Bakelite® PF 2560 | PF-X | Momentive Specialty Chemicals
商品の説明文
Product description:
Phenolic moulding compound, inorganically/organically filled, average heat resistance, high surface quality, lower water absorption than PF 31, minimal distortion, UL listed moulding compound 1.5 mm / V-1 (ALL), 3.0 mm / V-0 (ALL).
Application areas:
Housings for domestic appliances, oven strips.| Property Name | Value | Unit | Standard No. |
|---|---|---|---|
| Apparent density (moulding compound) | 0.75 | g/cm³ | ISO 60 |
| Moulding shrinkage (injection moulding, longitudinal) | 0.75 | % | ISO 2577 |
| Post shrinkage (injection moulding, 168h/110°C) | 0.4 | % | ISO 2577 |
| Tensile strength (5mm/min) | 50 | MPa | ISO 527-1/2 |
| Compr. strength (test spec. flat tested) | 220 | MPa | ISO 604 |
| Flexural strength (2mm/min) | 90 | MPa | ISO 178 |
| Flexural modulus | 9000 | MPa | ISO 178 |
| Ball indentation hardness (H 961/30) | 350 | MPa | ISO 2039/P1 |
| Water absorption (24h/23°C) | 20 | mg | similar to ISO 62 |
| Additional characteristics: | A, EL, UL |
Preparation of Test Specimens of Thermosetting Moulding Compound
- Compression to ISO 295
- Injection to ISO 10724
Storage capability
2 years (relative humidity of 50-60% and maximum storage temperature of approximately 20°C)
| レオロジー特性 | 値 | 単位 | テスト基準 |
| 成形収縮率, 平行 | 0.8 | % | ISO 294-4, 2577 |
| 機械的特性 | 値 | 単位 | テスト基準 |
| 引張弾性率 | 9000 | MPa | ISO 527-1/-2 |
| シャルピー衝撃強さ, +23°C | 6 | kJ/m² | ISO 179/1eU |
| ノッチ付きシャルピー衝撃強さ, +23°C | 1.6 | kJ/m² | ISO 179/1eA |
| 熱的特性 | 値 | 単位 | テスト基準 |
| 荷重たわみ温度, 8.00 MPa | 115 | °C | ISO 75-1/-2 |
| 1.5mm厚さでの燃焼性 | V-1 | class | IEC 60695-11-10 |
| 試験片の厚さ | 1.5 | mm | IEC 60695-11-10 |
| UL認定 | UL | - | - |
| 厚さhでの燃焼性 | V-0 | class | IEC 60695-11-10 |
| 試験片の厚さ | 3.0 | mm | IEC 60695-11-10 |
| UL認定 | UL | - | - |
| 電気的特性. | 値 | 単位 | テスト基準 |
| 比誘電率, 100Hz | 14.5 | - | IEC 60250 |
| 誘電正接, 100Hz | 0.2 | E-4 | IEC 60250 |
| 体積抵抗率 | 1E9 | Ohm*m | IEC 60093 |
| 表面抵抗率 | 1E10 | Ohm | IEC 60093 |
| 耐電圧 | 6 | kV/mm | IEC 60243-1 |
| 耐トラッキング性 | 125 | - | IEC 60112 |
| その他の特性. | 値 | 単位 | テスト基準 |
| 密度 | 1590 | kg/m³ | ISO 1183 |
| 試験片の成形条件. | 値 | 単位 | テスト基準 |
| 射出成形, 樹脂温度 | 115 | °C | ISO 10724 |
| 射出成形, 射出速度 | 170 | mm/s | ISO 10724 |
| 射出成形, 保圧 | 100 | MPa | ISO 10724 |
| 射出成形, 硬化時間 | 25 | min | ISO 10724 |
| 圧縮成形, 金型温度 | 160 | °C | ISO 295 |
| 圧縮成形, 硬化時間 | 1 | min | ISO 295 |
機能
Disclaimer
Momentive Specialty Chemicals GmbH
Gennaer Str. 2 - 4
58642 Iserlohn - Letmathe, Germany
Telefon +49 (0) 2374 / 925 280
Fax +49 (0) 2374 / 925 723
E-mail: michael.stahl@momentive.com
----------------------------------------------------------------------
Important Information
As international harmonization of testing procedures progresses,
previously used national standards are increasingly being replaced by
ISO (DIN EN ISO) standards.
All information, recommendations and suggestions provided by Bakelite AG
in the form of verbal or written communication, or in pertinent data
bases, represent our best knowledge and experience. Such data are
non-binding in character, and do not represent, either explicitly or
implicitly, assurances or a guarantee of specific properties. The
specified parameters merely represent typical data; they do not form a
basis for either a guarantee or a specification. The information,
recommendations and suggestions we provide describe our products and
possible applications in general or exemplary terms; they do not relate
to specific cases. The process of constant continued development and
improvement of our products can lead to changes in pertinent parameters,
texts and illustrations; no special mention is made of possible
alterations. Our technical advice does not free the customer of its
responsibility to verify our current information, in particular our
technical data sheets, safety data sheets and technical information
leaflets.
The customer will conduct its own tests of our products to determine
their suitability for the intended processes and uses, as well as to
establish that their processing properties are appropriate in the
pertinent situation, since our products may be used in a wide range of
technical applications that involve very different requirements
according to the specific situation. Therefore, such specific cases
are outside our control, and are the exclusive responsibility of the
customer. A pertinent agreement is necessary in case a binding assurance
of specific parameters is required. Customers and users of our products
must themselves observe possible patent rights, existing legislation
and regulations. This publication does not represent a license, nor
does it authorize infringement of any type of patent.
Note: This version supersedes and replaces all previous publications on
this subject. "Bakelite" is a registered brand of Bakelite AG in more
than 50 countries throughout the world. In the USA, "Bakelite" is a
registered brand of the Georgia Pacific Corporation. Bakelite AG is
licensed to use the brand name "Bakelite" for epoxy resins in the USA.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012