Grade Name Family Producer
Akulon® CE-KMV6 PA6-MD30 FR DSM Engineering Plastics
Akulon® F-X9182 PA6 DSM Engineering Plastics
Akulon® F-X9183 PA6 DSM Engineering Plastics
Akulon® F126-C PA6 DSM Engineering Plastics
Akulon® F127 PA6 DSM Engineering Plastics
Akulon® F128 PA6 DSM Engineering Plastics
Akulon® F130 PA6 DSM Engineering Plastics
Akulon® F130-C PA6 DSM Engineering Plastics
Akulon® F130-C1 PA6 DSM Engineering Plastics
Akulon® F130-C2 PA6 DSM Engineering Plastics
Akulon® F130-C3 PA6 DSM Engineering Plastics
Akulon® F130-E1 PA6 DSM Engineering Plastics
Akulon® F132-C1 PA6 DSM Engineering Plastics
Akulon® F132-E2 PA6 DSM Engineering Plastics
Akulon® F136 PA6 DSM Engineering Plastics
Akulon® F136-C PA6 DSM Engineering Plastics
Akulon® F136-C1 PA6 DSM Engineering Plastics
Akulon® F136-DH PA6 DSM Engineering Plastics
Akulon® F136-E1 PA6 DSM Engineering Plastics
Akulon® F136-E2 PA6 DSM Engineering Plastics
Akulon® F150-CZ PA6 DSM Engineering Plastics
Akulon® F160-Z PA6 DSM Engineering Plastics
Akulon® F223-D PA6 DSM Engineering Plastics
Akulon® F223-D /B PA6 DSM Engineering Plastics
Akulon® F230-C PA6 DSM Engineering Plastics
Akulon® F232 PA6 DSM Engineering Plastics
Akulon® F232-D PA6 DSM Engineering Plastics
Akulon® F234-C PA6 DSM Engineering Plastics
Akulon® F236-C PA6 DSM Engineering Plastics
Akulon® F249-HG4 PA6-GF20 DSM Engineering Plastics
Akulon® Fuel Lock FL-LP PA6 DSM Engineering Plastics
Akulon® K-X04832 PA6-(GF+MD)30 DSM Engineering Plastics
Akulon® K222-D PA6 DSM Engineering Plastics
Akulon® K222-DL PA6 DSM Engineering Plastics
Akulon® K222-KGMV14 PA6-(GF+MD)25 FR(30) DSM Engineering Plastics
Akulon® K222-KGMV15 PA6-(GF+MD)30 FR DSM Engineering Plastics
Akulon® K222-KGV4 PA6-GF20 FR(30) DSM Engineering Plastics
Akulon® K222-KGV4 /A PA6-GF20 FR(30) DSM Engineering Plastics
Akulon® K222-KGV6 PA6-GF30 FR DSM Engineering Plastics
Akulon® K222-KMV5 PA6-MD25 FR(30) DSM Engineering Plastics
Akulon® K222-KMV5 /A PA6-MD25 FR(30) DSM Engineering Plastics
Akulon® K222-KWGV4 PA6-GF20 FR(30) DSM Engineering Plastics
Akulon® K223-HGM24 PA6-(GF+MD)30 DSM Engineering Plastics
Akulon® K223-HM6 PA6-MD30 DSM Engineering Plastics
Akulon® K223-KMV6 PA6-MD30 FR(17) DSM Engineering Plastics
Akulon® K223-P2 PA6-I DSM Engineering Plastics
Akulon® K224-G0 PA6-GF50 DSM Engineering Plastics
Akulon® K224-G3 PA6-GF15 DSM Engineering Plastics
Akulon® K224-G4U PA6-GF23 DSM Engineering Plastics
Akulon® K224-G6 PA6-GF30 DSM Engineering Plastics
Akulon® K224-G6U PA6-GF33 DSM Engineering Plastics
Akulon® K224-G8 PA6-GF40 DSM Engineering Plastics
Akulon® K224-HG0 PA6-GF50 DSM Engineering Plastics
Akulon® K224-HG3 PA6-GF15 DSM Engineering Plastics
Akulon® K224-HG4 PA6-GF20 DSM Engineering Plastics
Akulon® K224-HG6 PA6-GF30 DSM Engineering Plastics
Akulon® K224-HG6U PA6-GF33 DSM Engineering Plastics
Akulon® K224-HG7 PA6-GF35 DSM Engineering Plastics
Akulon® K224-HG8 PA6-GF40 DSM Engineering Plastics
Akulon® K224-HGM35 PA6-(GF+MD)40 DSM Engineering Plastics
Akulon® K224-HGR24 PA6-(GF+GB)30 DSM Engineering Plastics
Akulon® K224-HPG3 PA6-I-GF15 DSM Engineering Plastics
Akulon® K224-KG6 PA6-GF30 DSM Engineering Plastics
Akulon® K224-LG0 PA6-GF50 DSM Engineering Plastics
Akulon® K224-LG4U PA6-GF22 DSM Engineering Plastics
Akulon® K224-LG6 PA6-GF30 DSM Engineering Plastics
Akulon® K224-LG6 /E PA6-GF30 DSM Engineering Plastics
Akulon® K224-LGM35 PA6-(GF+MD)40 DSM Engineering Plastics
Akulon® K224-PG2 PA6-I-GF8 DSM Engineering Plastics
Akulon® K224-PG3 PA6-I-GF15 DSM Engineering Plastics
Akulon® K224-PG6 PA6-I-GF30 DSM Engineering Plastics
Akulon® K224-PG8 PA6-I-GF40 DSM Engineering Plastics
Akulon® K224-TG9 PA6-GF45 DSM Engineering Plastics
Akulon® K224-TG9/A PA6-GF45 DSM Engineering Plastics
Akulon® K225-KS PA6 FR(30) DSM Engineering Plastics
Akulon® K225-KV PA6 FR(30) DSM Engineering Plastics
Akulon® K225-KWS PA6 FR(30) DSM Engineering Plastics
Akulon® K240-HPG3 PA6-I-GF15 DSM Engineering Plastics
Akulon® N22D PA6 DSM Engineering Plastics
Akulon® N24-G6 PA6-GF30 DSM Engineering Plastics
Akulon® N24-G7 PA6-GF35 DSM Engineering Plastics
Akulon® N24-LG6 PA6-GF30 DSM Engineering Plastics
Akulon® N24-LG6U PA6-GF30 DSM Engineering Plastics
Akulon® Ultraflow K-FG0 PA6-GF50 DSM Engineering Plastics
Akulon® Ultraflow K-FG12 PA6-GF60 DSM Engineering Plastics
Akulon® Ultraflow K-FG3 PA6-GF15 DSM Engineering Plastics
Akulon® Ultraflow K-FG5 PA6-GF25 DSM Engineering Plastics
Akulon® Ultraflow K-FG6 PA6-GF30 DSM Engineering Plastics
Akulon® Ultraflow K-FG7 PA6-GF35 DSM Engineering Plastics
Akulon® Ultraflow K-FG8 PA6-GF40 DSM Engineering Plastics
Akulon® Ultraflow K-FG9 PA6-GF45 DSM Engineering Plastics
Akulon® Ultraflow K-FHG0 PA6-GF50 DSM Engineering Plastics
Akulon® Ultraflow K-FHG12 PA6-GF60 DSM Engineering Plastics
Akulon® Ultraflow K-FHG6 PA6-GF30 DSM Engineering Plastics
Akulon® Ultraflow K-FHG6 /A PA6-GF30 DSM Engineering Plastics
Akulon® Ultraflow K-FHG7 PA6-GF35 DSM Engineering Plastics
Akulon® Ultraflow K-FHG8 PA6-GF40 DSM Engineering Plastics
