CAMPUS® datasheet | ALCOM® MABS 560/1 SV 1214-04 MCF
This datasheet of ALCOM® MABS 560/1 SV 1214-04 MCF from ALBIS Plastic GmbH is provided by the international plastics database CAMPUS.
You may contact the supplier for more information about this grade.
ALCOM® MABS 560/1 SV 1214-04 MCF | ABS | ALBIS Plastic GmbH
| レオロジー特性 | 値 | 単位 | テスト基準 |
| メルトボリュームレイト, MVR | 5 | cm³/10min | ISO 1133 |
| 温度 | 220 | °C | ISO 1133 |
| 荷重 | 10 | kg | ISO 1133 |
| 機械的特性 | 値 | 単位 | テスト基準 |
| 引張弾性率 | 2100 | MPa | ISO 527-1/-2 |
| 破壊応力 | 40 | MPa | ISO 527-1/-2 |
| 破壊ひずみ | 8 | % | ISO 527-1/-2 |
| シャルピー衝撃強さ, +23°C | 25 | kJ/m² | ISO 179/1eU |
| ノッチ付きシャルピー衝撃強さ, +23°C | 4 | kJ/m² | ISO 179/1eA |
| 熱的特性 | 値 | 単位 | テスト基準 |
| 荷重たわみ温度, 1.80 MPa | 85 | °C | ISO 75-1/-2 |
| ビカット軟化温度, 50°C/h 50N | 75 | °C | ISO 306 |
| その他の特性. | 値 | 単位 | テスト基準 |
| 密度 | 1120 | kg/m³ | ISO 1183 |
Disclaimer
Any information given on the chemical and physical characteristics of our products, including technical advice on applications whether verbally, in writing or by testing the product, is given to the best of our knowledge, but without warranty. It does not exempt the buyer from carrying out his own investigations and tests in order to ascertain the products' specific suitability for the purpose intended. The buyer is solely responsible for the application, utilisation and processing of the products, and must observe the laws and government regulations and the consequential rights of any third party. At all times our Conditions of Sale apply. The test values given are guide values, not binding minimum or maximum figures, which have been determined on standardized test specimen and can be affected by pigmentation, mold design and processing conditions.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012