CAMPUS® datasheet | Bergaflex® BFI 60A-3114
This datasheet of Bergaflex® BFI 60A-3114 from PolyOne Engineered Materials Europe is provided by the international plastics database CAMPUS.
Styrene Ethylene Buthylene Styrene
thermoplastic elastomer
transparent grade, hardness: Shore 60A
rubberlike, elastic properties and thermoplastic
processing
| 機械的特性 | 値 | 単位 | テスト基準 |
| 伸び率100%時の応力 | 2.5 | MPa | ISO 527-1/-2 |
| 伸び率300%時の応力 | 3.8 | MPa | ISO 527-1/-2 |
| 破壊応力 TPE | 5.4 | MPa | ISO 527-1/-2 |
| 破壊ひずみ TPE | >300 | % | ISO 527-1/-2 |
| 圧縮永久ひずみ, 23°C | 16 | % | ISO 815 |
| 圧縮永久ひずみ, 70°C | 88 | % | ISO 815 |
| 圧縮永久ひずみ, 100°C | 93 | % | ISO 815 |
| ショア硬さA, 3s | 60 | - | ISO 868 |
| その他の特性. | 値 | 単位 | テスト基準 |
| 密度 | 890 | kg/m³ | ISO 1183 |
| 試験片の成形条件. | 値 | 単位 | テスト基準 |
| 射出成形, 樹脂温度 | 170 | °C | ISO 294 |
| 射出成形, 金型温度 | 30 | °C | ISO 10724 |
PolyOnePolyOne Engineered Materials Europe
PolyOne Th.Bergmann GmbH
PolyOne Corporation makes no representations, guarantees or warranties of any kind with respect to the information contained in this document about its accuracy, suitability for particular applications ort he result obtained or obtainable using the information. Some of the information arises from laboratory work with small-case equipment which may not provide a reliable indication of performance or properties obtained or obtainable on larger-scale equipment. Processing conditions can cause material properties to shift from the values stated in data bases. PolyOne Corporation makes no guarantees or warranties respecting suitability of either PolyOne’s products or the information for your process or end-use application. You have the responsibility to conduct full-scale end-product performance testing to determine suitability in your application, and you assume all risks and liability arising from your use of the information and/or handling of any product. PolyOne Corporation makes no warranties, express or implied, including, but not limited to, implied warranties of merchantability and fitness for a particular purpose, either with respect to the information or products reflected by the information. These information shall not operate as permission, recommendation or inducement to practice any patented invention without permission of the patent owner.
Germany:
PolyOne Th.Bergmann GmbH
Adolf-Dambach-Strasse 2-4
D-76571 Gaggenau
Tel.: 07225 6802 0
Fax:07225 6802 10
France:
PolyOne Engineered Materials SA, FRANCE
20, Rue Salvador Allende, BP 105
42353 La Talaudière Cedex, France
Tel.: +33 (0) 477 47 64 00
Tel.:+33 (0) 477 57 13
Spain:
Pol. Ind. Valle del Cinca
22300 Barbastro, Spain
Tel.: +34 (0) 974 31 03 14
Fax.: +34 (0) 974 31 43 11
United Kingdom:
PolyOne Engineered Materials UL Ltd.
Newton Ayecliff
Durham DL5 6EA, UK
Tel.:+44 (0) 1325 30 08 48
Fax.:+44 (0) 1325 30 14 13
Turkey:
Tekno Polimer
103 Kücükcekmece
Istanbul, Turkey
Tel:+90 212 549 2256
Fax.:+90 212 549 2241
CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012