Akulon® Ultraflow K-FHGM35 PA6-(GF+MD)40 DSM Engineering Plastics
Akulon® Ultraflow K-FHGR24 PA6-(GF+GB)30 DSM Engineering Plastics
Akulon® Ultraflow K-FKGS6 /B PA6-GF30 FR(17) DSM Engineering Plastics
Akulon® Ultraflow K-FKGV4 /A PA6-GF20 FR DSM Engineering Plastics
Akulon® Ultraflow K-FKMV5 PA6-MD25 FR(30) DSM Engineering Plastics
Akulon® Ultraflow K-FKMV5 /C PA6-MD25 DSM Engineering Plastics
Akulon® Ultraflow K-FLG6/E PA6-GF30 DSM Engineering Plastics
Akulon® Ultraflow K-FPG8 PA6-I-GF40 DSM Engineering Plastics
Akulon® Ultraflow K220-HGM44 PA6-(GF+MD)40 DSM Engineering Plastics
Akulon® XG-FKGS6 PA6-GF30 FR DSM Engineering Plastics
Akulon® XP32-C1 PA6 DSM Engineering Plastics
Akulon® XP32-E1 PA6 DSM Engineering Plastics
Akulon® XP36-C1 PA6 DSM Engineering Plastics
Akulon® XP36-D1H PA6 DSM Engineering Plastics
Akulon® XP36-E1 PA6 DSM Engineering Plastics
ALCOM® PA6 900/1 CF10 GF25 IM PA6-I-(GF+CF)35 ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF10 GB20 PA6-(GF+GB)30 ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF10 MR20 PA6-(GF+MX)30 ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF10 MR30 PA6-(GF+MX)40 ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF15 GB15 PA6-(GF+GB)30 ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF15 MR25 PA6-(GF+MX)40 ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF15 MR25 UV PA6-(GF+MX)40 ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF20 MR25 PA6-(GF+MX)45 ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF30 MO2 PA6-GF... ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF30 PTFE15 Si2 (PA6+PTFE)-GF... ALBIS Plastic GmbH
ALCOM® PA6 900/1 GF5 GB25 PA6-(GF+GB)30 ALBIS Plastic GmbH
ALCOM® PA6 900/1 MO1 PA6... ALBIS Plastic GmbH
ALCOM® PA6 900/1 PTFE10 IM (PA6+PTFE)-I ALBIS Plastic GmbH
ALCOM® PA6 900/1 Si3 PA6... ALBIS Plastic GmbH
ALCOM® PA6 900/11 GF10 MR20 PA6-I-(GF+MX)30 ALBIS Plastic GmbH
ALCOM® PA6 900/11 GF10 MR20 MCF PA6-(GF+MX)30 ALBIS Plastic GmbH
ALCOM® PA6 900/11 GF30 RD1303-06MCF PA6-GF30 ALBIS Plastic GmbH
ALCOM® PA6 900/11 GF30 SV 12-778MCF PA6-GF30 ALBIS Plastic GmbH
ALCOM® PA6 900/30.1 TCE10 PA6... ALBIS Plastic GmbH
ALCOM® PA6 900/7 GF15 PTFE10 (PA6+PTFE)-GF15 ALBIS Plastic GmbH
ALCOM® PA6 900/8 GF10 MR20 PA6-(GF+MX)30 ALBIS Plastic GmbH
ALCOM® PA6 900/8 GF10 MR20 IM PA6-I-(GF+MX)30 ALBIS Plastic GmbH
ALCOM® PA6 900/8 SV 1403-04 MCF PA6 ALBIS Plastic GmbH
ALCOM® PA6 99/0701 EC PA6-CD ALBIS Plastic GmbH
ALTECH 6 PA 1461 Z 2 PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 1000/107 PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/108 PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/109 PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/110 IM PA6-I ALBIS Plastic GmbH
ALTECH PA6 A 1000/120 UV PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/126 UV PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/149 FR PA6 FR ALBIS Plastic GmbH
ALTECH PA6 A 1000/310 IM PA6-I ALBIS Plastic GmbH
ALTECH PA6 A 1000/316 IM PA6-I ALBIS Plastic GmbH
ALTECH PA6 A 1000/506 HV PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/510 IM PA6-I ALBIS Plastic GmbH
ALTECH PA6 A 1000/518 IM PA6-I ALBIS Plastic GmbH
ALTECH PA6 A 1000/520 UV HV PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/586 PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/700 PA6 ALBIS Plastic GmbH
ALTECH PA6 A 1000/716 IM PA6-I ALBIS Plastic GmbH
ALTECH PA6 A 2003/710 GF3 IM PA6-I-GF3 ALBIS Plastic GmbH
ALTECH PA6 A 2010/100 GF10 PA6-GF10 ALBIS Plastic GmbH
ALTECH PA6 A 2015/109 GF15 PA6-GF15 ALBIS Plastic GmbH
ALTECH PA6 A 2015/210 GF15 IM PA6-I-GF15 ALBIS Plastic GmbH
ALTECH PA6 A 2015/220 GF15 UV PA6-GF15 ALBIS Plastic GmbH
ALTECH PA6 A 2015/310 GF15 IM PA6-I-GF15 ALBIS Plastic GmbH
ALTECH PA6 A 2015/321 GF15 UV IM PA6-I-GF15 ALBIS Plastic GmbH
ALTECH PA6 A 2015/610 GF15 IM PA6-I-GF15 ALBIS Plastic GmbH
ALTECH PA6 A 2015/710 GF15 IM PA6-I-GF15 ALBIS Plastic GmbH
ALTECH PA6 A 2020/109 GF20 PA6-GF20 ALBIS Plastic GmbH
ALTECH PA6 A 2025/109 GF25 PA6-GF25 ALBIS Plastic GmbH
ALTECH PA6 A 2030/109 GF30 PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2030/209 GF30 PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2030/212 GF30 IM UV PA6-I-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2030/319 GF30 IM PA6-I-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2030/320 GF30 UV PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2030/577 GF30 PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2030/586 GF30 PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2030/587 GF30 PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2030/610 GF30 IM PA6-I-GF30 ALBIS Plastic GmbH
ALTECH PA6 A 2035/109 GF35 PA6-GF35 ALBIS Plastic GmbH
ALTECH PA6 A 4030/109 MR30 PA6-MX30 ALBIS Plastic GmbH
ALTECH PA6 A 4030/210 MR30 PA6-MX30 ALBIS Plastic GmbH
ALTECH PA6 A 4040/100 MR40 PA6-MX40 ALBIS Plastic GmbH
ALTECH PA6 B 1000/109 PA6 ALBIS Plastic GmbH
ALTECH PA6 B 1000/209 PA6 ALBIS Plastic GmbH
