CAMPUS® datasheet | Zytel® FG70G30HSLR NC010
This datasheet of Zytel® FG70G30HSLR NC010 from DuPont Engineering Polymers is provided by the international plastics database CAMPUS.
Zytel® FG70G30HSLR NC010 | PA66-GF30 | DuPont Engineering Polymers
Product Texts
Common features of Zytel® nylon resin include mechanical and physical properties such as high mechanical strength, excellent balance of stiffness and toughness, good high temperature performance, good electrical and flammability properties, good abrasion and chemical resistance. In addition, Zytel® nylon resins are available in different modified and reinforced grades to create a wide range of products with tailored properties for specific processes and end-uses. Zytel® nylon resin, including
most flame retardant grades, offer the ability to be coloured.
The good melt stability of Zytel® nylon resin normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-31kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.
Zytel® nylon resin typically is used in demanding applications in the automotive, furniture, domestic appliances, sporting goods and construction industry.
Zytel® FG70G30HSLR is a 30% glass fibre reinforced, heat stabilised, lubricated, hydrolysis resistant polyamide 66 for injection molding. It is specifically suitable for the food industry.
Food compliance:
Specific statement available
| Rheological properties | dry / cond | Unit | Test Standard |
| Molding shrinkage, parallel | 0.3 / * | % | ISO 294-4, 2577 |
| Molding shrinkage, normal | 1.1 / * | % | ISO 294-4, 2577 |
| Mechanical properties | dry / cond | Unit | Test Standard |
| Tensile Modulus | 10000 / 7000 | MPa | ISO 527-1/-2 |
| Stress at break | 200 / 130 | MPa | ISO 527-1/-2 |
| Strain at break | 3.4 / 5 | % | ISO 527-1/-2 |
| Tensile creep modulus, 1h | * / 6800 | MPa | ISO 899-1 |
| Tensile creep modulus, 1000h | * / 5100 | MPa | ISO 899-1 |
| Charpy impact strength, +23°C | 70 / 90 | kJ/m² | ISO 179/1eU |
| Charpy impact strength, -30°C | 70 / 70 | kJ/m² | ISO 179/1eU |
| Charpy notched impact strength, +23°C | 12 / 16 | kJ/m² | ISO 179/1eA |
| Charpy notched impact strength, -30°C | 10 / 10 | kJ/m² | ISO 179/1eA |
| Thermal properties | dry / cond | Unit | Test Standard |
| Melting temperature, 10°C/min | 263 / * | °C | ISO 11357-1/-3 |
| Glass transition temperature, 10°C/min | 80 / * | °C | ISO 11357-1/-2 |
| Temp. of deflection under load, 1.80 MPa | 250 / * | °C | ISO 75-1/-2 |
| Temp. of deflection under load, 0.45 MPa | 260 / * | °C | ISO 75-1/-2 |
| Vicat softening temperature, 50°C/h 50N | 250 / * | °C | ISO 306 |
| Coeff. of linear therm. expansion, parallel | 28 / * | E-6/K | ISO 11359-1/-2 |
| Coeff. of linear therm. expansion, normal | 95 / * | E-6/K | ISO 11359-1/-2 |
| Burning Behav. at 1.5 mm nom. thickn. | HB / * | class | IEC 60695-11-10 |
| Thickness tested | 1.5 / * | mm | IEC 60695-11-10 |
| UL recognition | UL / * | - | - |
| Burning Behav. at thickness h | HB / * | class | IEC 60695-11-10 |
| Thickness tested | 0.8 / * | mm | IEC 60695-11-10 |
| UL recognition | UL / * | - | - |
| Oxygen index | 24 / * | % | ISO 4589-1/-2 |
| Electrical properties | dry / cond | Unit | Test Standard |
| Relative permittivity, 100Hz | 4.3 / 11 | - | IEC 60250 |
| Relative permittivity, 1MHz | 4.1 / 4.6 | - | IEC 60250 |
| Dissipation factor, 100Hz | 70 / 4600 | E-4 | IEC 60250 |
| Dissipation factor, 1MHz | 150 / 650 | E-4 | IEC 60250 |
| Volume resistivity | >1E13 / 1E9 | Ohm*m | IEC 60093 |
| Surface resistivity | * / 1E13 | Ohm | IEC 60093 |
| Electric strength | 38 / 32 | kV/mm | IEC 60243-1 |
| Comparative tracking index | 450 / - | - | IEC 60112 |
| Other properties | dry / cond | Unit | Test Standard |
| Water absorption | 6 / * | % | Sim. to ISO 62 |
| Humidity absorption | 1.9 / * | % | Sim. to ISO 62 |
| Density | 1370 / - | kg/m³ | ISO 1183 |
| Material specific properties | dry / cond | Unit | Test Standard |
| Viscosity number | 140 / * | cm³/g | ISO 307, 1157, 1628 |
| Rheological calculation properties | Value | Unit | Test Standard |
| Density of melt | 1200 | kg/m³ | - |
| Thermal conductivity of melt | 0.21 | W/(m K) | - |
| Spec. heat capacity of melt | 2290 | J/(kg K) | - |
| Eff. thermal diffusivity | 6.85E-8 | m²/s | - |
| Ejection temperature | 190 | °C | - |
Characteristics
Processing
Injection Molding
Delivery form
Pellets
Additives
Lubricants, Release agent
Special Characteristics
Heat stabilized or stable to heat
Regional Availability
Other text information
Injection molding
PREPROCESSING
Drying recommended = Yes, if moisture content of resin exceeds recommended level
Drying temperature = 80°C
Drying time, dehumidified dryer = 2-4 h
Processing moisture content = <0.2 %
PROCESSING
Melt temperature optimum = 295°C
Melt temperature range = 285-305°C
Mold temperature optimum = 100°C
Mold temperature range = 70-120°C
Maximum Screw tangential Speed : 0.15 m/s
Flow front speed : 150 mm/ s
Hold pressure optimum : 85 MPa
Hold pressure range : 50-100 MPa
Back pressure : low
Hold pressure time : 2.5 s/mm
Maximum hold-up time : 15 min
Moulding guide
Drying recommended = Yes, if moisture content of resin exceeds recommended level
Drying temperature = 80°C
Drying time, dehumidified dryer = 2-4 h
Processing moisture content = <0.2 %
PROCESSING
Melt temperature optimum = 295°C
Melt temperature range = 285-305°C
Mold temperature optimum = 100°C
Mold temperature range = 70-120°C
Maximum Screw tangential Speed : 0.15 m/s
Flow front speed : 150 mm/ s
Hold pressure optimum : 85 MPa
Hold pressure range : 50-100 MPa
Back pressure : low
Hold pressure time : 2.5 s/mm
Maximum hold-up time : 15 min
Moulding guide
Chemical Media Resistance
Disclaimer
All data provided according to ISO 10350 for single points and ISO 11403 for multipoints.
