  Grivory GV-5 FWA nat | PA*-GF50 | EMS-GRIVORY - a unit of EMS-CHEMIE AG
商品の説明文
Product designation according to ISO 1874:

PA66+PA6I/X, MH, 14-190, GF50

 

Partially aromatic Polyamide

Markets

  Industry & Consumer goods
  Housewares, Hydraulics & Pneumatics, Mechanical Engineering, Power transmission,
Sanitary, water and gas supply

Approvals

  Food Contact
  EU Requirements, FDA
  Water contact
  NSF 61, KTW, WRAS, ACS, DVGW W270
レオロジー特性乾燥/調湿単位テスト基準
成形収縮率, 平行 0.1 / * % ISO 294-4, 2577
成形収縮率, 直角 0.4 / * % ISO 294-4, 2577
機械的特性乾燥/調湿単位テスト基準
引張弾性率 18000 / 17000 MPa ISO 527-1/-2
破壊応力 250 / 220 MPa ISO 527-1/-2
破壊ひずみ 2.5 / 2.5 % ISO 527-1/-2
シャルピー衝撃強さ, +23°C 90 / 90 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 80 / 80 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 15 / 15 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 13 / 13 kJ/m² ISO 179/1eA
熱的特性乾燥/調湿単位テスト基準
溶融温度, 10°C/min 260 / * °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 235 / * °C ISO 75-1/-2
荷重たわみ温度, 8.00 MPa 165 / * °C ISO 75-1/-2
線膨張係数, 平行 15 / * E-6/K ISO 11359-1/-2
線膨張係数, 直角 90 / * E-6/K ISO 11359-1/-2
厚さhでの燃焼性 HB / * class IEC 60695-11-10
試験片の厚さ 0.8 / * mm IEC 60695-11-10
電気的特性.乾燥/調湿単位テスト基準
体積抵抗率 1E12 / 1E12 Ohm*m IEC 60093
表面抵抗率 * / 1E13 Ohm IEC 60093
耐電圧 33 / 33 kV/mm IEC 60243-1
耐トラッキング性 - / 600 - IEC 60112
その他の特性.乾燥/調湿単位テスト基準
吸水率 4 / * % Sim. to ISO 62
吸湿率 1.4 / * % Sim. to ISO 62
密度 1560 / - kg/m³ ISO 1183
流動解析用データ単位テスト基準
溶融時の密度 1370 kg/m³ -
溶融時の熱伝導率 0.28 W/(m K) -
溶融時の比熱 1800 J/(kg K) -
熱拡散率 1.14E-7 m²/s -
突き出し時の時の温度 230 °C -
機能
 粘度せん断速度. , Grivory GV-5 FWA nat, PA*-GF50, EMS-GRIVORY
 せん断応力-せん断速度. , Grivory GV-5 FWA nat, PA*-GF50, EMS-GRIVORY
 せん断弾性率-温度. , Grivory GV-5 FWA nat, PA*-GF50, EMS-GRIVORY
 せん断弾性率-温度. , Grivory GV-5 FWA nat, PA*-GF50, EMS-GRIVORY
 応力-ひずみ. , Grivory GV-5 FWA nat, PA*-GF50, EMS-GRIVORY
 応力-ひずみ. , Grivory GV-5 FWA nat, PA*-GF50, EMS-GRIVORY
 割線弾性率−ひずみ. , Grivory GV-5 FWA nat, PA*-GF50, EMS-GRIVORY
 割線弾性率−ひずみ. , Grivory GV-5 FWA nat, PA*-GF50, EMS-GRIVORY
 応力-ひずみ (等時的). 23°C, Grivory GV-5 FWA nat, PA*-GF50, EMS-GRIVORY
 クリープ弾性率−時間. 23°C, Grivory GV-5 FWA nat, PA*-GF50, EMS-GRIVORY
 応力-ひずみ (等時的). 60°C, Grivory GV-5 FWA nat, PA*-GF50, EMS-GRIVORY
 クリープ弾性率−時間. 60°C, Grivory GV-5 FWA nat, PA*-GF50, EMS-GRIVORY
 応力-ひずみ (等時的). 80°C, Grivory GV-5 FWA nat, PA*-GF50, EMS-GRIVORY
 クリープ弾性率−時間. 80°C, Grivory GV-5 FWA nat, PA*-GF50, EMS-GRIVORY
 pvT , Grivory GV-5 FWA nat, PA*-GF50, EMS-GRIVORY
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
領域別の利用可能性
Disclaimer
EMS-CHEMIE AG
Business Unit EMS-GRIVORY

Homepage : EMS-GRIVORY
eMail    : welcome@emsgrivory.com


The values are intended to serve as an aid in preselecting materials and for
an overview of the EMS-GRIVORY product  range. The information contained
in this publication is based on our present knowledge and experience.
The given figures and data are guidance values and do not represent binding
material specifications. No warranties of any kind, either express or implied,
including warranties of merchantability or fitness for a particular purpose, are
given regarding products, design, data and information. The customer is not
released from his obligation to investigate the products fitness and the suitability
for the intended application, compliance with legal requirements and intellectual
property rights. We reserve the right to change the information at any time and
without prior notice. The information in this publication is not to be considered
a contractual obligation and any liability whatsoever is expressly declined.
For further questions about our products please contact our experts.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012