ALTECH PA6 B 1000/509 PA6 ALBIS Plastic GmbH
ALTECH PA6 B 2015/100 GF15 PA6-GF15 ALBIS Plastic GmbH
ALTECH PA6 B 2015/106 GF15 PA6-GF15 ALBIS Plastic GmbH
ALTECH PA6 B 2025/309 GF25 PA6-GF25 ALBIS Plastic GmbH
ALTECH PA6 B 2030/209 GF30 PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 C 2030/100 GF30 PA6-GF30 ALBIS Plastic GmbH
ALTECH PA6 C 2030/119 GF30 IM PA6-I-GF30 ALBIS Plastic GmbH
ALTECH PA6 C 2030/219 GF30 IM PA6-I-GF30 ALBIS Plastic GmbH
ALTECH PA6 C 3030/100 GB30 PA6-GB30 ALBIS Plastic GmbH
ALTECH PA6 C 3030/320 GB30 UV PA6-GB30 ALBIS Plastic GmbH
ALTECH PA6 C 3230/100 GB20 GF10 PA6-(GB+GF)30 ALBIS Plastic GmbH
ALTECH PA6 C 4230/100 GF10 MR20 PA6-(GF+MX)30 ALBIS Plastic GmbH
ALTECH PA6+ASA A 1000/220 UV (PA6+ASA) ALBIS Plastic GmbH
ALTECH PA6+ASA A 1000/312 UV IM (PA6+ASA)-I ALBIS Plastic GmbH
ALTECH PA6+ASA A 4010/220 MR10 (PA6+ASA)-MX10 ALBIS Plastic GmbH
ALTECH PA6+ASA A4010221MR10UV IM (PA6+ASA)-I-MX10 ALBIS Plastic GmbH
ALTECH PA6+PA666 A2030/100GF30IM (PA6+PA666)-I-GF30 ALBIS Plastic GmbH
ALTECH PA66+PA6 A 1000/567 (PA66+PA6) ALBIS Plastic GmbH
BERGAMID® B70/75/80 PA6 PolyOne Engineered Materials Europe
BERGAMID® B70/80G/GK30TM-Y PA6-(GF+GB)30 PolyOne Engineered Materials Europe
BERGAMID® B70/80G10TM-X PA6-GF10 PolyOne Engineered Materials Europe
BERGAMID® B70/80G15TM-Y PA6-GF15 PolyOne Engineered Materials Europe
BERGAMID® B70/80G15TM-Z PA6-GF15 PolyOne Engineered Materials Europe
BERGAMID® B70/80G30TM-X PA6-GF30 PolyOne Engineered Materials Europe
BERGAMID® B70/80G30TM-Y PA6-GF30 PolyOne Engineered Materials Europe
BERGAMID® B70/80G30TM-Z PA6-GF30 PolyOne Engineered Materials Europe
BERGAMID® B70/80PM-Y PA6 PolyOne Engineered Materials Europe
BERGAMID® B70/80PM-Z PA6 PolyOne Engineered Materials Europe
BERGAMID® B70/80TM-X PA6 PolyOne Engineered Materials Europe
BERGAMID® B70/80TM-Y PA6 PolyOne Engineered Materials Europe
BERGAMID® B70/80TM-Z PA6 PolyOne Engineered Materials Europe
BERGAMID® B70/80UF PA6 PolyOne Engineered Materials Europe
BERGAMID® B700-20 PA6 PolyOne Engineered Materials Europe
BERGAMID® B700/750/800 PA6 PolyOne Engineered Materials Europe
BERGAMID® B700G/GK30 PA6-(GF+GB)30 PolyOne Engineered Materials Europe
BERGAMID® B700G/GK30H PA6-(GF+GB)30 PolyOne Engineered Materials Europe
BERGAMID® B700G10H PA6-GF10 PolyOne Engineered Materials Europe
BERGAMID® B700G15H PA6-GF15 PolyOne Engineered Materials Europe
BERGAMID® B700G20H PA6-GF20 PolyOne Engineered Materials Europe
BERGAMID® B700G25H PA6-GF25 PolyOne Engineered Materials Europe
BERGAMID® B700G30H PA6-GF30 PolyOne Engineered Materials Europe
BERGAMID® B700G30TM-Z PA6-GF30 PolyOne Engineered Materials Europe
BERGAMID® B700G35H PA6-GF35 PolyOne Engineered Materials Europe
BERGAMID® B700G40H PA6-GF40 PolyOne Engineered Materials Europe
BERGAMID® B700G45H PA6-GF45 PolyOne Engineered Materials Europe
BERGAMID® B700G50H PA6-GF50 PolyOne Engineered Materials Europe
BERGAMID® B700UF PA6 PolyOne Engineered Materials Europe
BERGAMID® B700W25 PA6 PolyOne Engineered Materials Europe
BERGAMID® B70G/GK30 PA6-(GF+GB)30 PolyOne Engineered Materials Europe
BERGAMID® B70G/GK30UF PA6-(GF+GB)30 PolyOne Engineered Materials Europe
BERGAMID® B70G/MI30U PA6-(GF+MD)30 PolyOne Engineered Materials Europe
BERGAMID® B70G10 PA6-GF10 PolyOne Engineered Materials Europe
BERGAMID® B70G10/MI20 PA6-(GF+MD)30 PolyOne Engineered Materials Europe
BERGAMID® B70G15 PA6-GF15 PolyOne Engineered Materials Europe
BERGAMID® B70G15PM-Z PA6-GF15 PolyOne Engineered Materials Europe
BERGAMID® B70G20 PA6-GF20 PolyOne Engineered Materials Europe
BERGAMID® B70G25 PA6-GF25 PolyOne Engineered Materials Europe
BERGAMID® B70G25TM-Z PA6-GF25 PolyOne Engineered Materials Europe
BERGAMID® B70G30 PA6-GF30 PolyOne Engineered Materials Europe
BERGAMID® B70G35 PA6-GF35 PolyOne Engineered Materials Europe
BERGAMID® B70G40 PA6-GF40 PolyOne Engineered Materials Europe
BERGAMID® B70G45 PA6-GF45 PolyOne Engineered Materials Europe
BERGAMID® B70G50 PA6-GF50 PolyOne Engineered Materials Europe
BERGAMID® B70GK30 PA6-GB30 PolyOne Engineered Materials Europe
BERGAMID® B70GK30UF PA6-GB30 PolyOne Engineered Materials Europe
BERGAMID® B70L PA6 PolyOne Engineered Materials Europe
BERGAMID® B70MI20 PA6-MD20 PolyOne Engineered Materials Europe
BERGAMID® B70MI25UF PA6-MD25 PolyOne Engineered Materials Europe
BERGAMID® B70MI30 PA6-MD30 PolyOne Engineered Materials Europe
BERGAMID® B70MI30TM-X PA6-MD30 PolyOne Engineered Materials Europe
BERGAMID® B70MOS2 PA6 PolyOne Engineered Materials Europe
BERGAMID® B70NATUR 50 PA6 PolyOne Engineered Materials Europe
BERGAMID® B70W25 PA6 PolyOne Engineered Materials Europe
BERGAMID® B70W25G30 PA6-GF30 PolyOne Engineered Materials Europe
BERGAMID® B80NATUR 90 PA6 PolyOne Engineered Materials Europe
CELSTRAN PA6-GF30-01 PA6-GF30 Ticona
CELSTRAN PA6-GF40-01 PA6-GF40 Ticona
CELSTRAN PA6-GF40-03 PA6-GF40 Ticona
CELSTRAN PA6-GF50-01 PA6-GF50 Ticona
CELSTRAN PA6-GF50-03 PA6-GF50 Ticona
CELSTRAN PA6-GF60-01 PA6-GF60 Ticona
