Texto del producto
VESTORAN® 1900 blk 2.7024


Unfilled, amorphous PPE resin.

As a material of amorphous structure VESTORAN® 1900 blk 2.7024 shows very small mold shrinkage. Therefore

molded parts have a very low tendency to warp. The impact modified compound is of low density and easy to

process. Further properties are excellent impact strength, heat deflection under load and suitability for being

coated with lacquers.
Moldings of VESTORAN® 1900 blk 2.7024 are dimensionally stable and hydrolysis resistant even in hot water, but

are more sensitive to organic solvents than semi-crystalline plastics. VESTORAN® 1900 blk 2.7024 is resistant to

aqueous alkalines and acides, certain alcohols, and glycol solutions.

VESTORAN® 1900 blk 2.7024 is particularly suitable for the adhesion promoter-free manufacturing of plastic/ rubber

composites by the Evonik Industries AG -patented K&K process.
VESTORAN® 1900 blk 2.7024 is supplied as cylindrical granules in PE-bags.

Propiedades reológicasValorUnidadesMétodo de ensayo
Indice de fluidez volumétrico, MVR 40 cm³/10min ISO 1133
Temperatura 300 °C ISO 1133
Carga 21.6 kg ISO 1133
Contracción posterior al moldeo, paralelo 0.9 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.8 % ISO 294-4, 2577
Propiedades mecánicasValorUnidadesMétodo de ensayo
Módulo de tracción 2000 MPa ISO 527-1/-2
Esfuerzo de fluencia 60 MPa ISO 527-1/-2
Alarg. en límite elástico 6 % ISO 527-1/-2
Alarg. nominal a rotura >50 % ISO 527-1/-2
Módulo de plastodeformación, 1h 2000 MPa ISO 899-1
Módulo de plastodeformación, 1000h 2000 MPa ISO 899-1
Resistencia al impacto Charpy, +23°C 250 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalla, +23°C 25 kJ/m² ISO 179/1eA
Resistencia al impacto a tracción, +23°C 110 kJ/m² ISO 8256/1
Propiedades térmicasValorUnidadesMétodo de ensayo
Estabilidad al calor, 1.80 MPa 170 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 190 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, 50°C/h 50N 190 °C ISO 306
Coef.de expansión térmica lineal, paralelo 80 E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 80 E-6/K ISO 11359-1/-2
Propiedades eléctricasValorUnidadesMétodo de ensayo
Constante dieléctrica, 100Hz 2.6 - IEC 60250
Constante dieléctrica, 1MHz 2.9 - IEC 60250
Factor de pérdidas dieléctricas, 100Hz 8 E-4 IEC 60250
Factor de pérdidas dieléctricas, 1MHz 16 E-4 IEC 60250
Resistividad volumétrica específica >1E13 Ohm*m IEC 60093
Resistividad superficial específica 2E14 Ohm IEC 60093
Resistencia dieléctrica 40 kV/mm IEC 60243-1
Indice comparativo de linea de fuga 225 - IEC 60112
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1040 kg/m³ ISO 1183
Cálculo propiedades reológicasValorUnidadesMétodo de ensayo
Densidad de fusión 900 kg/m³ -
Conductibilidad termica de fusión 0.21 W/(m K) -
Calor especifico de la masa 1910 J/(kg K) -
Temperatura de expulsión 200 °C -
Condiciones de transformaciónValorUnidadesMétodo de ensayo
Moldeo por inyección, temperatura de la masa 320 °C ISO 294
Moldeo por inyección, temperatura del molde 80 °C ISO 10724
Moldeo por inyección, velocidad de inyección 200 mm/s ISO 294
Funciones
Viscosidad-velocidad de cizallamiento , VESTORAN® 1900 blk (sw) 2.7024, PPE-I, Evonik Industries
Tensión de cizalla-velocidad de cizalla , VESTORAN® 1900 blk (sw) 2.7024, PPE-I, Evonik Industries
Módulo de cizallamiento dinámico-temperatura , VESTORAN® 1900 blk (sw) 2.7024, PPE-I, Evonik Industries
Esfuerzo-alargamiento , VESTORAN® 1900 blk (sw) 2.7024, PPE-I, Evonik Industries
Módulo secante-alargamiento , VESTORAN® 1900 blk (sw) 2.7024, PPE-I, Evonik Industries
Esfuerzo-alargamiento (isocrono) 23°C, VESTORAN® 1900 blk (sw) 2.7024, PPE-I, Evonik Industries
Módulo de plastodeformación-tiempo 23°C, VESTORAN® 1900 blk (sw) 2.7024, PPE-I, Evonik Industries
Volumen especifico-temperatura (pvT) , VESTORAN® 1900 blk (sw) 2.7024, PPE-I, Evonik Industries
Características
Procesamiento y forma de entrega
Moldeo por inyección, Extrusion del film, Extrusión de perfiles, Extrusión de láminas, Otros tipos de extrusión, Moldeo por soplado, Termoconformación
Forma de suministro
Sémola
Características especiales
Galvanizable, Estable contra el calor
Disponibilidad regional
Aviso
All listed technical data are typical values intended for your guidance.
They are given without obligation and do not constitute a materials
specification. Should you have any further questions concerning material
behavior or properties, please contact us at the following address :

