  Grivory HT2VZ-33H black 9205 | PA6T/66-GF33 | EMS-GRIVORY - a unit of EMS-CHEMIE AG
商品の説明文
Product designation according to ISO 1874:

PA 6T/66, MH, 14-110, GF33

 

Product Attributes

  Improved impact resistance, Improved heat resistance, Improved UV resistance (outdoor use)

Markets

  Automotive
  Automotive electr. and electronics, lighting, Fuel systems, Powertrain and Chassis , Interior,
Exterior
  Electricals & Electronics
  Electrical equipment, Connectors
  Industry & Consumer goods
  Housewares, Hydraulics & Pneumatics, Mechanical Engineering, Power transmission, Sports & Leisure,
Tools & Accessories
レオロジー特性乾燥/調湿単位テスト基準
成形収縮率, 平行 0.1 / * % ISO 294-4, 2577
成形収縮率, 直角 0.9 / * % ISO 294-4, 2577
機械的特性乾燥/調湿単位テスト基準
引張弾性率 11000 / 11000 MPa ISO 527-1/-2
破壊応力 200 / 180 MPa ISO 527-1/-2
破壊ひずみ 2.5 / 2.5 % ISO 527-1/-2
シャルピー衝撃強さ, +23°C 55 / 55 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 50 / 45 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 10 / 10 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 9 / 9 kJ/m² ISO 179/1eA
熱的特性乾燥/調湿単位テスト基準
溶融温度, 10°C/min 310 / * °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 285 / * °C ISO 75-1/-2
荷重たわみ温度, 8.00 MPa 200 / * °C ISO 75-1/-2
線膨張係数, 平行 20 / * E-6/K ISO 11359-1/-2
線膨張係数, 直角 60 / * E-6/K ISO 11359-1/-2
厚さhでの燃焼性 HB / * class IEC 60695-11-10
試験片の厚さ 0.8 / * mm IEC 60695-11-10
電気的特性.乾燥/調湿単位テスト基準
体積抵抗率 1E10 / 1E10 Ohm*m IEC 60093
表面抵抗率 * / 1E12 Ohm IEC 60093
耐電圧 38 / 37 kV/mm IEC 60243-1
耐トラッキング性 - / 600 - IEC 60112
その他の特性.乾燥/調湿単位テスト基準
吸水率 5 / * % Sim. to ISO 62
吸湿率 2 / * % Sim. to ISO 62
密度 1440 / - kg/m³ ISO 1183
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
特殊な特性.
紫外線安定化., 熱安定化.
領域別の利用可能性
Disclaimer
EMS-CHEMIE AG
Business Unit EMS-GRIVORY

Homepage : EMS-GRIVORY
eMail    : welcome@emsgrivory.com


The values are intended to serve as an aid in preselecting materials and for
an overview of the EMS-GRIVORY product  range. The information contained
in this publication is based on our present knowledge and experience.
The given figures and data are guidance values and do not represent binding
material specifications. No warranties of any kind, either express or implied,
including warranties of merchantability or fitness for a particular purpose, are
given regarding products, design, data and information. The customer is not
released from his obligation to investigate the products fitness and the suitability
for the intended application, compliance with legal requirements and intellectual
property rights. We reserve the right to change the information at any time and
without prior notice. The information in this publication is not to be considered
a contractual obligation and any liability whatsoever is expressly declined.
For further questions about our products please contact our experts.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012