CELSTRAN PA6-GF60-03 PA6-GF60 Ticona
Durethan® B 30 S PA6 LANXESS Deutschland GmbH
Durethan® B 30 S F30 PA6 FR LANXESS Deutschland GmbH
Durethan® B 30 S FN40 PA6 LANXESS Deutschland GmbH
Durethan® B 31 F PA6 LANXESS Deutschland GmbH
Durethan® B 31 SK PA6 LANXESS Deutschland GmbH
Durethan® B 35 F PA6 LANXESS Deutschland GmbH
Durethan® B 35 FA PA6 LANXESS Deutschland GmbH
Durethan® B 35 FKA PA6 LANXESS Deutschland GmbH
Durethan® B 38 FKA PA6 LANXESS Deutschland GmbH
Durethan® B 40 E PA6 LANXESS Deutschland GmbH
Durethan® B 40 F PA6 LANXESS Deutschland GmbH
Durethan® B 40 FA PA6 LANXESS Deutschland GmbH
Durethan® B 40 FAM PA6 LANXESS Deutschland GmbH
Durethan® B 40 FKA PA6 LANXESS Deutschland GmbH
Durethan® B 40 SK PA6 LANXESS Deutschland GmbH
Durethan® BC 30 PA6 LANXESS Deutschland GmbH
Durethan® BC 304 H3.0 PA6 LANXESS Deutschland GmbH
Durethan® BC 40 SR2 PA6 LANXESS Deutschland GmbH
Durethan® BC 700 HTS PA6-I LANXESS Deutschland GmbH
Durethan® BCF 30X H2.0 PA6-(GF+CF)30 LANXESS Deutschland GmbH
Durethan® BG 30 X PA6-(GF+GB)30 LANXESS Deutschland GmbH
Durethan® BG 30 X H2.0 PA6-(GF+GB)30 LANXESS Deutschland GmbH
Durethan® BG 30 X H3.0 PA6-(GF+GB)30 LANXESS Deutschland GmbH
Durethan® BG 30X W1 PA6-(GF+GB)30 LANXESS Deutschland GmbH
Durethan® BKV 115 PA6-GF15 LANXESS Deutschland GmbH
Durethan® BKV 115 H2.0 PA6-GF15 LANXESS Deutschland GmbH
Durethan® BKV 130 PA6-GF30 LANXESS Deutschland GmbH
Durethan® BKV 130 GIT PA6-GF30 LANXESS Deutschland GmbH
Durethan® BKV 130 H2.0 PA6-GF30 LANXESS Deutschland GmbH
Durethan® BKV 130 H3.0 PA6-GF30 LANXESS Deutschland GmbH
Durethan® BKV 140 PA6-GF40 LANXESS Deutschland GmbH
Durethan® BKV 140 H2.0 PA6-GF40 LANXESS Deutschland GmbH
Durethan® BKV 15 PA6-GF15 LANXESS Deutschland GmbH
Durethan® BKV 15 G H2.0 PA6-GF15 LANXESS Deutschland GmbH
Durethan® BKV 15 H2.0 PA6-GF15 LANXESS Deutschland GmbH
Durethan® BKV 15 H3.0 PA6-GF15 LANXESS Deutschland GmbH
Durethan® BKV 20 FN00 PA6-GF18 LANXESS Deutschland GmbH
Durethan® BKV 20 FN20 PA6-GF20 FR LANXESS Deutschland GmbH
Durethan® BKV 215 PA6-I-GF15 LANXESS Deutschland GmbH
Durethan® BKV 215 H2.0 PA6-I-GF15 LANXESS Deutschland GmbH
Durethan® BKV 215 H3.0 PA6-I-GF15 LANXESS Deutschland GmbH
Durethan® BKV 215 W1 PA6-I-GF15 LANXESS Deutschland GmbH
Durethan® BKV 230 H2.0 PA6-GF30 LANXESS Deutschland GmbH
Durethan® BKV 25 H2.0 LT PA6-GF25 LANXESS Deutschland GmbH
Durethan® BKV 25 H3.0 PA6-GF25 LANXESS Deutschland GmbH
Durethan® BKV 30 PA6-GF LANXESS Deutschland GmbH
Durethan® BKV 30 EF PA6-GF30 LANXESS Deutschland GmbH
Durethan® BKV 30 FN00 PA6-GF LANXESS Deutschland GmbH
Durethan® BKV 30 G H2.0 PA6-GF30 LANXESS Deutschland GmbH
Durethan® BKV 30 G W1 PA6-GF30 LANXESS Deutschland GmbH
Durethan® BKV 30 H2.0 PA6-GF30 LANXESS Deutschland GmbH
Durethan® BKV 30 H2.0 EF PA6-GF30 LANXESS Deutschland GmbH
Durethan® BKV 30 H3.0 PA6-GF30 LANXESS Deutschland GmbH
Durethan® BKV 30 HTS PA6-GF30 LANXESS Deutschland GmbH
Durethan® BKV 30 W1 PA6-GF30 LANXESS Deutschland GmbH
Durethan® BKV 315 Z H2.0 PA6-GF15 LANXESS Deutschland GmbH
Durethan® BKV 325 Z H2.0 PA6-I-GF25 LANXESS Deutschland GmbH
Durethan® BKV 330 H2.0 PA6-GF30 LANXESS Deutschland GmbH
Durethan® BKV 35 CX H2.0 PA6-GF35 LANXESS Deutschland GmbH
Durethan® BKV 35 H2.0 PA6-GF35 LANXESS Deutschland GmbH
Durethan® BKV 35 H2.0 EF PA6-GF35 LANXESS Deutschland GmbH
Durethan® BKV 35 HTS PA6-GF35 LANXESS Deutschland GmbH
Durethan® BKV 40 H2.0 PA6-GF40 LANXESS Deutschland GmbH
Durethan® BKV 50 H EF DUS022 PA6-GF50 LANXESS Deutschland GmbH
Durethan® BKV 50 H2.0 PA6-GF50 LANXESS Deutschland GmbH
Durethan® BKV 50 H2.0 EF PA6-GF50 LANXESS Deutschland GmbH
Durethan® BKV 50 H3.0 PA6-GF50 LANXESS Deutschland GmbH
Durethan® BM 240 PA6-MD40 LANXESS Deutschland GmbH
Durethan® BM 240 H2.0 PA6-MD40 LANXESS Deutschland GmbH
Durethan® BM 240 H3.0 PA6-MD40 LANXESS Deutschland GmbH
Durethan® BM 25 FN20 PA6-MX25 FR LANXESS Deutschland GmbH
Durethan® BM 25 FN20 DUS013 PA6-MX25 FR LANXESS Deutschland GmbH
Durethan® BM 40 X H2.0 DUS009 PA6-(GF+MD)40 LANXESS Deutschland GmbH
Durethan® C 38 FA PA6 LANXESS Deutschland GmbH
Durethan® C 38 FKAM PA6 LANXESS Deutschland GmbH
Durethan® CI 31 F PA6 LANXESS Deutschland GmbH
Durethan® DP 1100/30 H2.0 PA6-GB30 LANXESS Deutschland GmbH
Durethan® DP 1441/40 H2.0 EF PA6-(GF+MD)40 LANXESS Deutschland GmbH
Durethan® DP 1801/30 H3.0 PA6-GF30 FR LANXESS Deutschland GmbH
Durethan® DP 1802 H3.0 PA6 FR LANXESS Deutschland GmbH
Durethan® DP 1852/30 PA6-GF30 FR LANXESS Deutschland GmbH
Durethan® DP 2037/30 H2.0 LT PA6-GF30 LANXESS Deutschland GmbH
Durethan® DP 2131/20 H2.0 PA6-GF20 LANXESS Deutschland GmbH
Durethan® DP 2131/20 W1 PA6-GF20 LANXESS Deutschland GmbH
Durethan® DP BC 310 EF PA6 LANXESS Deutschland GmbH
Durethan® DP BC 500 H2.0 PA6 LANXESS Deutschland GmbH
Durethan® DP BC 600 HTS PA6 LANXESS Deutschland GmbH
Durethan® DP BKV 240 H2.0 PA6-GF40 LANXESS Deutschland GmbH
Durethan® DP BKV 30 XF PA6-GF30 LANXESS Deutschland GmbH
Durethan® DP BKV 35 XF PA6-GF35 LANXESS Deutschland GmbH
