This datasheet of Grivory HT2VZ-33H black 9205 from EMS-GRIVORY | a unit of EMS-CHEMIE AG is provided by the international plastics database CAMPUS.
You may contact the supplier for more information about this grade.
Grivory HT2VZ-33H black 9205 | PA6T/66-GF33 | EMS-GRIVORY - a unit of EMS-CHEMIE AG
Testo del prodotto
Product designation according to ISO 1874:
PA 6T/66, MH, 14-110, GF33
Product Attributes
| Improved impact resistance, Improved heat resistance, Improved UV resistance (outdoor use) |
Markets
| Automotive | |
| Automotive electr. and electronics, lighting, Fuel systems, Powertrain and Chassis , Interior, Exterior | |
| Electricals & Electronics | |
| Electrical equipment, Connectors | |
| Industry & Consumer goods | |
| Housewares, Hydraulics & Pneumatics, Mechanical Engineering, Power transmission, Sports & Leisure, Tools & Accessories |
| Proprietà Reologiche | secco/cond | Unitá | Norma del test |
| Ritiro di stampaggio, parallelo | 0.1 / * | % | ISO 294-4, 2577 |
| Ritiro di stampaggio, perpendicolare | 0.9 / * | % | ISO 294-4, 2577 |
| Proprietà Meccaniche | secco/cond | Unitá | Norma del test |
| Modulo a trazione | 11000 / 11000 | MPa | ISO 527-1/-2 |
| Carico unitario a rottura | 200 / 180 | MPa | ISO 527-1/-2 |
| Deformazione a rottura | 2.5 / 2.5 | % | ISO 527-1/-2 |
| Resistenza all'urto Charpy, +23°C | 55 / 55 | kJ/m² | ISO 179/1eU |
| Resistenza all'urto Charpy, -30°C | 50 / 45 | kJ/m² | ISO 179/1eU |
| Resist. urto Charpy con intaglio, +23°C | 10 / 10 | kJ/m² | ISO 179/1eA |
| Resist. urto Charpy con intaglio, -30°C | 9 / 9 | kJ/m² | ISO 179/1eA |
| Proprietà Termiche | secco/cond | Unitá | Norma del test |
| Temperatura di fusione, 10°C/min | 310 / * | °C | ISO 11357-1/-3 |
| Temp.di inflessione sotto carico, 1.80 MPa | 285 / * | °C | ISO 75-1/-2 |
| Temp.di inflessione sotto caricor, 8.00 MPa | 200 / * | °C | ISO 75-1/-2 |
| Coeff.di dilatazione termica lin., parallelo | 20 / * | E-6/K | ISO 11359-1/-2 |
| Coeff.di dilatazione termica lin., perpend. | 60 / * | E-6/K | ISO 11359-1/-2 |
| Reazione al fuoco a spessore h | HB / * | class | IEC 60695-11-10 |
| Spessore provato | 0.8 / * | mm | IEC 60695-11-10 |
| Proprietà Elettriche | secco/cond | Unitá | Norma del test |
| Resistività volumica | 1E10 / 1E10 | Ohm*m | IEC 60093 |
| Resistività superficiale | * / 1E12 | Ohm | IEC 60093 |
| Rigidità dielettrica | 38 / 37 | kV/mm | IEC 60243-1 |
| Res. Alle correnti striscianti superficiali | - / 600 | - | IEC 60112 |
| Altre Proprietà | secco/cond | Unitá | Norma del test |
| Assorbimento d'acqua | 5 / * | % | Sim. alla ISO 62 |
| Assorbimento d'umidità | 2 / * | % | Sim. alla ISO 62 |
| Massa volumica | 1440 / - | kg/m³ | ISO 1183 |
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Caratteristiche speciali
Stab. agli U.V. o per applicaz.in esterni, Stabilizzato o stabile al calore
Disponibilità geografica
Disclaimer
EMS-CHEMIE AG Business Unit EMS-GRIVORY Homepage : EMS-GRIVORY eMail : welcome@emsgrivory.com The values are intended to serve as an aid in preselecting materials and for an overview of the EMS-GRIVORY product range. The information contained in this publication is based on our present knowledge and experience. The given figures and data are guidance values and do not represent binding material specifications. No warranties of any kind, either express or implied, including warranties of merchantability or fitness for a particular purpose, are given regarding products, design, data and information. The customer is not released from his obligation to investigate the products fitness and the suitability for the intended application, compliance with legal requirements and intellectual property rights. We reserve the right to change the information at any time and without prior notice. The information in this publication is not to be considered a contractual obligation and any liability whatsoever is expressly declined. For further questions about our products please contact our experts.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012