CAMPUS® datasheet | Technyl® C 502XT


This datasheet of Technyl® C 502XT from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.

This datasheet includes:

  Technyl® C 502XT | PA6 | Rhodia Polyamide Engineering Plastics
Texto del producto
Unreinforced polyamide 6, very high viscosity, for extrusion.
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
Módulo de tracción 2800 / 900 MPa ISO 527-1/-2
Esfuerzo de fluencia 80 / - MPa ISO 527-1/-2
Alarg. en límite elástico 4.1 / - % ISO 527-1/-2
Alarg. nominal a rotura >50 / - % ISO 527-1/-2
Resistencia al impacto Charpy, +23°C N / - kJ/m² ISO 179/1eU
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
Temperatura de fusión, 10°C/min 222 / * °C ISO 11357-1/-3
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de humedad 1.37 / * % Sim. to ISO 62
Densidad 1130 / - kg/m³ ISO 1183
Funciones
Esfuerzo-alargamiento , Technyl® C 502XT, PA6, Rhodia
Aviso
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012