  ALCOM® POM 770/1 PTFE15 | (POM+PTFE) | ALBIS Plastic GmbH
Propiedades mecánicasValorUnidadesMétodo de ensayo
Módulo de tracción 2300 MPa ISO 527-1/-2
Esfuerzo de fluencia 47 MPa ISO 527-1/-2
Alarg. en límite elástico 9 % ISO 527-1/-2
Resistencia al impacto Charpy, +23°C 40 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalla, +23°C 3.5 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
Temperatura de fusión, 10°C/min 166 °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 88 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, 50°C/h 50N 143 °C ISO 306
Propiedades eléctricasValorUnidadesMétodo de ensayo
Resistividad superficial específica 1E13 Ohm IEC 60093
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1490 kg/m³ ISO 1183
Características
Procesamiento y forma de entrega
Moldeo por inyección
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Aviso
Any information given on the chemical and physical characteristics of
our products, including technical advice on applications whether
verbally, in writing or by testing the product, is given to the best
of our knowledge, but without warranty. It does not exempt the buyer
from carrying out his own investigations and tests in order to
ascertain the products' specific suitability for the purpose intended.

The buyer is solely responsible for the application, utilisation and
processing of the products, and must observe the laws and government
regulations and the consequential rights of any third party. At all
times our Conditions of Sale apply.

The test values given are guide values, not binding minimum or maximum
figures, which have been determined on standardized test specimen and
can be affected by pigmentation, mold design and processing conditions.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012