| Propiedades mecánicas | Valor | Unidades | Método de ensayo |
| Tensión a 100% alargamiento | 5.8 | MPa | ISO 527-1/-2 |
| Alargamiento a rotura TPE | >300 | % | ISO 527-1/-2 |
| Valor de compr. bajo tensión const., 100°C | 60 | % | ISO 815 |
| Resistencia al desgarro | 50 | kN/m | ISO 34-1 |
| Dureza Shore A, 3s | 90 | - | ISO 868 |
| Propiedades térmicas | Valor | Unidades | Método de ensayo |
| Combustibilidad a espesor h | HB | class | IEC 60695-11-10 |
| Espesores de probeta | 3.0 | mm | IEC 60695-11-10 |
| Otras propiedades | Valor | Unidades | Método de ensayo |
| Densidad | 970 | kg/m³ | ISO 1183 |
Características
Procesamiento y forma de entrega
Moldeo por inyección, Otros tipos de extrusión
Características especiales
Estable contra rayos U.V./interperie
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Aviso
Any information given on the chemical and physical characteristics of our products, including technical advice on applications whether verbally, in writing or by testing the product, is given to the best of our knowledge, but without warranty. It does not exempt the buyer from carrying out his own investigations and tests in order to ascertain the products' specific suitability for the purpose intended. The buyer is solely responsible for the application, utilisation and processing of the products, and must observe the laws and government regulations and the consequential rights of any third party. At all times our Conditions of Sale apply. The test values given are guide values, not binding minimum or maximum figures, which have been determined on standardized test specimen and can be affected by pigmentation, mold design and processing conditions.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012