CAMPUS® datasheet | ALFATER XL® A55I 2GP0000
This datasheet of ALFATER XL® A55I 2GP0000 from ALBIS Plastic GmbH is provided by the international plastics database CAMPUS.
You may contact the supplier for more information about this grade.
ALFATER XL® A55I 2GP0000 | TPV | ALBIS Plastic GmbH
| Propriétés mécaniques | Valeur | Unité | Norme du test |
| Contrainte à 100% de déformation | 2 | MPa | ISO 527-1/-2 |
| Déformation à la rupture TPE | >300 | % | ISO 527-1/-2 |
| Déformation rémanente en compression, 100°C | 34 | % | ISO 815 |
| Résistance à la déchirure | 20 | kN/m | ISO 34-1 |
| Dureté Shore A, 3s | 55 | - | ISO 868 |
| Propriétés diverses | Valeur | Unité | Norme du test |
| Masse volumique | 960 | kg/m³ | ISO 1183 |
Caractéristiques
Transformation
Moulage par injection
Propriétés spéciales
Stabilisé aux intempéries
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Any information given on the chemical and physical characteristics of our products, including technical advice on applications whether verbally, in writing or by testing the product, is given to the best of our knowledge, but without warranty. It does not exempt the buyer from carrying out his own investigations and tests in order to ascertain the products' specific suitability for the purpose intended. The buyer is solely responsible for the application, utilisation and processing of the products, and must observe the laws and government regulations and the consequential rights of any third party. At all times our Conditions of Sale apply. The test values given are guide values, not binding minimum or maximum figures, which have been determined on standardized test specimen and can be affected by pigmentation, mold design and processing conditions.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012