Testo del prodotto
PA 6, 25 % mineral, injection moulding, halogen free flame retardant, optimized for laser marking (1064nm)
Proprietà Reologichesecco/condUnitáNorma del test
Indice di fusione di volume, MVR 27 / * cm³/10min ISO 1133
Temperatura 260 / * °C ISO 1133
Carico 5 / * kg ISO 1133
Ritiro di stampaggio, parallelo 0.9 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.9 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
Modulo a trazione 5700 / 2100 MPa ISO 527-1/-2
Carico unitario a rottura 80 / 30 MPa ISO 527-1/-2
Deformazione a rottura 3 / 50 % ISO 527-1/-2
Resistenza all'urto Charpy, +23°C 38 / 135 kJ/m² ISO 179/1eU
Proprietà Termichesecco/condUnitáNorma del test
Temperatura di fusione, 10°C/min 220 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 90 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 195 / * °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 60 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 70 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-2 / * class IEC 60695-11-10
Spessore provato 1.5 / * mm IEC 60695-11-10
Reazione al fuoco a spessore h V-2 / * class IEC 60695-11-10
Spessore provato 3.0 / * mm IEC 60695-11-10
Proprietà Elettrichesecco/condUnitáNorma del test
Res. Alle correnti striscianti superficiali 450 / - - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 6.7 / * % Sim. alla ISO 62
Massa volumica 1430 / - kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Disponibilità geografica
Disclaimer
This information and our  technical advice - whether verbal, in  writing
or by way of trials - are  given in good faith but without warranty, and
this  also  applies  where  proprietary  rights  of  third  parties  are
involved.  Our advice does not release you from  the obligation to check
its validity and to test our  products  as to their  suitability for the
intended processes and uses.  The  application, use  and  processing  of
our products and the products manufactured  by  you  on the basis of our
technical  advice  are  beyond our control and, therefore, entirely your
own  responsibility.  Our  products  are  sold  in  accordance  with our
General  Conditions of Sale and Delivery.
The values  stored in the databank should only be used as guidelines for
component   design.  In  giving  these  values  neither  guarantee,  nor
assurance of particular material properties can be given.

techcenter.lanxess.com