Texto del producto
PA 6, non-reinforced, extrusion, Blasform, impact modified, heat-ageing stabilized
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
Módulo de tracción 980 / 210 MPa ISO 527-1/-2
Esfuerzo de fluencia 28 / - MPa ISO 527-1/-2
Alarg. en límite elástico 6.5 / - % ISO 527-1/-2
Resistencia al impacto Charpy, -30°C 105 / - kJ/m² ISO 179/1eU
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
Temperatura de fusión, 10°C/min 211 / * °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 48 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 53 / * °C ISO 75-1/-2
Coef.de expansión térmica lineal, paralelo 200 / * E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 200 / * E-6/K ISO 11359-1/-2
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Densidad 1030 / - kg/m³ ISO 1183
Características
Procesamiento y forma de entrega
Moldeo por soplado
Forma de suministro
Sémola
Aditivos
Lubricante
Características especiales
Estable contra el calor
Disponibilidad regional
Aviso
This information and our  technical advice - whether verbal, in  writing
or by way of trials - are  given in good faith but without warranty, and
this  also  applies  where  proprietary  rights  of  third  parties  are
involved.  Our advice does not release you from  the obligation to check
its validity and to test our  products  as to their  suitability for the
intended processes and uses.  The  application, use  and  processing  of
our products and the products manufactured  by  you  on the basis of our
technical  advice  are  beyond our control and, therefore, entirely your
own  responsibility.  Our  products  are  sold  in  accordance  with our
General  Conditions of Sale and Delivery.
The values  stored in the databank should only be used as guidelines for
component   design.  In  giving  these  values  neither  guarantee,  nor
assurance of particular material properties can be given.

techcenter.lanxess.com

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012