CAMPUS® datasheet | Zytel® HTNFE350038 BK083


This datasheet of Zytel® HTNFE350038 BK083 from DuPont Engineering Polymers is provided by the international plastics database CAMPUS.

This datasheet includes:

  Zytel® HTNFE350038 BK083 | PA6T/XT-GF33 | DuPont Engineering Polymers
商品の説明文
Common features of Zytel® nylon resin include mechanical and physical properties such as high mechanical strength, excellent balance of stiffness and toughness, good high temperature performance, good electrical and flammability properties, good abrasion and chemical resistance. In addition, Zytel® nylon resins are available in different modified and reinforced grades to create a wide range of products with tailored properties for specific processes and end-uses. Zytel® nylon resin, including most flame retardant grades, offer the ability to be coloured.

 

The good melt stability of Zytel® nylon resin normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-31kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.

 

Zytel® nylon resin typically is used in demanding applications in the automotive, furniture, domestic appliances, sporting goods and construction industry.

 

 Zytel® HTNFE350038 is a 33% glass reinforced, heat stabilized, lubricated, hydrolysis resistant high performance polyamide resin for injection molding. It has improved mechanical properties.

機械的特性乾燥/調湿単位テスト基準
引張弾性率 10000 / - MPa ISO 527-1/-2
破壊応力 200 / - MPa ISO 527-1/-2
破壊ひずみ 2.9 / - % ISO 527-1/-2
シャルピー衝撃強さ, +23°C 70 / - kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 10 / - kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 10 / - kJ/m² ISO 179/1eA
熱的特性乾燥/調湿単位テスト基準
溶融温度, 10°C/min 304 / * °C ISO 11357-1/-3
その他の特性.乾燥/調湿単位テスト基準
密度 1420 / - kg/m³ ISO 1183
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
添加剤.
滑剤., 離型剤.
特殊な特性.
熱安定化.
領域別の利用可能性
Disclaimer
All data provided according to ISO 10350 for single points and ISO 11403 for multipoints.

Contact DuPont for Material Safety Data Sheet, general guides and/or additional information about ventilation, handling, purging, drying, etc.
Test temperatures are 23°C unless otherwise stated.

The DuPont Oval Logo, DuPont™, The miracles of science™ and ® are trademarks or registered trademarks of DuPont Company.
Copyright© 2011 E.I. du Pont de Nemours and Company. All Rights Reserved.

The information provided in this data sheet corresponds to our knowledge on the subject at the date of its publication.
This information may be subject to revision as new knowledge and experience becomes available.
The data provided fall within the normal range of product properties and relate only to the specific material designated; these data may not be
valid for such material used in combination with any other materials, additives or pigments or in any process, unless expressly indicated otherwise.
The data provided should not be used to establish specification limits or used alone as the basis of design; they are not intended to substitute
for any testing you may need to conduct to determine for yourself the suitability of a specific material for your particular purposes.
Since DuPont cannot anticipate all variations in actual end-use conditions DuPont makes no warranties and assumes no liability in connection
with any use of this information.
Nothing in this publication is to be considered as a license to operate under or a recommendation to infringe any patent rights.
DuPont advises you to seek independent counsel for a freedom to practice opinion on the intended application or end-use of our products.

CAUTION: DO NOT USE DUPONT MATERIALS IN MEDICAL APPLICATIONS INVOLVING IMPLANTATION IN THE HUMAN BODY OR
CONTACT WITH INTERNAL BODY FLUIDS OR TISSUES UNLESS THE MATERIAL HAS BEEN PROVIDED FROM DUPONT UNDER A
WRITTEN CONTRACT THAT IS CONSISTENT WITH DUPONT POLICY REGARDING MEDICAL APPLICATIONS AND EXPRESSLY
ACKNOWLEDGES THE CONTEMPLATED USE.

For further information, please contact your DuPont representative. You may also request a copy of DuPont POLICY Regarding Medical
Applications... H-50103-3 and DuPont CAUTION Regarding Medical Applications... H-50102-3.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012