Durethan® DP BKV 60 EF PA6-GF60 LANXESS Deutschland GmbH
Durethan® DP BKV 60 H2.0 EF PA6-GF60 LANXESS Deutschland GmbH
Durethan® DP BM 29 X H2.0 EF PA6-(GF+MD)30 LANXESS Deutschland GmbH
Durethan® DP BM 410 H2.0 PA6-(GF+MD)10 LANXESS Deutschland GmbH
Durethan® DP BM 65 X FM30 PA6-(MD+GF)65 FR LANXESS Deutschland GmbH
Durethan® ECO BV 30 H2 PA6-GF30 LANXESS Deutschland GmbH
Durethan® ECO BV 35 H2 PA6-GF35 LANXESS Deutschland GmbH
Durethan® ECO PA GF 30 PA6-GF30 LANXESS Deutschland GmbH
Grilon B 70 GFE 15 H PA6-GF15 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon B 70 GFE 30 H PA6-GF30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BFZ 3 PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-15 PA6-GF15 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-15 HM PA6-GF15 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-15 S PA6-GF15 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-15/2 PA6-GF15 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-25 HM PA6-GF25 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-25 S PA6-GF25 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-30 PA6-GF30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-30 EC PA6-GF30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-30 FC PA6-GF30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-30 FR PA6-GF30 FR EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-30 HM PA6-GF30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-30 S PA6-GF30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-30 S FA PA6-GF30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-30/2 PA6-GF30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-35 PA6-GF35 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-35 S PA6-GF35 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-40 FC PA6-GF40 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-40 HM PA6-GF40 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-40 S PA6-GF40 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-50 PA6-GF50 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-50 FC PA6-GF50 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-50 H PA6-GF50 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-50 HM PA6-GF50 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-50 S PA6-GF50 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BG-60 FC PA6-GF60 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BGK-30 X PA6-(GF+GB)30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BGM-30 X PA6-(GF+MD)30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BGM-40 X PA6-(GF+MD)40 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BGM-65 X V0 PA6-(GF+MD)65 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BGZ-15 PA6-GF15 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BGZ-15/2 PA6-GF15 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BGZ-30 PA6-GF30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BGZ-30/2 PA6-GF30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BGZ-40 PA6-GF40 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BGZ-50/2 PA6-I-GF50 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BK-30 PA6-GB30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BK-50 PA6-GB50 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BKZ-30 PA6-GB30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BM-30 PA6-MD30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BM-30 FR PA6-MD30 FR EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BM-30/2 PA6-MD30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BR 40 PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BR 40 W PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BRZ 234/1 W PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BRZ 247 W PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BRZ 334 H PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BRZ 340 H PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BRZ 347 W PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BS PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BS 23 PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BS EC PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BS/2 PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BT 40 Z PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BZ 1 PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BZ 1/2 PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon BZ 3 PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon EB 50 H PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon EB 50 H DZ PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon EBV-15H black 9697 PA6-GF15 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon EBV-2H PA6-GF20 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon F 34 NL PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon F 40 NL PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon F 47 H NL nat 6020 PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon