CAMPUS® datasheet | Grilon F 47 H NL nat 6020
This datasheet of Grilon F 47 H NL nat 6020 from EMS-GRIVORY - a unit of EMS-CHEMIE AG is provided by the international plastics database CAMPUS.
You may contact the supplier for more information about this grade.
Grilon F 47 H NL nat 6020 | PA6 | EMS-GRIVORY - a unit of EMS-CHEMIE AG
Informations produit
Product designation according to ISO 1874:
PA6, FHS, 32-030/N
Product Attributes
| High viscosity, Improved heat resistance, Barrier material, Nucleated |
Markets
| Automotive | |
| Automotive electr. and electronics, lighting | |
| Electricals & Electronics | |
| Cables & Tubes |
| Propriétés rhéologiques | sec / cond | Unité | Norme du test |
| Indice de fluidité à chaud en volume, MVR | 15 / * | cm³/10min | ISO 1133 |
| Température | 275 / * | °C | ISO 1133 |
| Charge | 5 / * | kg | ISO 1133 |
| Propriétés mécaniques | sec / cond | Unité | Norme du test |
| Module en traction | 3000 / 750 | MPa | ISO 527-1/-2 |
| Propriétés thermiques | sec / cond | Unité | Norme du test |
| Température de fusion, 10°C/min | 222 / * | °C | ISO 11357-1/-3 |
| Propriétés diverses | sec / cond | Unité | Norme du test |
| Absorption d'eau | 9 / * | % | Sim. to ISO 62 |
| Absorption d'humidité | 3 / * | % | Sim. to ISO 62 |
| Masse volumique | 1140 / - | kg/m³ | ISO 1183 |
Caractéristiques
Transformation
Extrusion (autres)
Conditionnement
Granulés
Propriétés spéciales
Stabilisé à la chaleur
Disponibilité régionale
Conditions générales
EMS-CHEMIE AG Business Unit EMS-GRIVORY Homepage : EMS-GRIVORY eMail : welcome@emsgrivory.com The values are intended to serve as an aid in preselecting materials and for an overview of the EMS-GRIVORY product range. The information contained in this publication is based on our present knowledge and experience. The given figures and data are guidance values and do not represent binding material specifications. No warranties of any kind, either express or implied, including warranties of merchantability or fitness for a particular purpose, are given regarding products, design, data and information. The customer is not released from his obligation to investigate the products fitness and the suitability for the intended application, compliance with legal requirements and intellectual property rights. We reserve the right to change the information at any time and without prior notice. The information in this publication is not to be considered a contractual obligation and any liability whatsoever is expressly declined. For further questions about our products please contact our experts.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012