Texto del producto
Impact ABS grade with antistatic
| Propiedades reológicas | Valor | Unidades | Método de ensayo |
| Indice de fluidez volumétrico, MVR | 22 | cm³/10min | ISO 1133 |
| Temperatura | 220 | °C | ISO 1133 |
| Carga | 10 | kg | ISO 1133 |
| Propiedades mecánicas | Valor | Unidades | Método de ensayo |
| Módulo de tracción | 2200 | MPa | ISO 527-1/-2 |
| Esfuerzo de fluencia | 48 | MPa | ISO 527-1/-2 |
| Alarg. en límite elástico | 2.3 | % | ISO 527-1/-2 |
| Resistencia al impacto Charpy, +23°C | N | kJ/m² | ISO 179/1eU |
| Res. impacto Charpy c/entalla, +23°C | 18 | kJ/m² | ISO 179/1eA |
| Propiedades térmicas | Valor | Unidades | Método de ensayo |
| Temp. reblandecimiento Vicat, 50°C/h 50N | 96 | °C | ISO 306 |
| Combustibilidad a 1.5mm esp. nom. | HB | class | IEC 60695-11-10 |
| Espesores de probeta | 1.5 | mm | IEC 60695-11-10 |
| Valoración UL | UL | - | - |
| Propiedades eléctricas | Valor | Unidades | Método de ensayo |
| Resistividad volumétrica específica | >1E13 | Ohm*m | IEC 60093 |
| Resistividad superficial específica | >1E15 | Ohm | IEC 60093 |
| Otras propiedades | Valor | Unidades | Método de ensayo |
| Densidad | 1050 | kg/m³ | ISO 1183 |
Funciones
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Granulado
Características especiales
Antiestático
Disponibilidad regional
Aviso
The information and recommendations contained in this document are based upon
data collected by A. Schulman and are believed to be reliable; however, because
A. Schulman cannot anticipate or control the many different conditions under
which this information and/or product may be used, no representation is made
and no warranty is given of any kind, express or implied, for completeness,
accuracy, availability, suitability, usefulness, commercial value, or non-violation
of intellectual property rights of information, recommendations, and products
and services directly or indirectly provided. A. Schulman assumes no responsibility
for the results of the use of products and processes described herein and expressly
disclaims the implied warranties of merchantability and fitness for a particular use
If there are questions to given information, to further properties or further A. Schulman
products please contact
A. Schulman GmbH
Huettenstrasse 211
50170 Kerpen
Tel: 02273 / 561-0
Contact: aschulman@de.aschulman.com
Subject: Material data
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012