Contact DuPont for Material Safety Data Sheet, general guides and/or additional information about ventilation, handling, purging, drying, etc.
Test temperatures are 23°C unless otherwise stated.
The DuPont Oval Logo, DuPont™, The miracles of science™ and ® are trademarks or registered trademarks of DuPont Company.
Copyright© 2011 E.I. du Pont de Nemours and Company. All Rights Reserved.
The information provided in this data sheet corresponds to our knowledge on the subject at the date of its publication.
This information may be subject to revision as new knowledge and experience becomes available.
The data provided fall within the normal range of product properties and relate only to the specific material designated; these data may not be
valid for such material used in combination with any other materials, additives or pigments or in any process, unless expressly indicated otherwise.
The data provided should not be used to establish specification limits or used alone as the basis of design; they are not intended to substitute
for any testing you may need to conduct to determine for yourself the suitability of a specific material for your particular purposes.
Since DuPont cannot anticipate all variations in actual end-use conditions DuPont makes no warranties and assumes no liability in connection
with any use of this information.
Nothing in this publication is to be considered as a license to operate under or a recommendation to infringe any patent rights.
DuPont advises you to seek independent counsel for a freedom to practice opinion on the intended application or end-use of our products.
CAUTION: DO NOT USE DUPONT MATERIALS IN MEDICAL APPLICATIONS INVOLVING IMPLANTATION IN THE HUMAN BODY OR
CONTACT WITH INTERNAL BODY FLUIDS OR TISSUES UNLESS THE MATERIAL HAS BEEN PROVIDED FROM DUPONT UNDER A
WRITTEN CONTRACT THAT IS CONSISTENT WITH DUPONT POLICY REGARDING MEDICAL APPLICATIONS AND EXPRESSLY
ACKNOWLEDGES THE CONTEMPLATED USE.
For further information, please contact your DuPont representative. You may also request a copy of DuPont POLICY Regarding Medical
Applications... H-50103-3 and DuPont CAUTION Regarding Medical Applications... H-50102-3.
Contact DuPont for Material Safety Data Sheet, general guides and/or additional information about ventilation, handling, purging, drying, etc.
Test temperatures are 23°C unless otherwise stated.
The DuPont Oval Logo, DuPont™, The miracles of science™ and ® are trademarks or registered trademarks of DuPont Company.
Copyright© 2011 E.I. du Pont de Nemours and Company. All Rights Reserved.
The information provided in this data sheet corresponds to our knowledge on the subject at the date of its publication.
This information may be subject to revision as new knowledge and experience becomes available.
The data provided fall within the normal range of product properties and relate only to the specific material designated; these data may not be
valid for such material used in combination with any other materials, additives or pigments or in any process, unless expressly indicated otherwise.
The data provided should not be used to establish specification limits or used alone as the basis of design; they are not intended to substitute
for any testing you may need to conduct to determine for yourself the suitability of a specific material for your particular purposes.
Since DuPont cannot anticipate all variations in actual end-use conditions DuPont makes no warranties and assumes no liability in connection
with any use of this information.
Nothing in this publication is to be considered as a license to operate under or a recommendation to infringe any patent rights.
DuPont advises you to seek independent counsel for a freedom to practice opinion on the intended application or end-use of our products.
CAUTION: DO NOT USE DUPONT MATERIALS IN MEDICAL APPLICATIONS INVOLVING IMPLANTATION IN THE HUMAN BODY OR
CONTACT WITH INTERNAL BODY FLUIDS OR TISSUES UNLESS THE MATERIAL HAS BEEN PROVIDED FROM DUPONT UNDER A
WRITTEN CONTRACT THAT IS CONSISTENT WITH DUPONT POLICY REGARDING MEDICAL APPLICATIONS AND EXPRESSLY
ACKNOWLEDGES THE CONTEMPLATED USE.
For further information, please contact your DuPont representative. You may also request a copy of DuPont POLICY Regarding Medical
Applications... H-50103-3 and DuPont CAUTION Regarding Medical Applications... H-50102-3.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012