View list of
CAMPUS® datasheet | Technyl® A 221 Natural FA
This datasheet of Technyl® A 221 Natural FA from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.
Technyl® A 221 Natural FA | PA66 | Rhodia Polyamide Engineering Plastics
Testo del prodotto
Unreinforced polyamide 66, medium viscosity, for injection moulding, with a special crystallizing agent, for fast cycles.
Suitable for food contact applications
TECHNYL® A 221 NATURAL FA offers a good combination between primary properties of the unreinforced polyamide 66 and processing properties leading to increased productivity. These performances are associated with excellent dimensional stability and good rigidity of moulded parts. This grade is used in a wide variety of industries:
- Automotive: connectors
- Electrical: connectors, rotary switches
- Consumer goods: lighters, aerosol valves.
This product is available in natural.
| Proprietà Meccaniche | secco/cond | Unitá | Norma del test |
| Modulo a trazione | 3200 / - | MPa | ISO 527-1/-2 |
| Carico unitario a rottura | 95 / - | MPa | ISO 527-1/-2 |
| Deformazione a rottura | 20 / - | % | ISO 527-1/-2 |
| Resistenza all'urto Charpy, +23°C | N / * | kJ/m² | ISO 179/1eU |
| Resist. urto Charpy con intaglio, +23°C | 2.5 / * | kJ/m² | ISO 179/1eA |
| Resist. urto Charpy con intaglio, -30°C | 2 / * | kJ/m² | ISO 179/1eA |
| Proprietà Termiche | secco/cond | Unitá | Norma del test |
| Temperatura di fusione, 10°C/min | 263 / * | °C | ISO 11357-1/-3 |
| Temp.di inflessione sotto carico, 1.80 MPa | 80 / * | °C | ISO 75-1/-2 |
| Coeff.di dilatazione termica lin., perpend. | 65 / * | E-6/K | ISO 11359-1/-2 |
| Altre Proprietà | secco/cond | Unitá | Norma del test |
| Assorbimento d'acqua | 1.1 / * | % | Sim. alla ISO 62 |
| Massa volumica | 1140 / - | kg/m³ | ISO 1183 |
| Preparazione Provette | Valore | Unitá | Norma del test |
| Stamp. ad Iniezione, temperatura dello stampo | 80 | °C | ISO 10724 |
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Disponibilità geografica
Disclaimer
WARRANTY This information is supplied to assist you in your choice of the material best suited to your requirements and does not in any way constitute a product specification. The values given relate to unpigmented materials (natural colour). Pigmentation can alter results. The characteristics supplied are typical values. Our specialists are available to advise you on the values to be used in order to carry out calculations correctly on part dimensions. The information contained in this document is supplied in good faith. However it is given purely as an indication. It shall not be considered in any way as a formal commitment or warranty on our part, notably in respect of the eventual infringement of any rights of third parties who may use our products. We remain at your entire disposal to provide you with any information that you might require.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.