CAMPUS® datasheet | ALTECH PA66 A 3015/100 GB15


This datasheet of ALTECH PA66 A 3015/100 GB15 from ALBIS Plastic GmbH is provided by the international plastics database CAMPUS.

You may contact the supplier for more information about this grade.

This datasheet includes:

  ALTECH PA66 A 3015/100 GB15 | PA66-GB15 | ALBIS Plastic GmbH
Propriétés mécaniquesValeurUnitéNorme du test
Module en traction 4500 MPa ISO 527-1/-2
Contrainte à la rupture 70 MPa ISO 527-1/-2
Déformation à la rupture 8 % ISO 527-1/-2
Résistance au choc Charpy, +23°C 35 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 3 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
Température de fusion, 10°C/min 260 °C ISO 11357-1/-3
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1240 kg/m³ ISO 1183
Caractéristiques
Transformation
Moulage par injection
Propriétés spéciales
Stabilisé à la chaleur
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Any information given on the chemical and physical characteristics of
our products, including technical advice on applications whether
verbally, in writing or by testing the product, is given to the best
of our knowledge, but without warranty. It does not exempt the buyer
from carrying out his own investigations and tests in order to
ascertain the products' specific suitability for the purpose intended.

The buyer is solely responsible for the application, utilisation and
processing of the products, and must observe the laws and government
regulations and the consequential rights of any third party. At all
times our Conditions of Sale apply.

The test values given are guide values, not binding minimum or maximum
figures, which have been determined on standardized test specimen and
can be affected by pigmentation, mold design and processing conditions.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012