  ALFATER XL® A55I 2GP0000 | TPV | ALBIS Plastic GmbH
Propiedades mecánicasValorUnidadesMétodo de ensayo
Tensión a 100% alargamiento 2 MPa ISO 527-1/-2
Alargamiento a rotura TPE >300 % ISO 527-1/-2
Valor de compr. bajo tensión const., 100°C 34 % ISO 815
Resistencia al desgarro 20 kN/m ISO 34-1
Dureza Shore A, 3s 55 - ISO 868
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 960 kg/m³ ISO 1183
Características
Procesamiento y forma de entrega
Moldeo por inyección
Características especiales
Estable contra rayos U.V./interperie
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Aviso
Any information given on the chemical and physical characteristics of
our products, including technical advice on applications whether
verbally, in writing or by testing the product, is given to the best
of our knowledge, but without warranty. It does not exempt the buyer
from carrying out his own investigations and tests in order to
ascertain the products' specific suitability for the purpose intended.

The buyer is solely responsible for the application, utilisation and
processing of the products, and must observe the laws and government
regulations and the consequential rights of any third party. At all
times our Conditions of Sale apply.

The test values given are guide values, not binding minimum or maximum
figures, which have been determined on standardized test specimen and
can be affected by pigmentation, mold design and processing conditions.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012