| Propiedades mecánicas | Seco / Cond | Unidades | Método de ensayo |
| Módulo de tracción | 6500 / 4500 | MPa | ISO 527-1/-2 |
| Resistencia a la tracción | 90 / 75 | MPa | ISO 527-1/-2 |
| Alargamiento a rotura | 6 / 15 | % | ISO 527-1/-2 |
| Resistencia al impacto Charpy, +23°C | 80 / - | kJ/m² | ISO 179/1eU |
| Res. impacto Charpy c/entalla, +23°C | 4 / - | kJ/m² | ISO 179/1eA |
| Propiedades térmicas | Seco / Cond | Unidades | Método de ensayo |
| Temperatura de fusión, 10°C/min | 253 / * | °C | ISO 11357-1/-3 |
| Estabilidad al calor, 1.80 MPa | 120 / * | °C | ISO 75-1/-2 |
| Estabilidad al calor, 0.45 MPa | 235 / * | °C | ISO 75-1/-2 |
| Temp. reblandecimiento Vicat, 50°C/h 50N | 200 / * | °C | ISO 306 |
| Propiedades eléctricas | Seco / Cond | Unidades | Método de ensayo |
| Resistividad volumétrica específica | 1E13 / 1E10 | Ohm*m | IEC 60093 |
| Resistividad superficial específica | * / 1E12 | Ohm | IEC 60093 |
| Indice comparativo de linea de fuga | 550 / - | - | IEC 60112 |
| Otras propiedades | Seco / Cond | Unidades | Método de ensayo |
| Absorción de agua | 5 / * | % | Sim. to ISO 62 |
| Absorción de humedad | 1.3 / * | % | Sim. to ISO 62 |
| Densidad | 1500 / - | kg/m³ | ISO 1183 |
Características
Procesamiento y forma de entrega
Moldeo por inyección
Características especiales
Estable contra el calor
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Aviso
Any information given on the chemical and physical characteristics of our products, including technical advice on applications whether verbally, in writing or by testing the product, is given to the best of our knowledge, but without warranty. It does not exempt the buyer from carrying out his own investigations and tests in order to ascertain the products' specific suitability for the purpose intended. The buyer is solely responsible for the application, utilisation and processing of the products, and must observe the laws and government regulations and the consequential rights of any third party. At all times our Conditions of Sale apply. The test values given are guide values, not binding minimum or maximum figures, which have been determined on standardized test specimen and can be affected by pigmentation, mold design and processing conditions.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012