PA 6, non-reinforced, extrusion, Blasform, impact modified, heat-ageing stabilized
Propriétés rhéologiquessec / condUnitéNorme du test
Retrait au moulage, parallèle 1.7 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.4 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
Module en traction 1300 / 350 MPa ISO 527-1/-2
Contrainte d'écoulement 39 / 29 MPa ISO 527-1/-2
Déformation au seuil d'écoulement 6.3 / 50 % ISO 527-1/-2
Résistance au choc Charpy, +23°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 100 / 110 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 70 / 60 kJ/m² ISO 179/1eA
Propriétés thermiquessec / condUnitéNorme du test
Température de fusion, 10°C/min 219 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 55 / * °C ISO 75-1/-2
Propriétés diversessec / condUnitéNorme du test
Masse volumique 1040 / - kg/m³ ISO 1183
Caractéristiques
Transformation
Extrusion (autres), Soufflage
Disponibilité régionale
Conditions générales
This information and our  technical advice - whether verbal, in  writing
or by way of trials - are  given in good faith but without warranty, and
this  also  applies  where  proprietary  rights  of  third  parties  are
involved.  Our advice does not release you from  the obligation to check
its validity and to test our  products  as to their  suitability for the
intended processes and uses.  The  application, use  and  processing  of
our products and the products manufactured  by  you  on the basis of our
technical  advice  are  beyond our control and, therefore, entirely your
own  responsibility.  Our  products  are  sold  in  accordance  with our
General  Conditions of Sale and Delivery.
The values  stored in the databank should only be used as guidelines for
component   design.  In  giving  these  values  neither  guarantee,  nor
assurance of particular material properties can be given.