CAMPUS® datasheet | ALTECH PC C 1000/100


This datasheet of ALTECH PC C 1000/100 from ALBIS Plastic GmbH is provided by the international plastics database CAMPUS.

You may contact the supplier for more information about this grade.

This datasheet includes:

  ALTECH PC C 1000/100 | PC | ALBIS Plastic GmbH
Propiedades reológicasValorUnidadesMétodo de ensayo
Indice de fluidez volumétrico, MVR 11 cm³/10min ISO 1133
Temperatura 300 °C ISO 1133
Carga 1.2 kg ISO 1133
Propiedades mecánicasValorUnidadesMétodo de ensayo
Resistencia al impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalla, +23°C 10 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
Temp. reblandecimiento Vicat, 50°C/h 50N 141 °C ISO 306
Propiedades eléctricasValorUnidadesMétodo de ensayo
Resistividad volumétrica específica 1E11 Ohm*m IEC 60093
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1200 kg/m³ ISO 1183
Características
Procesamiento y forma de entrega
Moldeo por inyección
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Aviso
Any information given on the chemical and physical characteristics of
our products, including technical advice on applications whether
verbally, in writing or by testing the product, is given to the best
of our knowledge, but without warranty. It does not exempt the buyer
from carrying out his own investigations and tests in order to
ascertain the products' specific suitability for the purpose intended.

The buyer is solely responsible for the application, utilisation and
processing of the products, and must observe the laws and government
regulations and the consequential rights of any third party. At all
times our Conditions of Sale apply.

The test values given are guide values, not binding minimum or maximum
figures, which have been determined on standardized test specimen and
can be affected by pigmentation, mold design and processing conditions.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012