PA 6, 25 % mineral, injection moulding, halogen free flame retardant, optimized for laser marking (1064nm)
| Propriétés rhéologiques | sec / cond | Unité | Norme du test |
| Indice de fluidité à chaud en volume, MVR | 27 / * | cm³/10min | ISO 1133 |
| Température | 260 / * | °C | ISO 1133 |
| Charge | 5 / * | kg | ISO 1133 |
| Retrait au moulage, parallèle | 0.9 / * | % | ISO 294-4, 2577 |
| Retrait au moulage, perpendiculaire | 0.9 / * | % | ISO 294-4, 2577 |
| Propriétés mécaniques | sec / cond | Unité | Norme du test |
| Module en traction | 5700 / 2100 | MPa | ISO 527-1/-2 |
| Contrainte à la rupture | 80 / 30 | MPa | ISO 527-1/-2 |
| Déformation à la rupture | 3 / 50 | % | ISO 527-1/-2 |
| Résistance au choc Charpy, +23°C | 38 / 135 | kJ/m² | ISO 179/1eU |
| Propriétés thermiques | sec / cond | Unité | Norme du test |
| Température de fusion, 10°C/min | 220 / * | °C | ISO 11357-1/-3 |
| Température de fléchissement s/chrg, 1.80 MPa | 90 / * | °C | ISO 75-1/-2 |
| Température de fléchissement s/chrg, 0.45 MPa | 195 / * | °C | ISO 75-1/-2 |
| Coeffic. de dilatation therm. linéique, parallèle | 60 / * | E-6/K | ISO 11359-1/-2 |
| Coeffic. de dilatation therm. linéique, perpend. | 70 / * | E-6/K | ISO 11359-1/-2 |
| Inflammabilité ep. nom. 1.5 mm | V-2 / * | class | IEC 60695-11-10 |
| Epaisseur de l'éprouvette | 1.5 / * | mm | IEC 60695-11-10 |
| Inflammabilité pr. épaisseur h | V-2 / * | class | IEC 60695-11-10 |
| Epaisseur de l'éprouvette | 3.0 / * | mm | IEC 60695-11-10 |
| Propriétés électriques | sec / cond | Unité | Norme du test |
| Indice de résistance au cheminement | 450 / - | - | IEC 60112 |
| Propriétés diverses | sec / cond | Unité | Norme du test |
| Absorption d'eau | 6.7 / * | % | Sim. to ISO 62 |
| Masse volumique | 1430 / - | kg/m³ | ISO 1183 |
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Disponibilité régionale
Conditions générales
This information and our technical advice - whether verbal, in writing or by way of trials - are given in good faith but without warranty, and this also applies where proprietary rights of third parties are involved. Our advice does not release you from the obligation to check its validity and to test our products as to their suitability for the intended processes and uses. The application, use and processing of our products and the products manufactured by you on the basis of our technical advice are beyond our control and, therefore, entirely your own responsibility. Our products are sold in accordance with our General Conditions of Sale and Delivery. The values stored in the databank should only be used as guidelines for component design. In giving these values neither guarantee, nor assurance of particular material properties can be given. techcenter.lanxess.com
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012