CAMPUS® datasheet | Crastin® S600F40 NC010
This datasheet of Crastin® S600F40 NC010 from DuPont Engineering Polymers is provided by the international plastics database CAMPUS.
The good melt stability of Crastin® thermoplastic polyester resin normally enables the recycling of properly handled production waste.
If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-24 kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.
Crastin® thermoplastic polyester resin typically is used in demanding applications in the electronics, electrical, automotive, mechanical engineering, chemical, domestic appliances and sporting goods industry.
Crastin® S600F40 is an unreinforced, lubricated, low viscosity polybutylene terephtalate for injection molding.
Food compliance:
Specific statement for EU available
Applications: bezels
| Proprietà Reologiche | Valore | Unitá | Norma del test |
| Indice di fusione di volume, MVR | 32 | cm³/10min | ISO 1133 |
| Temperatura | 250 | °C | ISO 1133 |
| Carico | 2.16 | kg | ISO 1133 |
| Ritiro di stampaggio, parallelo | 1.9 | % | ISO 294-4, 2577 |
| Ritiro di stampaggio, perpendicolare | 1.8 | % | ISO 294-4, 2577 |
| Proprietà Meccaniche | Valore | Unitá | Norma del test |
| Modulo a trazione | 2600 | MPa | ISO 527-1/-2 |
| Carico unitario a trazione | 58 | MPa | ISO 527-1/-2 |
| Deformazione a snervamento | 4 | % | ISO 527-1/-2 |
| Deformazione nominale a rottura | 30 | % | ISO 527-1/-2 |
| Modulo di scorrimento a trazione, 1h | 2500 | MPa | ISO 899-1 |
| Modulo di scorrimento a trazione, 1000h | 1800 | MPa | ISO 899-1 |
| Resistenza all'urto Charpy, +23°C | N | kJ/m² | ISO 179/1eU |
| Resistenza all'urto Charpy, -30°C | N | kJ/m² | ISO 179/1eU |
| Resist. urto Charpy con intaglio, +23°C | 4 | kJ/m² | ISO 179/1eA |
| Resist. urto Charpy con intaglio, -30°C | 4 | kJ/m² | ISO 179/1eA |
| Proprietà Termiche | Valore | Unitá | Norma del test |
| Temperatura di fusione, 10°C/min | 225 | °C | ISO 11357-1/-3 |
| Temperatura di transizione vetrosa, 10°C/min | 55 | °C | ISO 11357-1/-2 |
| Temp.di inflessione sotto carico, 1.80 MPa | 50 | °C | ISO 75-1/-2 |
| Temp.di inflessione sotto carico, 0.45 MPa | 115 | °C | ISO 75-1/-2 |
| Temp.di rammollimento Vicat, 50°C/h 50N | 175 | °C | ISO 306 |
| Coeff.di dilatazione termica lin., parallelo | 130 | E-6/K | ISO 11359-1/-2 |
| Coeff.di dilatazione termica lin., perpend. | 130 | E-6/K | ISO 11359-1/-2 |
| Reaz. al fuoco spess.nom. 1.5mm | HB | class | IEC 60695-11-10 |
| Spessore provato | 1.5 | mm | IEC 60695-11-10 |
| Omologazione UL | UL | - | - |
| Reazione al fuoco a spessore h | HB | class | IEC 60695-11-10 |
| Spessore provato | 0.8 | mm | IEC 60695-11-10 |
| Omologazione UL | UL | - | - |
| Indice di ossigeno | 22 | % | ISO 4589-1/-2 |
| Proprietà Elettriche | Valore | Unitá | Norma del test |
| Costante dielettrica relativa, 1MHz | 3.2 | - | IEC 60250 |
| Fattore di dissipazione, 100Hz | 20 | E-4 | IEC 60250 |
| Fattore di dissipazione, 1MHz | 200 | E-4 | IEC 60250 |
| Resistività volumica | >1E13 | Ohm*m | IEC 60093 |
| Resistività superficiale | 1E12 | Ohm | IEC 60093 |
| Rigidità dielettrica | 26 | kV/mm | IEC 60243-1 |
| Res. Alle correnti striscianti superficiali | 600 | - | IEC 60112 |
| Altre Proprietà | Valore | Unitá | Norma del test |
| Assorbimento d'acqua | 0.4 | % | Sim. alla ISO 62 |
| Assorbimento d'umidità | 0.2 | % | Sim. alla ISO 62 |
| Massa volumica | 1310 | kg/m³ | ISO 1183 |
| Proprietà Specifiche Materiale | Valore | Unitá | Norma del test |
| Numero di viscosità | 120 | cm³/g | ISO 307, 1157, 1628 |
| Proprietà reologiche per la simulazione | Valore | Unitá | Norma del test |
| Densità del fuso | 1110 | kg/m³ | - |
| Conduttività termica del fuso | 0.21 | W/(m K) | - |
| Capacità termica specifica del fuso | 2110 | J/(kg K) | - |
| Temperatura di estrazione | 165 | °C | - |
Contact DuPont for Material Safety Data Sheet, general guides and/or additional information about ventilation, handling, purging, drying, etc.
Test temperatures are 23°C unless otherwise stated.
The DuPont Oval Logo, DuPont™, The miracles of science™ and ® are trademarks or registered trademarks of DuPont Company.
Copyright© 2011 E.I. du Pont de Nemours and Company. All Rights Reserved.
The information provided in this data sheet corresponds to our knowledge on the subject at the date of its publication.
This information may be subject to revision as new knowledge and experience becomes available.
The data provided fall within the normal range of product properties and relate only to the specific material designated; these data may not be
valid for such material used in combination with any other materials, additives or pigments or in any process, unless expressly indicated otherwise.
The data provided should not be used to establish specification limits or used alone as the basis of design; they are not intended to substitute
for any testing you may need to conduct to determine for yourself the suitability of a specific material for your particular purposes.
Since DuPont cannot anticipate all variations in actual end-use conditions DuPont makes no warranties and assumes no liability in connection
with any use of this information.
Nothing in this publication is to be considered as a license to operate under or a recommendation to infringe any patent rights.
DuPont advises you to seek independent counsel for a freedom to practice opinion on the intended application or end-use of our products.
CAUTION: DO NOT USE DUPONT MATERIALS IN MEDICAL APPLICATIONS INVOLVING IMPLANTATION IN THE HUMAN BODY OR
CONTACT WITH INTERNAL BODY FLUIDS OR TISSUES UNLESS THE MATERIAL HAS BEEN PROVIDED FROM DUPONT UNDER A
WRITTEN CONTRACT THAT IS CONSISTENT WITH DUPONT POLICY REGARDING MEDICAL APPLICATIONS AND EXPRESSLY
ACKNOWLEDGES THE CONTEMPLATED USE.
For further information, please contact your DuPont representative. You may also request a copy of DuPont POLICY Regarding Medical
Applications... H-50103-3 and DuPont CAUTION Regarding Medical Applications... H-50102-3.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012