for PA:           Evonik Industries AG
                     PP-HP-CRM
                     Gebäude 1227 / PB 16
                     D-45764 Marl
                     Phone: +49-(0)2365/49-2720
                     Fax:+49-(0)2365/49-2070
                     E-Mail: campusplastics@evonik.com

for PMMA:     Evonik Industries AG
                     Marketing / Campus
                     Kirschenallee
                     D-64293 Darmstadt
                     Germany
                     Phone: +49 - (0) 61 51 / 18-47 11
                     Fax: +49 - (0) 61 51 / 18-31 77
                     E-Mail: campusplastics@evonik.com
                     Internet: http://www.plexiglas-polymers.com

 

® = registered trademark

 

PLEXIGLAS® is a registered trademark of Evonik Röhm GmbH, Germany,

outside of the Americas. Within the Americas it is sold as ACRYLITE®,

which is a registered trademark of Evonik Cyro LLC, USA.

PLEXIMID® is a registered trademarks of Evonik Röhm GmbH, Germany.

CYROLITE® and XT® polymer are registered trademarks of Evonik Cyro LLC, USA.

 

This information and all further technical advice is based on our present knowledge

and experience. However, it implies no liability or other legal responsibility on our part,

including with regard to existing third party intellectual property rights, especially

patent rights. In particular, no warranty, whether express or implied, or guarantee of

product properties in the legal sense is intended or implied. We reserve the right to

make any changes according to technological progress or further developments. The

customer is not released from the obligation to conduct careful inspection and testing

of incoming goods. Performance of the product described herein should be verified by

testing, which should be carried out only by qualified experts in the sole responsibility

of a customer. Reference to trade names used by other companies is neither a

recommendation, nor does it imply that similar products could not be used.

 

NAFTA:

This information and all technical and other advice are based on Evonik’s

present knowledge and experience. However, Evonik assumes no liability for

such information or advice, including the extent to which such information or

advice may relate to third party intellectual property rights. Evonik reserves the

right to make any changes to information or advice at any time, without prior

or subsequent notice. EVONIK DISCLAIMS ALL REPRESENTATIONS AND

WARRANTIES, WHETHER EXPRESS OR IMPLIED, AND SHALL HAVE NO LIABILITY

FOR, MERCHANTABILITY OF THE PRODUCT OR ITS FITNESS FOR A PARTICULAR

PURPOSE (EVEN IF EVONIK IS AWARE OF SUCH PURPOSE), OR OTHERWISE.

EVONIK SHALL NOT BE RESPONSIBLE FOR CONSEQUENTIAL, INDIRECT OR

INCIDENTAL DAMAGES (INCLUDING LOSS OF PROFITS) OF ANY KIND. It is the

customer’s sole responsibility to arrange for inspection and testing of all

products by qualified experts. Reference to trade names used by other

companies is neither a recommendation nor an endorsement of the

corresponding product, and does not imply that similar products could not be

used.

 

Sales range and technical data subject to alteration.