View list of
  • All LANXESS grades
  • All PA6 grades
  • All grades beginning with D

CAMPUS® datasheet | Durethan® BC 700 HTS


This datasheet of Durethan® BC 700 HTS from LANXESS Deutschland GmbH is provided by the international plastics database CAMPUS.

This datasheet includes:

  Durethan® BC 700 HTS | PA6-I | LANXESS Deutschland GmbH
Testo del prodotto
PA 6, non-reinforced, extrusion, Blasform, impact modified, heat-ageing stabilized
Proprietà Meccanichesecco/condUnitáNorma del test
Modulo a trazione 980 / 210 MPa ISO 527-1/-2
Carico unitario a trazione 28 / - MPa ISO 527-1/-2
Deformazione a snervamento 6.5 / - % ISO 527-1/-2
Resistenza all'urto Charpy, -30°C 105 / - kJ/m² ISO 179/1eU
Proprietà Termichesecco/condUnitáNorma del test
Temperatura di fusione, 10°C/min 211 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 48 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 53 / * °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 200 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 200 / * E-6/K ISO 11359-1/-2
Altre Proprietàsecco/condUnitáNorma del test
Massa volumica 1030 / - kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Soffiaggio
Forma fisica disponibile
Pellet
Additivi
Lubrificanti
Caratteristiche speciali
Stabilizzato o stabile al calore
Disponibilità geografica
Disclaimer
This information and our  technical advice - whether verbal, in  writing
or by way of trials - are  given in good faith but without warranty, and
this  also  applies  where  proprietary  rights  of  third  parties  are
involved.  Our advice does not release you from  the obligation to check
its validity and to test our  products  as to their  suitability for the
intended processes and uses.  The  application, use  and  processing  of
our products and the products manufactured  by  you  on the basis of our
technical  advice  are  beyond our control and, therefore, entirely your
own  responsibility.  Our  products  are  sold  in  accordance  with our
General  Conditions of Sale and Delivery.
The values  stored in the databank should only be used as guidelines for
component   design.  In  giving  these  values  neither  guarantee,  nor
assurance of particular material properties can be given.

techcenter.lanxess.com

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012