CAMPUS® datasheet | Grilon BGZ-15


This datasheet of Grilon BGZ-15 from EMS-GRIVORY - a unit of EMS-CHEMIE AG is provided by the international plastics database CAMPUS.

You may contact the supplier for more information about this grade.

This datasheet includes:

  Grilon BGZ-15 | PA6-GF15 | EMS-GRIVORY - a unit of EMS-CHEMIE AG
Informations produit
Product designation according to ISO 1874:

PA6-Hi, MHR, 14-060N, GF 15

 

Product Attributes

  Improved impact resistance
Propriétés rhéologiquessec / condUnitéNorme du test
Retrait au moulage, parallèle 0.2 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.7 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
Module en traction 5400 / 2900 MPa ISO 527-1/-2
Contrainte à la rupture 120 / 70 MPa ISO 527-1/-2
Déformation à la rupture 4 / 8 % ISO 527-1/-2
Résistance au choc Charpy, +23°C 70 / 80 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 60 / 70 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 13 / 20 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 7 / 7 kJ/m² ISO 179/1eA
Propriétés thermiquessec / condUnitéNorme du test
Température de fusion, 10°C/min 222 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 190 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 8.00 MPa 120 / * °C ISO 75-1/-2
Coeffic. de dilatation therm. linéique, parallèle 40 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 100 / * E-6/K ISO 11359-1/-2
Inflammabilité pr. épaisseur h HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 / * mm IEC 60695-11-10
Propriétés électriquessec / condUnitéNorme du test
Résistivité transversale 1E12 / 1E10 Ohm*m IEC 60093
Résistivité superficielle * / 1E12 Ohm IEC 60093
Rigidité diélectrique 35 / 32 kV/mm IEC 60243-1
Indice de résistance au cheminement 500 / 500 - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 7 / * % Sim. to ISO 62
Absorption d'humidité 2 / * % Sim. to ISO 62
Masse volumique 1190 / - kg/m³ ISO 1183
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Disponibilité régionale
Conditions générales
EMS-CHEMIE AG
Business Unit EMS-GRIVORY

Homepage : EMS-GRIVORY
eMail    : welcome@emsgrivory.com


The values are intended to serve as an aid in preselecting materials and for
an overview of the EMS-GRIVORY product  range. The information contained
in this publication is based on our present knowledge and experience.
The given figures and data are guidance values and do not represent binding
material specifications. No warranties of any kind, either express or implied,
including warranties of merchantability or fitness for a particular purpose, are
given regarding products, design, data and information. The customer is not
released from his obligation to investigate the products fitness and the suitability
for the intended application, compliance with legal requirements and intellectual
property rights. We reserve the right to change the information at any time and
without prior notice. The information in this publication is not to be considered
a contractual obligation and any liability whatsoever is expressly declined.
For further questions about our products please contact our experts.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012