ALCOM® PC 740/4 UV OR1075-05LD | PC | ALBIS Plastic GmbH
| Proprietà Reologiche | Valore | Unitá | Norma del test |
| Indice di fusione di volume, MVR | 17 | cm³/10min | ISO 1133 |
| Temperatura | 300 | °C | ISO 1133 |
| Carico | 1.2 | kg | ISO 1133 |
| Proprietà Meccaniche | Valore | Unitá | Norma del test |
| Modulo a trazione | 2400 | MPa | ISO 527-1/-2 |
| Carico unitario a trazione | 66 | MPa | ISO 527-1/-2 |
| Deformazione a snervamento | 6 | % | ISO 527-1/-2 |
| Resistenza all'urto Charpy, +23°C | N | kJ/m² | ISO 179/1eU |
| Resist. urto Charpy con intaglio, +23°C | 11 | kJ/m² | ISO 179/1eA |
| Proprietà Termiche | Valore | Unitá | Norma del test |
| Temp.di inflessione sotto carico, 1.80 MPa | 124 | °C | ISO 75-1/-2 |
| Temp.di rammollimento Vicat, 50°C/h 50N | 142 | °C | ISO 306 |
| Reaz. al fuoco spess.nom. 1.5mm | HB | class | IEC 60695-11-10 |
| Spessore provato | 1.5 | mm | IEC 60695-11-10 |
| Reazione al fuoco a spessore h | V-2 | class | IEC 60695-11-10 |
| Spessore provato | 0.8 | mm | IEC 60695-11-10 |
| Altre Proprietà | Valore | Unitá | Norma del test |
| Massa volumica | 1200 | kg/m³ | ISO 1183 |
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Caratteristiche speciali
Stab. agli U.V. o per applicaz.in esterni
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Any information given on the chemical and physical characteristics of our products, including technical advice on applications whether verbally, in writing or by testing the product, is given to the best of our knowledge, but without warranty. It does not exempt the buyer from carrying out his own investigations and tests in order to ascertain the products' specific suitability for the purpose intended. The buyer is solely responsible for the application, utilisation and processing of the products, and must observe the laws and government regulations and the consequential rights of any third party. At all times our Conditions of Sale apply. The test values given are guide values, not binding minimum or maximum figures, which have been determined on standardized test specimen and can be affected by pigmentation, mold design and processing conditions.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012