Resin: ISO 7792-PBT,MHR, A10-07,M30
VESTODUR® X7095 is a glass fiber reinforced semicrystalline thermoplastic resin for injection molding, based on
polybutylene terephthalate (PBT) with low warpage at parts made of this resin. The compound is suitable for the
manufacture of parts, which are subjected to high mechanical and thermal load.
| Propiedades reológicas | Valor | Unidades | Método de ensayo |
| Indice de fluidez volumétrico, MVR | 12 | cm³/10min | ISO 1133 |
| Temperatura | 250 | °C | ISO 1133 |
| Carga | 2.16 | kg | ISO 1133 |
| Contracción posterior al moldeo, paralelo | 0.5 | % | ISO 294-4, 2577 |
| Contracción posterior al moldeo, normal | 1.8 | % | ISO 294-4, 2577 |
| Propiedades mecánicas | Valor | Unidades | Método de ensayo |
| Módulo de tracción | 7000 | MPa | ISO 527-1/-2 |
| Resistencia a la tracción | 105 | MPa | ISO 527-1/-2 |
| Alargamiento a rotura | 4 | % | ISO 527-1/-2 |
| Resistencia al impacto Charpy, +23°C | 30 | kJ/m² | ISO 179/1eU |
| Resistencia al impacto Charpy, -30°C | 30 | kJ/m² | ISO 179/1eU |
| Res. impacto Charpy c/entalla, +23°C | 5.5 | kJ/m² | ISO 179/1eA |
| Res. impacto Charpy c/entalla, -30°C | 4.5 | kJ/m² | ISO 179/1eA |
| Propiedades térmicas | Valor | Unidades | Método de ensayo |
| Temperatura de fusión, 10°C/min | 223 | °C | ISO 11357-1/-3 |
| Temp. de transición vítrea, 10°C/min | 45 | °C | ISO 11357-1/-2 |
| Estabilidad al calor, 1.80 MPa | 195 | °C | ISO 75-1/-2 |
| Estabilidad al calor, 0.45 MPa | 220 | °C | ISO 75-1/-2 |
| Temp. reblandecimiento Vicat, 50°C/h 50N | 210 | °C | ISO 306 |
| Coef.de expansión térmica lineal, paralelo | 60 | E-6/K | ISO 11359-1/-2 |
| Coef.de expansión térmica lineal, normal | 70 | E-6/K | ISO 11359-1/-2 |
| Combustibilidad a 1.5mm esp. nom. | HB | class | IEC 60695-11-10 |
| Espesores de probeta | 1.6 | mm | IEC 60695-11-10 |
| Combustibilidad a espesor h | HB | class | IEC 60695-11-10 |
| Espesores de probeta | 0.8 | mm | IEC 60695-11-10 |
| Propiedades eléctricas | Valor | Unidades | Método de ensayo |
| Constante dieléctrica, 100Hz | 4 | - | IEC 60250 |
| Resistividad volumétrica específica | 1E13 | Ohm*m | IEC 60093 |
| Resistividad superficial específica | 1E14 | Ohm | IEC 60093 |
| Resistencia dieléctrica | 27 | kV/mm | IEC 60243-1 |
| Indice comparativo de linea de fuga | 275 | - | IEC 60112 |
| Otras propiedades | Valor | Unidades | Método de ensayo |
| Absorción de agua | 0.5 | % | Sim. to ISO 62 |
| Densidad | 1530 | kg/m³ | ISO 1183 |
| Condiciones de transformación | Valor | Unidades | Método de ensayo |
| Condiciones de transformación según ISO | 7790 | - | ISO ....-2 |
| Moldeo por inyección, temperatura de la masa | 260 | °C | ISO 294 |
| Moldeo por inyección, temperatura del molde | 80 | °C | ISO 10724 |
| Moldeo por inyección, velocidad de inyección | 200 | mm/s | ISO 294 |
| Moldeo por inyección, presión de mantenimiento | 70 | MPa | ISO 294 |
All listed technical data are typical values intended for your guidance.
They are given without obligation and do not constitute a materials
specification. Should you have any further questions concerning material
behavior or properties, please contact us at the following address :
for PA: Evonik Industries AG
PP-HP-CRM
Gebäude 1227 / PB 16
D-45764 Marl
Phone: +49-(0)2365/49-2720
Fax:+49-(0)2365/49-2070
E-Mail: campusplastics@evonik.com
for PMMA: Evonik Industries AG
Marketing / Campus
Kirschenallee
D-64293 Darmstadt
Germany
Phone: +49 - (0) 61 51 / 18-47 11
Fax: +49 - (0) 61 51 / 18-31 77
E-Mail: campusplastics@evonik.com
Internet: http://www.plexiglas-polymers.com
® = registered trademark
PLEXIGLAS® is a registered trademark of Evonik Röhm GmbH, Germany,
outside of the Americas. Within the Americas it is sold as ACRYLITE®,
which is a registered trademark of Evonik Cyro LLC, USA.
PLEXIMID® is a registered trademarks of Evonik Röhm GmbH, Germany.
CYROLITE® and XT® polymer are registered trademarks of Evonik Cyro LLC, USA.
This information and all further technical advice is based on our present knowledge
and experience. However, it implies no liability or other legal responsibility on our part,
including with regard to existing third party intellectual property rights, especially
patent rights. In particular, no warranty, whether express or implied, or guarantee of
product properties in the legal sense is intended or implied. We reserve the right to
make any changes according to technological progress or further developments. The
customer is not released from the obligation to conduct careful inspection and testing
of incoming goods. Performance of the product described herein should be verified by
testing, which should be carried out only by qualified experts in the sole responsibility
of a customer. Reference to trade names used by other companies is neither a
recommendation, nor does it imply that similar products could not be used.
NAFTA:
This information and all technical and other advice are based on Evonik’s
present knowledge and experience. However, Evonik assumes no liability for
such information or advice, including the extent to which such information or
advice may relate to third party intellectual property rights. Evonik reserves the
right to make any changes to information or advice at any time, without prior
or subsequent notice. EVONIK DISCLAIMS ALL REPRESENTATIONS AND
WARRANTIES, WHETHER EXPRESS OR IMPLIED, AND SHALL HAVE NO LIABILITY
FOR, MERCHANTABILITY OF THE PRODUCT OR ITS FITNESS FOR A PARTICULAR
PURPOSE (EVEN IF EVONIK IS AWARE OF SUCH PURPOSE), OR OTHERWISE.
EVONIK SHALL NOT BE RESPONSIBLE FOR CONSEQUENTIAL, INDIRECT OR
INCIDENTAL DAMAGES (INCLUDING LOSS OF PROFITS) OF ANY KIND. It is the
customer’s sole responsibility to arrange for inspection and testing of all
products by qualified experts. Reference to trade names used by other
companies is neither a recommendation nor an endorsement of the
corresponding product, and does not imply that similar products could not be
used.
Sales range and technical data subject to alteration.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012