This datasheet of Minlon® 10B40HS1 BK061 from DuPont Engineering Polymers is provided by the international plastics database CAMPUS.

This datasheet includes:

  Minlon® 10B40HS1 BK061 | PA66-MD40 | DuPont Engineering Polymers
レオロジー特性乾燥/調湿単位テスト基準
成形収縮率, 平行 0.4 / * % ISO 294-4, 2577
成形収縮率, 直角 0.9 / * % ISO 294-4, 2577
機械的特性乾燥/調湿単位テスト基準
引張弾性率 10000 / - MPa ISO 527-1/-2
破壊応力 95 / - MPa ISO 527-1/-2
破壊ひずみ 2.5 / - % ISO 527-1/-2
ノッチ付きシャルピー衝撃強さ, +23°C 3 / - kJ/m² ISO 179/1eA
熱的特性乾燥/調湿単位テスト基準
溶融温度, 10°C/min 263 / * °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 170 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 240 / * °C ISO 75-1/-2
線膨張係数, 平行 36 / * E-6/K ISO 11359-1/-2
線膨張係数, 直角 66 / * E-6/K ISO 11359-1/-2
その他の特性.乾燥/調湿単位テスト基準
密度 1510 / - kg/m³ ISO 1183
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
添加剤.
離型剤.
領域別の利用可能性
Disclaimer
All data provided according to ISO 10350 for single points and ISO 11403 for multipoints.

Contact DuPont for Material Safety Data Sheet, general guides and/or additional information about ventilation, handling, purging, drying, etc.
Test temperatures are 23°C unless otherwise stated.

The DuPont Oval Logo, DuPont™, The miracles of science™ and ® are trademarks or registered trademarks of DuPont Company.
Copyright© 2013 E.I. du Pont de Nemours and Company. All Rights Reserved.

The information provided in this data sheet corresponds to our knowledge on the subject at the date of its publication.
This information may be subject to revision as new knowledge and experience becomes available.
The data provided fall within the normal range of product properties and relate only to the specific material designated; these data may not be
valid for such material used in combination with any other materials, additives or pigments or in any process, unless expressly indicated otherwise.
The data provided should not be used to establish specification limits or used alone as the basis of design; they are not intended to substitute
for any testing you may need to conduct to determine for yourself the suitability of a specific material for your particular purposes.
Since DuPont cannot anticipate all variations in actual end-use conditions DuPont makes no warranties and assumes no liability in connection
with any use of this information.
Nothing in this publication is to be considered as a license to operate under or a recommendation to infringe any patent rights.
DuPont advises you to seek independent counsel for a freedom to practice opinion on the intended application or end-use of our products.

CAUTION: DO NOT USE DUPONT MATERIALS IN MEDICAL APPLICATIONS INVOLVING IMPLANTATION IN THE HUMAN BODY OR
CONTACT WITH INTERNAL BODY FLUIDS OR TISSUES UNLESS THE MATERIAL HAS BEEN PROVIDED FROM DUPONT UNDER A
WRITTEN CONTRACT THAT IS CONSISTENT WITH DUPONT POLICY REGARDING MEDICAL APPLICATIONS AND EXPRESSLY
ACKNOWLEDGES THE CONTEMPLATED USE.

For further information, please contact your DuPont representative. You may also request a copy of DuPont POLICY Regarding Medical
Applications... H-50103-3 and DuPont CAUTION Regarding Medical Applications... H-50102-3.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012