  ALTECH PA66 A 2015/710 GF15 IM | PA66-I-GF15 | ALBIS Plastic GmbH
機械的特性単位テスト基準
引張弾性率 5000 MPa ISO 527-1/-2
破壊応力 90 MPa ISO 527-1/-2
破壊ひずみ 4.5 % ISO 527-1/-2
シャルピー衝撃強さ, +23°C 65 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 20 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
溶融温度, 10°C/min 260 °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 200 °C ISO 75-1/-2
ビカット軟化温度, 50°C/h 50N 200 °C ISO 306
その他の特性.単位テスト基準
密度 1170 kg/m³ ISO 1183
特殊な特性
成形加工法.
射出成形.
特殊な特性.
熱安定化.
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 南・中央アメリカ., 近東/アフリカ
Disclaimer
Any information given on the chemical and physical characteristics of
our products, including technical advice on applications whether
verbally, in writing or by testing the product, is given to the best
of our knowledge, but without warranty. It does not exempt the buyer
from carrying out his own investigations and tests in order to
ascertain the products' specific suitability for the purpose intended.

The buyer is solely responsible for the application, utilisation and
processing of the products, and must observe the laws and government
regulations and the consequential rights of any third party. At all
times our Conditions of Sale apply.

The test values given are guide values, not binding minimum or maximum
figures, which have been determined on standardized test specimen and
can be affected by pigmentation, mold design and processing conditions.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012