Ultraform® W2320 003 Q600 | POM | BASF
Informations produit
Very free-flowing, rapidly solidifying grade for use where processing is extremely difficult but mechanical properties are lower.
Abbreviated designation according to ISO 1043: POM
Designation according to ISO 9988-1: POM-K, M-GNR, 05-002
Abbreviated designation according to ISO 1043: POM
Designation according to ISO 9988-1: POM-K, M-GNR, 05-002
| Propriétés rhéologiques | Valeur | Unité | Norme du test |
| Indice de fluidité à chaud en volume, MVR | 25 | cm³/10min | ISO 1133 |
| Température | 190 | °C | ISO 1133 |
| Charge | 2.16 | kg | ISO 1133 |
| Propriétés mécaniques | Valeur | Unité | Norme du test |
| Module en traction | 2800 | MPa | ISO 527-1/-2 |
| Contrainte d'écoulement | 65 | MPa | ISO 527-1/-2 |
| Déformation au seuil d'écoulement | 7.5 | % | ISO 527-1/-2 |
| Déformation nominale à la rupture | 24 | % | ISO 527-1/-2 |
| Module de fluage en traction, 1h | 2100 | MPa | ISO 899-1 |
| Module de fluage en traction, 1000h | 1350 | MPa | ISO 899-1 |
| Résistance au choc Charpy, +23°C | 150 | kJ/m² | ISO 179/1eU |
| Résistance au choc Charpy, -30°C | 150 | kJ/m² | ISO 179/1eU |
| Résistance au choc Charpy (entaillé), +23°C | 5 | kJ/m² | ISO 179/1eA |
| Résistance au choc Charpy (entaillé), -30°C | 4 | kJ/m² | ISO 179/1eA |
| Propriétés thermiques | Valeur | Unité | Norme du test |
| Température de fusion, 10°C/min | 167 | °C | ISO 11357-1/-3 |
| Température de fléchissement s/chrg, 1.80 MPa | 100 | °C | ISO 75-1/-2 |
| Température de fléchissement s/chrg, 0.45 MPa | 156 | °C | ISO 75-1/-2 |
| Température de ramolliss. Vicat, 50°C/h 50N | 150 | °C | ISO 306 |
| Coeffic. de dilatation therm. linéique, parallèle | 110 | E-6/K | ISO 11359-1/-2 |
| Inflammabilité ep. nom. 1.5 mm | HB | class | IEC 60695-11-10 |
| Epaisseur de l'éprouvette | 1.6 | mm | IEC 60695-11-10 |
| Classement UL | UL | - | - |
| Inflammabilité pr. épaisseur h | HB | class | IEC 60695-11-10 |
| Epaisseur de l'éprouvette | 0.8 | mm | IEC 60695-11-10 |
| Classement UL | UL | - | - |
| Aptitude à l'allumage | 15 | % | ISO 4589-1/-2 |
| Propriétés électriques | Valeur | Unité | Norme du test |
| Permittivité relative, 100Hz | 3.8 | - | IEC 60250 |
| Permittivité relative, 1MHz | 3.8 | - | IEC 60250 |
| Facteur de pertes, 100Hz | 10 | E-4 | IEC 60250 |
| Facteur de pertes, 1MHz | 50 | E-4 | IEC 60250 |
| Résistivité transversale | 1E13 | Ohm*m | IEC 60093 |
| Résistivité superficielle | 1E13 | Ohm | IEC 60093 |
| Rigidité diélectrique | 40 | kV/mm | IEC 60243-1 |
| Indice de résistance au cheminement | 600 | - | IEC 60112 |
| Propriétés diverses | Valeur | Unité | Norme du test |
| Absorption d'eau | 0.8 | % | Sim. to ISO 62 |
| Absorption d'humidité | 0.2 | % | Sim. to ISO 62 |
| Masse volumique | 1400 | kg/m³ | ISO 1183 |
| Propriétés rhéologiques calculées | Valeur | Unité | Norme du test |
| Température d'éjection | 110 | °C | - |
| Préparation et conditionnement des éprouvettes | Valeur | Unité | Norme du test |
| Injection, température de la matière fondue | 200 | °C | ISO 294 |
| Injection, température du moule | 90 | °C | ISO 10724 |
| Injection, vitesse d'injection | 200 | mm/s | ISO 294 |
Fonctions
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Additifs
Agent de démoulage
Disponibilité régionale
Résistance Chimique
Conditions générales
The data contained in this publication are based on our current
knowledge and experience. In view of the many factors that may affect
processing and application of our product, these data do not relieve
processors from carrying out their own investigations and tests. Any
descriptions, drawings, photographs, data, proportions, weights etc.
given herein may change without prior information and do not constitute
the agreed contractual quality of the product. It is the responsibility
of the recipient of our products to ensure that any proprietary rights
and existing laws and legislation are observed. NO WARRANTIES OF ANY
KIND, EITHER EXPRESS OR IMPLIED, INCLUDING WARRANTIES OFMERCHANTABILITY
OR FITNESS FOR A PARTICULAR PURPOSE, ARE MADE REGARDING PRODUCTS
DESCRIBED OR DESIGNS, DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY BE USED WITHOUT INFRINGING
THEINTELLECTUAL PROPERTY RIGHTS OF OTHERS.
In order to check the availability of products please contact us or our
sales agency.
For more information about our products contact your local BASF
representative or
BASF SE
Dept. PM/K
Fax: 0621-60-49497
e-mail: e-mail
CAMPUS® is a registered trademark of CWFG (Chemie
Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)
knowledge and experience. In view of the many factors that may affect
processing and application of our product, these data do not relieve
processors from carrying out their own investigations and tests. Any
descriptions, drawings, photographs, data, proportions, weights etc.
given herein may change without prior information and do not constitute
the agreed contractual quality of the product. It is the responsibility
of the recipient of our products to ensure that any proprietary rights
and existing laws and legislation are observed. NO WARRANTIES OF ANY
KIND, EITHER EXPRESS OR IMPLIED, INCLUDING WARRANTIES OFMERCHANTABILITY
OR FITNESS FOR A PARTICULAR PURPOSE, ARE MADE REGARDING PRODUCTS
DESCRIBED OR DESIGNS, DATA OR INFORMATION SET FORTH, OR THAT THE
PRODUCTS, DESIGNS, DATA OR INFORMATION MAY BE USED WITHOUT INFRINGING
THEINTELLECTUAL PROPERTY RIGHTS OF OTHERS.
In order to check the availability of products please contact us or our
sales agency.
For more information about our products contact your local BASF
representative or
BASF SE
Dept. PM/K
Fax: 0621-60-49497
e-mail: e-mail
CAMPUS® is a registered trademark of CWFG (Chemie
Wirtschaftsfoerderungsgesellschaft GmbH, Frankfurt)
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012