CAMPUS® datasheet | Delrin® FG100TL NC010


This datasheet of Delrin® FG100TL NC010 from DuPont Engineering Polymers is provided by the international plastics database CAMPUS.

This datasheet includes:

  Delrin® FG100TL NC010 | POM | DuPont Engineering Polymers
Texto del producto
Common features of Delrin® acetal resin include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating and available in a variety of colours and speciality grades.

 

The good melt stability of Delrin® acetal resin normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-17 kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.

 

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics and consumer goods industries.

 

Delrin® FG100TL is a 1.5% Teflon® PTFE Micropowder filled, high viscosity acetal homopolymer for injection molding. It is specifically suitable for the food industry.

Design guide

 

Propiedades reológicasValorUnidadesMétodo de ensayo
Indice de fluidez volumétrico, MVR 1.9 cm³/10min ISO 1133
Temperatura 190 °C ISO 1133
Carga 2.16 kg ISO 1133
Contracción posterior al moldeo, paralelo 1.8 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 1.7 % ISO 294-4, 2577
Propiedades mecánicasValorUnidadesMétodo de ensayo
Módulo de tracción 3000 MPa ISO 527-1/-2
Esfuerzo de fluencia 71 MPa ISO 527-1/-2
Alarg. en límite elástico 25 % ISO 527-1/-2
Alarg. nominal a rotura 33 % ISO 527-1/-2
Resistencia al impacto Charpy, +23°C 150 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalla, +23°C 9 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalla, -30°C 8 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
Temperatura de fusión, 10°C/min 178 °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 95 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 158 °C ISO 75-1/-2
Coef.de expansión térmica lineal, paralelo 110 E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 110 E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB class IEC 60695-11-10
Espesores de probeta 1.5 mm IEC 60695-11-10
Combustibilidad a espesor h HB class IEC 60695-11-10
Espesores de probeta 0.8 mm IEC 60695-11-10
Propiedades eléctricasValorUnidadesMétodo de ensayo
Resistividad superficial específica >1E15 Ohm IEC 60093
Indice comparativo de linea de fuga 600 - IEC 60112
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.9 % Sim. to ISO 62
Absorción de humedad 0.2 % Sim. to ISO 62
Densidad 1430 kg/m³ ISO 1183
Cálculo propiedades reológicasValorUnidadesMétodo de ensayo
Densidad de fusión 1180 kg/m³ -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Disponibilidad regional
Aviso
All data provided according to ISO 10350 for single points and ISO 11403 for multipoints.

Contact DuPont for Material Safety Data Sheet, general guides and/or additional information about ventilation, handling, purging, drying, etc.
Test temperatures are 23°C unless otherwise stated.

The DuPont Oval Logo, DuPont™, The miracles of science™ and ® are trademarks or registered trademarks of DuPont Company.
Copyright© 2011 E.I. du Pont de Nemours and Company. All Rights Reserved.

The information provided in this data sheet corresponds to our knowledge on the subject at the date of its publication.
This information may be subject to revision as new knowledge and experience becomes available.
The data provided fall within the normal range of product properties and relate only to the specific material designated; these data may not be
valid for such material used in combination with any other materials, additives or pigments or in any process, unless expressly indicated otherwise.
The data provided should not be used to establish specification limits or used alone as the basis of design; they are not intended to substitute
for any testing you may need to conduct to determine for yourself the suitability of a specific material for your particular purposes.
Since DuPont cannot anticipate all variations in actual end-use conditions DuPont makes no warranties and assumes no liability in connection
with any use of this information.
Nothing in this publication is to be considered as a license to operate under or a recommendation to infringe any patent rights.
DuPont advises you to seek independent counsel for a freedom to practice opinion on the intended application or end-use of our products.

CAUTION: DO NOT USE DUPONT MATERIALS IN MEDICAL APPLICATIONS INVOLVING IMPLANTATION IN THE HUMAN BODY OR
CONTACT WITH INTERNAL BODY FLUIDS OR TISSUES UNLESS THE MATERIAL HAS BEEN PROVIDED FROM DUPONT UNDER A
WRITTEN CONTRACT THAT IS CONSISTENT WITH DUPONT POLICY REGARDING MEDICAL APPLICATIONS AND EXPRESSLY
ACKNOWLEDGES THE CONTEMPLATED USE.

For further information, please contact your DuPont representative. You may also request a copy of DuPont POLICY Regarding Medical
Applications... H-50103-3 and DuPont CAUTION Regarding Medical Applications... H-50102-3.