  HOSTAFORM C 9021 TF5 | POM | Ticona
Texto del producto
Hostaform® C 9021 TF5 is a standard flow low level
polytetraflouroethylene filled (PTFE) product designed for use in wear
applications against plastics, metal, glass or ceramic mating surfaces
where silicone lubricants can not be tolerated.
Propiedades reológicasValorUnidadesMétodo de ensayo
Indice de fluidez volumétrico, MVR 8.5 cm³/10min ISO 1133
Temperatura 190 °C ISO 1133
Carga 2.16 kg ISO 1133
Propiedades mecánicasValorUnidadesMétodo de ensayo
Módulo de tracción 2600 MPa ISO 527-1/-2
Resistencia al impacto Charpy, +23°C 125 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 110 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalla, +23°C 5.2 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
Temperatura de fusión, 10°C/min 166 °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 102 °C ISO 75-1/-2
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 0.65 % Sim. to ISO 62
Absorción de humedad 0.2 % Sim. to ISO 62
Densidad 1440 kg/m³ ISO 1183
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Aditivos
Lubricante, Desmoldeante
Disponibilidad regional
Aviso
NOTICE TO USERS: Values shown are based on testing
of laboratory test specimens and represent data that fall
within the standard range of properties for natural material.
These values alone do not represent a sufficient basis for
any part design and are not intended for use in
establishing maximum, minimum, or ranges of values for
specification purposes. Colorants or other additives may
cause significant variations in data values.

Properties of molded parts can be influenced by a wide
variety of factors including, but not limited to, material
selection, additives, part design, processing conditions and
environmental exposure. Any determination of the
suitability of a particular material and part design for any
use contemplated by the users and the manner of such
use is the sole responsibility of the users, who must assure
themselves that the material as subsequently processed
meets the needs of their particular product or use.

To the best of our knowledge, the information contained in
this publication is accurate; however, we do not assume
any liability whatsoever for the accuracy and completeness
of such information. The information contained in this
publication should not be construed as a promise or
guarantee of specific properties of our products. It is the
sole responsibility of the users to investigate whether any
existing patents are infringed by the use of the materials
mentioned in this publication.

Moreover, there is a need to reduce human exposure to
many materials to the lowest practical limits in view of
possible adverse effects. To the extent that any hazards
may have been mentioned in this publication, we neither
suggest nor guarantee that such hazards are the only ones
which exist. We recommend that persons intending to rely
on any recommendation or to use any equipment,
processing technique, or material mentioned in this
publication should satisfy themselves that they can meet
all applicable safety and health standards.

We strongly recommend that users seek and adhere to the
manufacturer's current instructions for handling each
material they use, and to entrust the handling of such
material to adequately trained personnel only. Please call
the telephone numbers listed for additional technical
information. Call Customer Services for the appropriate
Materials Safety Data Sheets (MSDS) before attempting to
process our products.

The products mentioned herein are not intended for use in
medical or dental implants.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012