F 47 NL nat 6028 PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon F 50 nat 6368 PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon FG 34 NL nat 6023 PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon FG 40 NL nat 6018 PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon FG 40 NL nat 6021 PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon FG 40 NL nat 6025 PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon FG 47 NL nat 6028 PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon R 47 HW 10 PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon R 50 H NZ PA6 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon XE 5026 (BG-30 H) PA6-GF30 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon XE 5031 (BS V0 X) PA6 FR EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon XE 5051 (BGZ-40 FC) PA6-GF40 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Grilon XE 5052 (BGZ-15 FC) PA6-GF15 EMS-GRIVORY - a unit of EMS-CHEMIE AG
Minlon® 73GM40 NC010 PA6-(MD+GF)40 DuPont Engineering Polymers
Minlon® 73M30 NC010 PA6-MD30 DuPont Engineering Polymers
Minlon® 73M40 NC010 PA6-MD40 DuPont Engineering Polymers
Novamid® 1007 PA6 DSM Engineering Plastics
Novamid® 1010C2 PA6 DSM Engineering Plastics
Novamid® 1010GN2-30 PA6-GF30 FR(17) DSM Engineering Plastics
Novamid® 1010N2 1ES PA6 FR(30) DSM Engineering Plastics
Novamid® 1011CH5 2 PA6 DSM Engineering Plastics
Novamid® 1011CH5KR PA6 DSM Engineering Plastics
Novamid® 1013C5 PA6 DSM Engineering Plastics
Novamid® 1013G15 1 PA6-GF15 DSM Engineering Plastics
Novamid® 1013G30 1 PA6-GF30 DSM Engineering Plastics
Novamid® 1013G45 1 PA6-GF45 DSM Engineering Plastics
Novamid® 1013GH15 1 PA6-GF15 DSM Engineering Plastics
Novamid® 1013GH30 1 PA6-GF30 DSM Engineering Plastics
Novamid® 1013GH45 1 PA6-GF45 DSM Engineering Plastics
Novamid® 1013GMF H2 PA6-GF30 DSM Engineering Plastics
Novamid® 1015G35 PA6-GF35 DSM Engineering Plastics
Novamid® 1015GH35 BK37 PA6-GF35 DSM Engineering Plastics
Novamid® 1017GH33 BK701 PA6-GF33 DSM Engineering Plastics
Novamid® ST145 PA6-I DSM Engineering Plastics
Novamid® ST220 PA6-I DSM Engineering Plastics
Orgalloy® LE 6000 PA6... ARKEMA
Orgalloy® LE 60LM PA6... ARKEMA
Orgalloy® LE 60LMXV PA6... ARKEMA
Orgalloy® LE 60THM PA6... ARKEMA
Orgalloy® LT 4060 PA6... ARKEMA
Orgalloy® LT 4060ES noir T6L PA6... ARKEMA
Orgalloy® LT 5050 T6L PA6... ARKEMA
Orgalloy® LT 5050ES noir PA6... ARKEMA
Orgalloy® R 60ES PA6... ARKEMA
Orgalloy® RS 6000 PA6... ARKEMA
Orgalloy® RS 6010 PA6... ARKEMA
Orgalloy® RS 6030 PA6-GF30... ARKEMA
POLYFLAM® RMMK 125 (ABS+PA6) FR... A. Schulman GmbH
RADIFLAM® S AE PA6 FR RadiciPlastics
RADIFLAM® S FR PA6 FR RadiciPlastics
RADIFLAM® S RV250FR PA6-GF25 FR RadiciPlastics
RADIFLAM® S RV300AE PA6-GF30 FR RadiciPlastics
RADILON® CS 35FL PA6 RadiciPlastics
RADILON® CS 38FL PA6 RadiciPlastics
RADILON® CS T PA6 RadiciPlastics
RADILON® CS T 38FL PA6 RadiciPlastics
RADILON® S 32HS PA6 RadiciPlastics
RADILON® S 35FL PA6 RadiciPlastics
RADILON® S 35HR PA6 RadiciPlastics
RADILON® S 38F PA6 RadiciPlastics
RADILON® S 38M PA6-I RadiciPlastics
RADILON® S 40 EP3215 PA6-I RadiciPlastics
RADILON® S 40E PA6 RadiciPlastics
RADILON® S 40FL PA6 RadiciPlastics
RADILON® S CP300 PA6-MX30 RadiciPlastics
RADILON® S CP400 PA6-MX40 RadiciPlastics
RADILON® S CV300 PA6-GB30 RadiciPlastics
RADILON® S ERV3808K PA6-I-MX30 RadiciPlastics
RADILON® S ESL128 PA6-I RadiciPlastics
RADILON® S HS PA6 RadiciPlastics
RADILON® S HSX PA6-I RadiciPlastics
RADILON® S HSX88 PA6-I RadiciPlastics
RADILON® S LHS PA6 RadiciPlastics
RADILON® S LVHPL128 PA6-I RadiciPlastics
RADILON® S RCP3010LK PA6-(GF+MX)30 RadiciPlastics
RADILON® S RCV3015 PA6-(GF+GB)30 RadiciPlastics
RADILON® S RCV3515 PA6-(GF+GB)35 RadiciPlastics
RADILON® S RV150 PA6-GF15 RadiciPlastics
RADILON® S RV200 PA6-GF20 RadiciPlastics
RADILON® S RV250 PA6-GF25 RadiciPlastics
RADILON® S RV300 PA6-GF30 RadiciPlastics
RADILON® S RV300LK PA6-GF30 RadiciPlastics
RADILON® S RV300R PA6-GF30 RadiciPlastics
RADILON® S RV330 PA6-GF33 RadiciPlastics
RADILON® S RV350 PA6-GF35 RadiciPlastics
RADILON® S RV500 PA6-GF50 RadiciPlastics
RADILON® S USX200 PA6-I RadiciPlastics
RADILON® S USZ200 PA6-I RadiciPlastics
SCHULABLEND® (ABS/PA) M/MK (ABS+PA6)... A. Schulman GmbH
SCHULABLEND® (ABS/PA) M/MK 20 GF (ABS+PA6)-GF20... A. Schulman GmbH
SCHULABLEND® (ABS/PA) M/MK 8 GF (ABS+PA6)-GF8 A. Schulman GmbH
SCHULABLEND® (ABS/PA) M/MK K2004 (ABS+PA6) A. Schulman GmbH
SCHULABLEND® (ABS/PA) M/MK NC 800 (ABS+PA6)-MD20 A. Schulman GmbH
SCHULABLEND® (ASA/PA) M/MW (ASA+PA6) A. Schulman GmbH
SCHULABLEND® (ASA/PA) M/MW NC 800 (ASA+PA6)-MD20 A. Schulman GmbH
SCHULABLEND® (ASA/PA) M/MW NC100 SF (ASA+PA6) A. Schulman GmbH
SCHULABLEND® (ASA/PA) M/MW SF UV (ASA+PA6) A. Schulman GmbH
SCHULAMID® 6 GB 10 FR PA6-GB10 FR(30) A. Schulman GmbH
SCHULAMID® 6 GB 15 LS PA6-GB15 A. Schulman GmbH
SCHULAMID® 6 GB 30 PA6-GB30 A. Schulman GmbH
SCHULAMID® 6 GB 30 LS PA6-GB30 A. Schulman GmbH
SCHULAMID® 6 GBF 3010 H PA6-(GB+GF)30 A. Schulman GmbH
