  HERAFLEX® A 70-21-22 | TPS | RadiciPlastics
商品の説明文
No predrying necessary

DESIGNATION:
Thermoplastics ISO 1043-1 TPS

BRIEF DESCRIPTION:
Shore hardness: 70A
Low odour level, easy to demould
Application examples: Automotive interior parts
(matts without sunlight contact)
機械的特性単位テスト基準
伸び率100%時の応力 2 MPa ISO 527-1/-2
伸び率300%時の応力 2.6 MPa ISO 527-1/-2
破壊応力 TPE 11 MPa ISO 527-1/-2
破壊ひずみ TPE >300 % ISO 527-1/-2
ショア硬さA, 3s 70 - ISO 868
その他の特性.単位テスト基準
密度 960 kg/m³ ISO 1183
試験片の成形条件.単位テスト基準
射出成形, 樹脂温度 210 °C ISO 294
射出成形, 金型温度 40 °C ISO 10724
機能
 粘度せん断速度. , HERAFLEX® A 70-21-22, TPS, RadiciPlastics
 せん断応力-せん断速度. , HERAFLEX® A 70-21-22, TPS, RadiciPlastics
特殊な特性
成形加工法.
射出成形., その他の押出成形.
納入形状.
ペレット.
領域別の利用可能性
Disclaimer
This database provides the technical properties
of thermoplastics produced and marketed by
RADICI NOVACIPS
and his subsidiaries companies:

RADILON® A          Polyamide 66
RADILON® S          Polyamide 6
RADILON® CA       Copolyamide 66/6
RADILON® CS       Copolyamide 6 semiaromatic
RADITER® B          Poly(butylene terephthalate)
RADIFLAM® A         Polyamide 66,  self-extinguishing
RADIFLAM® S         Polyamide 6,   self-extinguishing
RADIFLAM® B         Polybutylene terephthalate, self-extinguishing
HERAFLEX® A        Stirenic Thermoplastic Elastomer SEBS
HERAFLEX® E        Ether-Ester Thermoplastic Elastomer
HERAFLEX® B        Stirenic Thermoplastic Elastomer SBS
HERAFLEX® P        Modified Polypropylene
RADILENE® R        Polyethylene and Polypropylene

The data and graphs contained in this database were carried out
by our Research Centers and shall in no event be held to
constitute or imply any warranty, undertaking, express or
implied commitment from our part.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012