  RADIFLAM® A RV250FR | PA66-GF25 FR | RadiciPlastics
商品の説明文
DESIGNATION:
Thermoplastics ISO1874-PA66,MFR,-140,GF25

BRIEF DESCRIPTION:
PA66 Flame retardant injection moulding grade
halogens or phosphorus free.
25% Glass fibre reinforced.
For high stiffness items. Good dimensional stability
UL94 V0 rated
機械的特性乾燥/調湿単位テスト基準
引張弾性率 14000 / - MPa ISO 527-1/-2
破壊応力 155 / - MPa ISO 527-1/-2
破壊ひずみ 2.3 / - % ISO 527-1/-2
シャルピー衝撃強さ, +23°C 40 / - kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 30 / - kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 4.2 / - kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 3.8 / - kJ/m² ISO 179/1eA
熱的特性乾燥/調湿単位テスト基準
溶融温度, 10°C/min 260 / * °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 210 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 220 / * °C ISO 75-1/-2
ビカット軟化温度, 50°C/h 50N 220 / * °C ISO 306
1.5mm厚さでの燃焼性 V-0 / * class IEC 60695-11-10
試験片の厚さ 1.6 / * mm IEC 60695-11-10
UL認定 UL / * - -
厚さhでの燃焼性 V-0 / * class IEC 60695-11-10
試験片の厚さ 0.8 / * mm IEC 60695-11-10
電気的特性.乾燥/調湿単位テスト基準
体積抵抗率 >1E13 / 1E13 Ohm*m IEC 60093
表面抵抗率 * / 1E14 Ohm IEC 60093
耐トラッキング性 * / 600 - IEC 60112
その他の特性.乾燥/調湿単位テスト基準
吸水率 2.4 / * % Sim. to ISO 62
吸湿率 0.9 / * % Sim. to ISO 62
密度 1680 / * kg/m³ ISO 1183
試験片の成形条件.単位テスト基準
ISO規格による成形条件 1870 - ISO ....-2
射出成形, 樹脂温度 290 °C ISO 294
射出成形, 金型温度 80 °C ISO 10724
機能
 応力-ひずみ. , RADIFLAM® A RV250FR, PA66-GF25 FR, RadiciPlastics
 割線弾性率−ひずみ. , RADIFLAM® A RV250FR, PA66-GF25 FR, RadiciPlastics
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
添加剤.
滑剤.
領域別の利用可能性
Disclaimer
This database provides the technical properties
of thermoplastics produced and marketed by
RADICI NOVACIPS
and his subsidiaries companies:

RADILON® A          Polyamide 66
RADILON® S          Polyamide 6
RADILON® CA       Copolyamide 66/6
RADILON® CS       Copolyamide 6 semiaromatic
RADITER® B          Poly(butylene terephthalate)
RADIFLAM® A         Polyamide 66,  self-extinguishing
RADIFLAM® S         Polyamide 6,   self-extinguishing
RADIFLAM® B         Polybutylene terephthalate, self-extinguishing
HERAFLEX® A        Stirenic Thermoplastic Elastomer SEBS
HERAFLEX® E        Ether-Ester Thermoplastic Elastomer
HERAFLEX® B        Stirenic Thermoplastic Elastomer SBS
HERAFLEX® P        Modified Polypropylene
RADILENE® R        Polyethylene and Polypropylene

The data and graphs contained in this database were carried out
by our Research Centers and shall in no event be held to
constitute or imply any warranty, undertaking, express or
implied commitment from our part.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012