CAMPUS® datasheet | XANTAR® MX 1021
This datasheet of XANTAR® MX 1021 from Mitsubishi Engineering-Plastics Corporation is provided by the international plastics database CAMPUS.
XANTAR® MX 1021 | PC | Mitsubishi Engineering-Plastics Corporation
Texto del producto
Stress Crack Modified
ISO 1043 PC
XANTAR® Polycarbonate & Blends, your global partner for innovative added value
ISO 1043 PC
XANTAR® Polycarbonate & Blends, your global partner for innovative added value
| Propiedades reológicas | Valor | Unidades | Método de ensayo |
| Indice de fluidez volumétrico, MVR | 4 | cm³/10min | ISO 1133 |
| Temperatura | 280 | °C | ISO 1133 |
| Carga | 1.2 | kg | ISO 1133 |
| Contracción posterior al moldeo, paralelo | 0.6 | % | ISO 294-4, 2577 |
| Propiedades mecánicas | Valor | Unidades | Método de ensayo |
| Módulo de tracción | 2100 | MPa | ISO 527-1/-2 |
| Esfuerzo de fluencia | 52 | MPa | ISO 527-1/-2 |
| Alarg. en límite elástico | 6 | % | ISO 527-1/-2 |
| Alarg. nominal a rotura | >50 | % | ISO 527-1/-2 |
| Perforación - energía, +23°C | 16 | J | ISO 6603-2 |
| Perforación - energía, -30°C | 16 | J | ISO 6603-2 |
| Propiedades térmicas | Valor | Unidades | Método de ensayo |
| Estabilidad al calor, 1.80 MPa | 129 | °C | ISO 75-1/-2 |
| Temp. reblandecimiento Vicat, 50°C/h 50N | 140 | °C | ISO 306 |
| Coef.de expansión térmica lineal, paralelo | 65 | E-6/K | ISO 11359-1/-2 |
| Propiedades eléctricas | Valor | Unidades | Método de ensayo |
| Resistencia dieléctrica | 18 | kV/mm | IEC 60243-1 |
| Otras propiedades | Valor | Unidades | Método de ensayo |
| Densidad | 1180 | kg/m³ | ISO 1183 |
| Cálculo propiedades reológicas | Valor | Unidades | Método de ensayo |
| Densidad de fusión | 1010 | kg/m³ | - |
| Conductibilidad termica de fusión | 0.24 | W/(m K) | - |
| Calor especifico de la masa | 1710 | J/(kg K) | - |
| Difusibidad termica | 1.4E-7 | m²/s | - |
| Temperatura de expulsión | 131 | °C | - |
| Condiciones de transformación | Valor | Unidades | Método de ensayo |
| Moldeo por inyección, temperatura de la masa | 280 | °C | ISO 294 |
| Moldeo por inyección, temperatura del molde | 80 | °C | ISO 10724 |
Funciones
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Aditivos
Desmoldeante
Disponibilidad regional
Aviso
All information supplied by or on behalf of Mitsubishi Engineering-Plastics Corporation in relation to its products, whether in the nature of data, recommendations or otherwise, is supported by research and, in good faith, believed reliable, but Mitsubishi Engineering-Plastics Corporation assumes no liability and makes no warranties of any kind, express or implied, including, but not limited to, those of title, merchantability, fitness for a particular purpose or non-infringement or any warranty arising from a course of dealing, usage, or trade practice whatsoever in respect of application, processing or use made of the aforementioned information or product. The user assumes all responsibility for the use of all information provided and shall verify quality and other properties or any consequence from the use of all such information. Typical values are indicative only and are not to be construed as being binding specifications.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.