SCHULAMID® 6 GBF 3015 FR 4 PA6-(GB+GF)30 FR A. Schulman GmbH
SCHULAMID® 6 GBF 3026 H LW PA6-(GF+GB)30 A. Schulman GmbH
SCHULAMID® 6 GF 15 PA6-GF15 A. Schulman GmbH
SCHULAMID® 6 GF 15 FR 4 K1681 PA6-GF15 FR A. Schulman GmbH
SCHULAMID® 6 GF 15 HI PA6-I-GF15 A. Schulman GmbH
SCHULAMID® 6 GF 15 HI BM PA6-I-GF15 A. Schulman GmbH
SCHULAMID® 6 GF 15 HI K2073 PA6-I-GF15 A. Schulman GmbH
SCHULAMID® 6 GF 15 HV PA6-GF15 A. Schulman GmbH
SCHULAMID® 6 GF 20 H LS PA6-I-GF20 A. Schulman GmbH
SCHULAMID® 6 GF 25 PA6-GF25 A. Schulman GmbH
SCHULAMID® 6 GF 25 FR PA6-GF25 FR A. Schulman GmbH
SCHULAMID® 6 GF 25 FR 2 A PA6-GF25 FR A. Schulman GmbH
SCHULAMID® 6 GF 30 PA6-GF30 A. Schulman GmbH
SCHULAMID® 6 GF 30 FR 2 PA6-GF30 FR A. Schulman GmbH
SCHULAMID® 6 GF 30 FR 4 PA6-GF30 FR A. Schulman GmbH
SCHULAMID® 6 GF 30 FR2A LM PA6-GF30 FR(30+40) A. Schulman GmbH
SCHULAMID® 6 GF 30 GID LS PA6-GF30 A. Schulman GmbH
SCHULAMID® 6 GF 30 GID natur PA6-GF30 A. Schulman GmbH
SCHULAMID® 6 GF 30 H PA6-GF30 A. Schulman GmbH
SCHULAMID® 6 GF 30 H BLACK REC PA6-GF30 A. Schulman GmbH
SCHULAMID® 6 GF 30 H LW PA6-GF30 A. Schulman GmbH
SCHULAMID® 6 GF 30 HI PA6-I-GF30 A. Schulman GmbH
SCHULAMID® 6 GF 30 HI K1871 PA6-I-GF30 A. Schulman GmbH
SCHULAMID® 6 GF 30 HI WIT PA6-I-GF30 A. Schulman GmbH
SCHULAMID® 6 GF 30 TC PA6-GF30 A. Schulman GmbH
SCHULAMID® 6 GF 35 PA6-GF35 A. Schulman GmbH
SCHULAMID® 6 GF 35 H BLACK REC PA6-GF35 A. Schulman GmbH
SCHULAMID® 6 GF 40 PA6-GF40 A. Schulman GmbH
SCHULAMID® 6 GF 50 PA6-GF50 A. Schulman GmbH
SCHULAMID® 6 GF 50 TSU PA6-GF50 A. Schulman GmbH
SCHULAMID® 6 HV 0 H FR PA6 FR A. Schulman GmbH
SCHULAMID® 6 HV 11 PA6 A. Schulman GmbH
SCHULAMID® 6 HV 2 FR PA6 FR A. Schulman GmbH
SCHULAMID® 6 MBF 6010 H PA6-(Z+GF)60 A. Schulman GmbH
SCHULAMID® 6 MGF 45 FR 6 PA6-(MX+GF)45 FR A. Schulman GmbH
SCHULAMID® 6 MKF 3010 H PA6-(MD+GF)30 A. Schulman GmbH
SCHULAMID® 6 MKF 3010 HI PA6-I-(MD+GF)30 A. Schulman GmbH
SCHULAMID® 6 MKF 4015 PA6-(MD+GF)40 A. Schulman GmbH
SCHULAMID® 6 MT 25 FR PA6-MX25 FR A. Schulman GmbH
SCHULAMID® 6 MT 30 PA6-T30 A. Schulman GmbH
SCHULAMID® 6 MV 13 PA6 A. Schulman GmbH
SCHULAMID® 6 MV 14 PA6 A. Schulman GmbH
SCHULAMID® 6 MV 14 FR PA6 FR A. Schulman GmbH
SCHULAMID® 6 MV 14 FR 4 K1681 PA6 FR A. Schulman GmbH
SCHULAMID® 6 MV HI PA6-I A. Schulman GmbH
SCHULAMID® 6 MV HI K1893 PA6-I A. Schulman GmbH
SCHULAMID® 6 MV SHI PA6-I A. Schulman GmbH
SCHULAMID® 6 NV 12 PA6 A. Schulman GmbH
SCHULAMID® 6 NV 12 FR PA6 FR A. Schulman GmbH
SCHULAMID® 6 NV SI PA6 A. Schulman GmbH
SCHULAMID® 66/6 MT 20 K1849 (PA6+PA66)-T20 A. Schulman GmbH
SCHULAMID® B 6 MKF 4015 PA6-(GF+MX)40 A. Schulman GmbH
SCHULAMID® B 6 MV PA6 A. Schulman GmbH
SCHULAMID® K2050 GF30 SCHWARZ (PA6+PET)-GF30 A. Schulman GmbH
SCHULAMID® K2050 SCHWARZ (PA6+PET) A. Schulman GmbH
SCHULAMID® T MV PA6 A. Schulman GmbH
Technylstar™ S 216 L2 V30 BLACK PA6-GF30 Rhodia Polyamide Engineering Plastics
Technylstar™ S 216 V30 PA6-GF30 Rhodia Polyamide Engineering Plastics
Technylstar™ S 216 V35 PA6-GF35 Rhodia Polyamide Engineering Plastics
Technylstar™ S 218 MT40 PA6-MD40 Rhodia Polyamide Engineering Plastics
Technylstar™ S 218 V30 PA6-GF30 Rhodia Polyamide Engineering Plastics
Technylstar™ S 60G1 V30 PA6-GF30 FR Rhodia Polyamide Engineering Plastics
Technylstar™ SX 216 V50 PA6-GF50 Rhodia Polyamide Engineering Plastics
Technylstar™ SX 218 V50 PA6-GF50 Rhodia Polyamide Engineering Plastics
Technylstar™ SX 218 V60 PA6-GF60 Rhodia Polyamide Engineering Plastics
Technyl® C 206 PA6 Rhodia Polyamide Engineering Plastics
Technyl® C 216 PA6 Rhodia Polyamide Engineering Plastics
Technyl® C 216 V15 PA6-GF15 Rhodia Polyamide Engineering Plastics
Technyl® C 216 V30 PA6-GF30 Rhodia Polyamide Engineering Plastics
Technyl® C 216 V35 PA6-GF35 Rhodia Polyamide Engineering Plastics
Technyl® C 216 V40 PA6-GF40 Rhodia Polyamide Engineering Plastics
Technyl® C 216 V50 PA6-GF50 Rhodia Polyamide Engineering Plastics
Technyl® C 218 MZ20 V10 PA6-MD30 Rhodia Polyamide Engineering Plastics
Technyl® C 218 V15 PA6-GF15 Rhodia Polyamide Engineering Plastics
Technyl® C 218 V18 PA6-GF18 Rhodia Polyamide Engineering Plastics
Technyl® C 218 V30 PA6-GF30 Rhodia Polyamide Engineering Plastics
Technyl® C 218 V35 PA6-GF35 Rhodia Polyamide Engineering Plastics
Technyl® C 218 V45 PA6-GF45 Rhodia Polyamide Engineering Plastics
Technyl® C 218 V50 PA6-GF50 Rhodia Polyamide Engineering Plastics
Technyl® C 230 PA6 Rhodia Polyamide Engineering Plastics
Technyl® C 236SI PA6 Rhodia Polyamide Engineering Plastics
Technyl® C 246 V30 PA6-GF30 Rhodia Polyamide Engineering Plastics
Technyl® C 246M PA6 Rhodia Polyamide Engineering Plastics
Technyl® C 246SI V11 PA6-GF11 Rhodia Polyamide Engineering Plastics
Technyl® C 246SI V30 PA6-GF30 Rhodia Polyamide Engineering Plastics
Technyl® C 30H1 V30 PA6-GF30 FR Rhodia Polyamide Engineering Plastics
Technyl® C 402M PA6 Rhodia Polyamide Engineering Plastics
Technyl® C 442 BLACK V PA6-I Rhodia Polyamide Engineering Plastics
