CAMPUS® datasheet | Zytel® EFE7374 BK416
This datasheet of Zytel® EFE7374 BK416 from DuPont Engineering Polymers is provided by the international plastics database CAMPUS.
Zytel® EFE7374 BK416 | PA6-I-GF40 | DuPont Engineering Polymers
Texto del producto
Common features of Zytel® nylon resin include mechanical and physical properties such as high mechanical strength, excellent balance of stiffness and toughness, good high temperature performance, good electrical and flammability properties, good abrasion and chemical resistance. In addition, Zytel® nylon resins are available in different modified and reinforced grades to create a wide range of products with tailored properties for specific processes and end-uses. Zytel® nylon resin, including
most flame retardant grades, offer the ability to be coloured.
The good melt stability of Zytel® nylon resin normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-31kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.
Zytel® nylon resin typically is used in demanding applications in the automotive, furniture, domestic appliances, sporting goods and construction industry.
Zytel® EFE7374 is a 40% fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for injection molding. It has an improved impact resistance and excellent surface appearance and gloss.
| Propiedades reológicas | Seco / Cond | Unidades | Método de ensayo |
| Contracción posterior al moldeo, paralelo | 0.2 / * | % | ISO 294-4, 2577 |
| Contracción posterior al moldeo, normal | 0.6 / * | % | ISO 294-4, 2577 |
| Propiedades mecánicas | Seco / Cond | Unidades | Método de ensayo |
| Módulo de tracción | 12000 / 7500 | MPa | ISO 527-1/-2 |
| Resistencia a la tracción | 190 / 130 | MPa | ISO 527-1/-2 |
| Alargamiento a rotura | 3.5 / 7.5 | % | ISO 527-1/-2 |
| Resistencia al impacto Charpy, +23°C | 110 / 113 | kJ/m² | ISO 179/1eU |
| Resistencia al impacto Charpy, -30°C | 118 / 105 | kJ/m² | ISO 179/1eU |
| Res. impacto Charpy c/entalla, +23°C | 24 / 33 | kJ/m² | ISO 179/1eA |
| Propiedades térmicas | Seco / Cond | Unidades | Método de ensayo |
| Temperatura de fusión, 10°C/min | 221 / * | °C | ISO 11357-1/-3 |
| Estabilidad al calor, 1.80 MPa | 212 / * | °C | ISO 75-1/-2 |
| Otras propiedades | Seco / Cond | Unidades | Método de ensayo |
| Absorción de agua | 5.4 / * | % | Sim. to ISO 62 |
| Absorción de humedad | 1.7 / * | % | Sim. to ISO 62 |
| Densidad | 1410 / - | kg/m³ | ISO 1183 |
| Propiedades específicas del material | Seco / Cond | Unidades | Método de ensayo |
| Indice de viscosidad | 115 / * | cm³/g | ISO 307, 1157, 1628 |
Funciones
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Características especiales
Estable contra el calor
Disponibilidad regional
Resistencia a medios químicos
| Soluciones de sal | |
![]() | Solución de cloruro de cinc (50% por masa) (23°C) |
Aviso
All data provided according to ISO 10350 for single points and ISO 11403 for multipoints.
Contact DuPont for Material Safety Data Sheet, general guides and/or additional information about ventilation, handling, purging, drying, etc.
Test temperatures are 23°C unless otherwise stated.
The DuPont Oval Logo, DuPont™, The miracles of science™ and ® are trademarks or registered trademarks of DuPont Company.
Copyright© 2011 E.I. du Pont de Nemours and Company. All Rights Reserved.
The information provided in this data sheet corresponds to our knowledge on the subject at the date of its publication.
This information may be subject to revision as new knowledge and experience becomes available.
The data provided fall within the normal range of product properties and relate only to the specific material designated; these data may not be
valid for such material used in combination with any other materials, additives or pigments or in any process, unless expressly indicated otherwise.
The data provided should not be used to establish specification limits or used alone as the basis of design; they are not intended to substitute
for any testing you may need to conduct to determine for yourself the suitability of a specific material for your particular purposes.
Since DuPont cannot anticipate all variations in actual end-use conditions DuPont makes no warranties and assumes no liability in connection
with any use of this information.
Nothing in this publication is to be considered as a license to operate under or a recommendation to infringe any patent rights.
DuPont advises you to seek independent counsel for a freedom to practice opinion on the intended application or end-use of our products.
CAUTION: DO NOT USE DUPONT MATERIALS IN MEDICAL APPLICATIONS INVOLVING IMPLANTATION IN THE HUMAN BODY OR
CONTACT WITH INTERNAL BODY FLUIDS OR TISSUES UNLESS THE MATERIAL HAS BEEN PROVIDED FROM DUPONT UNDER A
WRITTEN CONTRACT THAT IS CONSISTENT WITH DUPONT POLICY REGARDING MEDICAL APPLICATIONS AND EXPRESSLY
ACKNOWLEDGES THE CONTEMPLATED USE.
For further information, please contact your DuPont representative. You may also request a copy of DuPont POLICY Regarding Medical
Applications... H-50103-3 and DuPont CAUTION Regarding Medical Applications... H-50102-3.
Contact DuPont for Material Safety Data Sheet, general guides and/or additional information about ventilation, handling, purging, drying, etc.
Test temperatures are 23°C unless otherwise stated.
The DuPont Oval Logo, DuPont™, The miracles of science™ and ® are trademarks or registered trademarks of DuPont Company.
Copyright© 2011 E.I. du Pont de Nemours and Company. All Rights Reserved.
The information provided in this data sheet corresponds to our knowledge on the subject at the date of its publication.
This information may be subject to revision as new knowledge and experience becomes available.
The data provided fall within the normal range of product properties and relate only to the specific material designated; these data may not be
valid for such material used in combination with any other materials, additives or pigments or in any process, unless expressly indicated otherwise.
The data provided should not be used to establish specification limits or used alone as the basis of design; they are not intended to substitute
for any testing you may need to conduct to determine for yourself the suitability of a specific material for your particular purposes.
Since DuPont cannot anticipate all variations in actual end-use conditions DuPont makes no warranties and assumes no liability in connection
with any use of this information.
Nothing in this publication is to be considered as a license to operate under or a recommendation to infringe any patent rights.
DuPont advises you to seek independent counsel for a freedom to practice opinion on the intended application or end-use of our products.
CAUTION: DO NOT USE DUPONT MATERIALS IN MEDICAL APPLICATIONS INVOLVING IMPLANTATION IN THE HUMAN BODY OR
CONTACT WITH INTERNAL BODY FLUIDS OR TISSUES UNLESS THE MATERIAL HAS BEEN PROVIDED FROM DUPONT UNDER A
WRITTEN CONTRACT THAT IS CONSISTENT WITH DUPONT POLICY REGARDING MEDICAL APPLICATIONS AND EXPRESSLY
ACKNOWLEDGES THE CONTEMPLATED USE.
For further information, please contact your DuPont representative. You may also request a copy of DuPont POLICY Regarding Medical
Applications... H-50103-3 and DuPont CAUTION Regarding Medical Applications... H-50102-3.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012