  VOLTALEF 302 | PTFE | ARKEMA
Product Texts
DESIGNATION : ISO 12086-PCTFE-H, GG3N, U.3.F.B.G ,,

VOLTALEF 302 is a fluorinated polymer which presents an exceptional
behaviour at very low temperatures : it is usable in continuation from  
-200°C to +150°C with allowable peaks at 200°C. Non-inflammability,
excellent chemical and radiation resistance, good barrier properties,
insensitivity to oxygen and water, good electrical properties.

The processing is critical but can be done by extrusion, injection and
compression molding.
Mechanical propertiesValueUnitTest Standard
Tensile Modulus 1400 MPa ISO 527-1/-2
Yield stress 43 MPa ISO 527-1/-2
Yield strain 7 % ISO 527-1/-2
Nominal strain at break >50 % ISO 527-1/-2
Charpy notched impact strength (+23°C) 80 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
Melting temperature (10°C/min) 214 °C ISO 11357-1/-3
Glass transition temperature (10°C/min) 55 °C ISO 11357-1/-2
Temp. of deflection under load (1.80 MPa) 70 °C ISO 75-1/-2
Temp. of deflection under load (0.45 MPa) 126 °C ISO 75-1/-2
Oxygen index 100 % ISO 4589-1/-2
Electrical propertiesValueUnitTest Standard
Volume resistivity 2E12 Ohm*m IEC 60093
Surface resistivity >1E15 Ohm IEC 60093
Electric strength 21 kV/mm IEC 60243-1
Other propertiesValueUnitTest Standard
Water absorption 0.01 % Sim. to ISO 62
Humidity absorption 0.01 % Sim. to ISO 62
Density 2130 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
Compression Molding, molding temperature 265 °C ISO 293
Compression Molding, molding time 5 min ISO 293
Compression Molding, demolding temperature 120 °C ISO 293
Characteristics
Processing
Injection Molding, Film Extrusion, Other Extrusion, Transfer Molding
Delivery form
Powder
Special Characteristics
Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heat
Regional Availability
Disclaimer

This database provides the main properties of technical thermoplastics
marketed by ARKEMA.

      The information contained in this document is based on trials carried
out by our Research Centres and data selected from the literature, but
shall in no event be held to constitute or imply any warranty,
undertaking, express or implied commitment from our part.
Our format specifications define the limit of our commitment.
No liability whatsoever can be accepted by ARKEMA with regard to the
handling processing or use of the product or products concerned which
much in all cases be employed in accordance with all relevant laws
and/or regulations in force in the country or countries concerned.

For information about the other products marketed
by our company consult :
ARKEMAGROUP.COM

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a Registered trademark of CWFG mbH, Frankfurt/Main, 1991