Technyl® C 502XT PA6 Rhodia Polyamide Engineering Plastics
Technyl® C 50H2 PA6 FR Rhodia Polyamide Engineering Plastics
Technyl® C 52G1 MX 25 Grey 7035 PA6-MF25 Rhodia Polyamide Engineering Plastics
Technyl® C 52G1 V20 PA6-GF20 Rhodia Polyamide Engineering Plastics
Technyl® C 52G1 V25 PA6-GF25 Rhodia Polyamide Engineering Plastics
Technyl® C 52G3 MZ25 PA6 Rhodia Polyamide Engineering Plastics
Technyl® C 52G4 MZ25 PA6-MF25 FR Rhodia Polyamide Engineering Plastics
Technyl® C 536XT PA6-I Rhodia Polyamide Engineering Plastics
Technyl® C 548B BLACK PA6-I Rhodia Polyamide Engineering Plastics
Technyl® C 548B V15 black PA6-GF15 Rhodia Polyamide Engineering Plastics
Technyl® CR 218 V30 black 1 N PA6-GF30 Rhodia Polyamide Engineering Plastics
Terblend® N NG-02 (ABS+PA6)-GF8 Styrolution Group GmbH
Terblend® N NG-02 EF (ABS+PA6)-GF8 Styrolution Group GmbH
Terblend® N NG-02 UV (ABS+PA6)-GF8 Styrolution Group GmbH
Terblend® N NG-04 (ABS+PA6)-GF20 Styrolution Group GmbH
Terblend® N NG-06 (ABS+PA6)-GF30 Styrolution Group GmbH
Terblend® N NM-11 (ABS+PA6) Styrolution Group GmbH
Terblend® N NM-12 (ABS+PA6) Styrolution Group GmbH
Terblend® N NM-12 UV (ABS+PA6) Styrolution Group GmbH
Terblend® N NM-13 (ABS+PA6) Styrolution Group GmbH
Terblend® N NM-19 (ABS+PA6) Styrolution Group GmbH
Terblend® N NM-19 XP (ABS+PA6) Styrolution Group GmbH
Terblend® N NM-21 EF (ABS+PA6) Styrolution Group GmbH
Terblend® N NMX04 (ABS+PA6) Styrolution Group GmbH
Terblend® S NM-31 (ASA+PA6) Styrolution Group GmbH
Ultramid® 8202 PA6 BASF
Ultramid® 8202 HS PA6 BASF
Ultramid® 8202C PA6 BASF
Ultramid® 8202C HS BK-102 PA6 BASF
Ultramid® 8231G HS PA6-GF15 BASF
Ultramid® 8232G HS FR BK-102 PA6-GF25 BASF
Ultramid® 8233G HS PA6-GF33 BASF
Ultramid® 8253 HS PA6 BASF
Ultramid® 8254 HS BK 102 PA6 BASF
Ultramid® 8255 HS PA6 BASF
Ultramid® 8260 PA6-MD40 BASF
Ultramid® 8262G HS BK-102 PA6-(MD+GF)20 BASF
Ultramid® 8266G HS BK102 PA6-(MD+GF)40 BASF
Ultramid® 8267G HS BK106 PA6-(MD+GF)40 BASF
Ultramid® 8272G HS BK-102 PA6-GF12 BASF
Ultramid® 8333G HI PA6-GF33 BASF
Ultramid® 8350 HS PA6 BASF
Ultramid® 8351 HS BK-102 PA6 BASF
Ultramid® B35EG3 PA6-GF15 BASF
Ultramid® B35G3 bk 564 PA6-GF15 BASF
Ultramid® B3EG10 PA6-GF50 BASF
Ultramid® B3EG3 PA6-GF15 BASF
Ultramid® B3EG5 PA6-GF25 BASF
Ultramid® B3EG6 PA6-GF30 BASF
Ultramid® B3EG6 LS SW23189 PA6-GF30 BASF
Ultramid® B3EG7 PA6-GF35 BASF
Ultramid® B3G10 SI PA6-GF50 BASF
Ultramid® B3G8 PA6-GF40 BASF
Ultramid® B3GK24 PA6-(GF+GB)30 BASF
Ultramid® B3GM35 bk 30564 PA6-(MD+GF)40 BASF
Ultramid® B3GM35 Q611 PA6-(GF+MD)40 BASF
Ultramid® B3GM35 Q643 PA6-(GF+MD)40 BASF
Ultramid® B3K PA6 BASF
Ultramid® B3L PA6-I BASF
Ultramid® B3M6 bk 30564 PA6-MD30 BASF
Ultramid® B3M6 bk 60564 PA6-MD30 BASF
Ultramid® B3S PA6 BASF
Ultramid® B3UG4 PA6-GF20 FR BASF
Ultramid® B3UGM210 PA6-(GF+MD)60 BASF
Ultramid® B3WG10 bk 564 PA6-GF50 BASF
Ultramid® B3WG3 sw23274 PA6-GF15 BASF
Ultramid® B3WG5 PA6-GF25 BASF
Ultramid® B3WG6 PA6-GF30 BASF
Ultramid® B3WG6 BGVW bk 564 PA6-GF30 BASF
Ultramid® B3WG6 GP bk 23210 PA6-GF30 BASF
Ultramid® B3WG7 PA6-GF35 BASF
Ultramid® B3WG7 BK00564 PA6-GF35 BASF
Ultramid® B3WG7 Q17 sw20560 PA6-GF35 BASF
Ultramid® B3WGM24 BK30564 PA6-(GF+MD)30 BASF
Ultramid® B3WGM24 HP bk 23210 PA6-(GF+MD)30 BASF
Ultramid® B3WGM24 sw23228 PA6-(GF+MD)30 BASF
Ultramid® B3ZG3 PA6-I-GF15 BASF
Ultramid® B3ZG6 PA6-I-GF30 BASF
Ultramid® B3ZG8 bk 20560 PA6-I-GF40 BASF
Ultramid® HMG13 HS BK-102 PA6-GF63 BASF
Ultramid® HPN 9350 HS PA6 BASF
Ultramid® HPN 9362 PA6-MD40 BASF
Ultramid® SEGM35HI BK-126 PA6-(MD+GF)40 BASF
Ultramid® TG7S BK-102 PA6-GF35 BASF
Zytel® 7301 NC010 PA6 DuPont Engineering Polymers
Zytel® 7304 NC010 PA6 DuPont Engineering Polymers
Zytel® 7331J NC010 PA6 DuPont Engineering Polymers
Zytel® 7335F NC010 PA6 DuPont Engineering Polymers
Zytel® 73G15HSL BK363 PA6-GF15 DuPont Engineering Polymers
Zytel® 73G15L NC010 PA6-GF15 DuPont Engineering Polymers
Zytel® 73G30HSL NC010 PA6-GF30 DuPont Engineering Polymers
Zytel® 73G30L NC010 PA6-GF30 DuPont Engineering Polymers
Zytel® 73G30T NC010 PA6-I-GF30 DuPont Engineering Polymers
Zytel® 73G30TGI BK267 PA6-I-GF30 DuPont Engineering Polymers
Zytel® 73G35HSL BK262 PA6-GF35 DuPont Engineering Polymers
Zytel® 73G45 BK263 PA6-GF45 DuPont Engineering Polymers
Zytel® 73G45L NC010 PA6-GF45 DuPont Engineering Polymers
Zytel® 73G50HSLA BK416 PA6-GF50 DuPont Engineering Polymers
Zytel® 74G33J NC010 (PA66+PA6)-GF33 DuPont Engineering Polymers
Zytel® 74G33W BK196 (PA66+PA6)-GF33 DuPont Engineering Polymers
Zytel® 84G33 BKB031 (PA66+PA6)-I-GF33 DuPont Engineering Polymers
Zytel® BM7300THS BK317 PA6-I DuPont Engineering Polymers
Zytel® BM73G15THS BK317 PA6-I-GF15 DuPont Engineering Polymers
Zytel® EFE7374 BK416 PA6-I-GF40 DuPont Engineering Polymers
Zytel® FG7301 NC010 PA6 DuPont Engineering Polymers
Zytel® FN727 NC010A PA6... DuPont Engineering Polymers
Zytel® PLS93G35DH1 BK549 PA6-GF35 DuPont Engineering Polymers
Zytel® ST7301 NC010 PA6-I DuPont Engineering Polymers
Zytel® ST811HS NC010 PA6-I DuPont Engineering Polymers