, polymer-modified polybutylene terephthalate compound.

Moldings of this compound show decreased shrinkage. The compound is suitable for parts that are subjected

to high mechanical or thermal loads. Compared with commonly used glass fiber reinforced PBT compounds

with a similar stiffness parts of VESTODUR® X9400 have in particular a high surface quality.

Rheological propertiesValueUnitTest Standard
Molding shrinkage (parallel) 0.3 % ISO 294-4, 2577
Molding shrinkage (normal) 0.4 % ISO 294-4, 2577
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 4500 MPa ISO 527-1/-2
Yield stress 90 MPa ISO 527-1/-2
Yield strain 4 % ISO 527-1/-2
Nominal strain at break 5.5 % ISO 527-1/-2
Charpy impact strength (+23°C) 45 kJ/m² ISO 179/1eU
Charpy impact strength (-30°C) 45 kJ/m² ISO 179/1eU
Charpy notched impact strength (+23°C) 5 kJ/m² ISO 179/1eA
Charpy notched impact strength (-30°C) 5 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
Temp. of deflection under load (1.80 MPa) 110 °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 200 °C ISO 75-1/-2
Coeff. of linear therm. expansion (parallel) 30 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion (normal) 40 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.6 mm IEC 60695-11-10
Other propertiesValueUnitTest Standard
Density 1350 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Processing conditions acc. ISO 7790 - ISO ....-2
Injection Molding, melt temperature 260 °C ISO 294
Injection Molding, mold temperature 80 °C ISO 10724
Injection Molding, injection velocity 200 mm/s ISO 294
Injection Molding, pressure at hold 70 MPa ISO 294
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding

PREPROCESSING INFORMATION
Maximum Water Content: 0.05 %
When the indicated water content is exceeded, the resin must be dried. The drying time is dependent

on the drying temperature. We recommend a drying time of approximately 5 hours at a temperature of

120°C in a fresh air dryer, better yet would be a dry air or vacuum dryer.

PROCESSING INFORMATION

Melt Temperature:240 - 280°C
Mold Temperature:50 - 120°C
Disclaimer
With the following data, which reflect our current knowledge and experience,
we wish to describe possible applications, however this information is given
without guarantee or assurance of the appropriate properties for a specific
application.

The processor is not relieved of the responsibility for incoming quality control
nor from his own testing and analysis.

All data concerning product safety (EG-guideline, BGVV, FDA) are of principle
nature and can be limitied regarding migration, temperature and type of food.
They reflect the status as of Feb. 29, 2012. To insure that this data reflects the
current state, please contact our Product Safety Department.

Should you have any questions, wishes or suggestions about CAMPUS,
please refer to the following address:

  Link to Evonik Industries AG homepage

In any case, we hope you enjoy working with CAMPUS!

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991