View list of

CAMPUS® datasheet | ALTECH PA66 A 3015/100 GB15


This datasheet of ALTECH PA66 A 3015/100 GB15 from ALBIS Plastic GmbH is provided by the international plastics database CAMPUS.

You may contact the supplier for more information about this grade.

This datasheet includes:

  ALTECH PA66 A 3015/100 GB15 | PA66-GB15 | ALBIS Plastic GmbH
Proprietà MeccanicheValoreUnitáNorma del test
Modulo a trazione 4500 MPa ISO 527-1/-2
Carico unitario a rottura 70 MPa ISO 527-1/-2
Deformazione a rottura 8 % ISO 527-1/-2
Resistenza all'urto Charpy, +23°C 35 kJ/m² ISO 179/1eU
Resist. urto Charpy con intaglio, +23°C 3 kJ/m² ISO 179/1eA
Proprietà TermicheValoreUnitáNorma del test
Temperatura di fusione, 10°C/min 260 °C ISO 11357-1/-3
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1240 kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Caratteristiche speciali
Stabilizzato o stabile al calore
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Any information given on the chemical and physical characteristics of
our products, including technical advice on applications whether
verbally, in writing or by testing the product, is given to the best
of our knowledge, but without warranty. It does not exempt the buyer
from carrying out his own investigations and tests in order to
ascertain the products' specific suitability for the purpose intended.

The buyer is solely responsible for the application, utilisation and
processing of the products, and must observe the laws and government
regulations and the consequential rights of any third party. At all
times our Conditions of Sale apply.

The test values given are guide values, not binding minimum or maximum
figures, which have been determined on standardized test specimen and
can be affected by pigmentation, mold design and processing conditions.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012