Impact ABS grade with antistatic


Propriétés rhéologiquesValeurUnitéNorme du test
Indice de fluidité à chaud en volume, MVR 22 cm³/10min ISO 1133
Température 220 °C ISO 1133
Charge 10 kg ISO 1133
Propriétés mécaniquesValeurUnitéNorme du test
Module en traction 2200 MPa ISO 527-1/-2
Contrainte d'écoulement 48 MPa ISO 527-1/-2
Déformation au seuil d'écoulement 2.3 % ISO 527-1/-2
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 18 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
Température de ramolliss. Vicat, 50°C/h 50N 96 °C ISO 306
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm IEC 60695-11-10
Classement UL UL - -
Propriétés électriquesValeurUnitéNorme du test
Résistivité transversale >1E13 Ohm*m IEC 60093
Résistivité superficielle >1E15 Ohm IEC 60093
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1050 kg/m³ ISO 1183
Fonctions
Volume spécifique (pvT) , POLYMAN® (ABS) LP 137 A, ABS, A. Schulman
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Grains
Propriétés spéciales
Antistatique
Disponibilité régionale
Conditions générales
The information and recommendations contained in this document are based upon
data collected by A. Schulman and are believed to be reliable; however, because
A. Schulman cannot anticipate or control the many different conditions under
which this information and/or product may be used, no representation is made
and no warranty is given of any kind, express or implied, for completeness,
accuracy, availability, suitability, usefulness, commercial value, or non-violation
of intellectual property rights of information, recommendations, and products
and services directly or indirectly provided. A. Schulman assumes no responsibility
for the results of the use of products and processes described herein and expressly
disclaims the implied warranties of merchantability and fitness for a particular use

If there are questions to given information, to further properties or further A. Schulman
products please contact

                  A. Schulman GmbH
                  Huettenstrasse 211
                  50170 Kerpen
                  Tel: 02273 / 561-0
                  Contact: aschulman@de.aschulman.com
                               Subject: Material data

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012