CAMPUSplastics | All PA66 grades
The international CAMPUS® database offers datasheets of the following grades that are related to the polymer family: PA66.Please click on the grade of interest to generate a datasheet. You also may select a material by choosing an other polymer family or a specific producer. In addition you may select by any part of the grade name using the input box on the left.
| Grade Name | Family | Producer |
|---|---|---|
| Akulon® M-1016 | PA66-GF33 | DSM Engineering Plastics |
| Akulon® S223-D | PA66 | DSM Engineering Plastics |
| Akulon® S223-DH | PA66 | DSM Engineering Plastics |
| Akulon® S223-DK | PA66 | DSM Engineering Plastics |
| Akulon® S223-E | PA66 | DSM Engineering Plastics |
| Akulon® S223-EH | PA66 | DSM Engineering Plastics |
| Akulon® S223-F | PA66 | DSM Engineering Plastics |
| Akulon® S223-G2U | PA66-GF13 | DSM Engineering Plastics |
| Akulon® S223-G4U | PA66-GF23 | DSM Engineering Plastics |
| Akulon® S223-G6 | PA66-GF30 | DSM Engineering Plastics |
| Akulon® S223-GM35 | PA66-(GF+MD)40 | DSM Engineering Plastics |
| Akulon® S223-HG6 | PA66-GF30 | DSM Engineering Plastics |
| Akulon® S223-HG7 | PA66-GF35 | DSM Engineering Plastics |
| Akulon® S223-HM8 | PA66-MD40 | DSM Engineering Plastics |
| Akulon® S223-HPG5 | PA66-I-GF25 | DSM Engineering Plastics |
| Akulon® S223-PG8 | PA66-GF40 | DSM Engineering Plastics |
| Akulon® S227-C | PA66 | DSM Engineering Plastics |
| Akulon® S245-C | PA66 | DSM Engineering Plastics |
| ALCOM® PA66 910/1 AR10 CF10 | PA66-(CF+RF) | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 AR15 PTFE10 | (PA66+PTFE)-RF | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 AR20 | PA66-RF | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 GB30 MO2 | PA66-GB... | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 GF15 GB25 | PA66-(GF+GB)40 | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 GF15 MR25 | PA66-(GF+MX)40 | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 GF15 PTFE10 | (PA66+PTFE)-GF15 | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 GF15 PTFE18 Si2 | (PA66+PTFE)-GF... | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 GF20 GB10 | PA66-(GF+GB)30 | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 GF20 GB10 PTFE10 | (PA66+PTFE)-(GF+GB)30 | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 GF30 MO2 | PA66-GF... | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 GF30 PTFE10 Si2 | (PA66+PTFE)-GF... | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 GF30 PTFE15 | (PA66+PTFE)-GF30 | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 GF30 PTFE15 Si2 | (PA66+PTFE)-GF... | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 GF30 PTFE20 | (PA66+PTFE)-GF30 | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 MO1 | PA66... | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 MO2 | PA66... | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 PTFE20 | (PA66+PTFE) | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 SV 1057-03 MCF | PA66 | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1 UV GY1187-06MCF | PA66 | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1.1 AR10 CF10 | PA66-(CF+RF) | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1.1 CF10 | PA66-CF | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1.1 CF10 GF10 IM | PA66-I-(CF+GF)20 | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1.1 CF10 GF20 | PA66-(CF+GF)30 | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1.1 CF10 PTFE10 | (PA66+PTFE)-CF | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1.1 CF15 | PA66-CF | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1.1 CF15 GF20 | PA66-(CF+GF)35 | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1.1 CF15 TF15 Si2 | (PA66+PTFE)-CF... | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1.1 CF20 | PA66-CF | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1.1 CF30 PTFE15 | (PA66+PTFE)-CF | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1.1 CF40 | PA66-CF | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1.2 CF30 | PA66-CF | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1.3 CF/GF30 | PA66-(CF+GF) | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1.3 CF5 GF25 | PA66-(CF+GF)30 | ALBIS Plastic GmbH |
| ALCOM® PA66 910/1.9 GF30 MO2 | PA66-GF... | ALBIS Plastic GmbH |
| ALCOM® PA66 910/30.1 GF15 TCE5 | PA66... | ALBIS Plastic GmbH |
| ALCOM® PA66 910/30.1 TCE10 | PA66... | ALBIS Plastic GmbH |
| ALCOM® PA66 910/30.1 TCE2 | PA66... | ALBIS Plastic GmbH |
| ALCOM® PA66 910/30.2 TCD2 | PA66... | ALBIS Plastic GmbH |
| ALCOM® PA66 910/30.3 TCD1 | PA66... | ALBIS Plastic GmbH |
| ALCOM® PA66 910/32.1 TCE5 | PA66-X | ALBIS Plastic GmbH |
| ALCOM® PA66 910/7 GF25 MR15 | PA66-(GF+MX)40 | ALBIS Plastic GmbH |
| ALCOM® PA66 910/7GF25MR15-22-956 | PA66-(GF+MX)40 | ALBIS Plastic GmbH |
| ALCOM® PA66 910/8 GF30 PTFE15 | (PA66+PTFE)-GF30 | ALBIS Plastic GmbH |
| ALCOM® PA66 910/8 MR40 PTFE15 | (PA66+PTFE)-MX | ALBIS Plastic GmbH |
| ALTECH PA66 A 1000/109 | PA66 | ALBIS Plastic GmbH |
| ALTECH PA66 A 1000/276 | PA66 | ALBIS Plastic GmbH |
| ALTECH PA66 A 1000/310 IM | PA66-I | ALBIS Plastic GmbH |
| ALTECH PA66 A 1000/510 IM | PA66-I | ALBIS Plastic GmbH |
| ALTECH PA66 A 1000/512 IM | PA66-I | ALBIS Plastic GmbH |
| ALTECH PA66 A 2015/109 GF15 | PA66-GF15 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2015/310 GF15 IM | PA66-I-GF15 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2015/510 GF15 IM | PA66-I-GF15 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2015/710 GF15 IM | PA66-I-GF15 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2020/100 GF20 | PA66-GF20 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2020/109 GF20 | PA66-GF20 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2025/109 GF25 | PA66-GF25 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2025/567 GF25 | PA66-GF25 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2025/568 GF25 | PA66-GF25 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2025/576 GF25 | PA66-GF25 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2030/100 GF30 | PA66-GF30 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2030/106 GF30 | PA66-GF30 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2030/109 GF30 | PA66-GF30 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2030/310 GF30 IM | PA66-I-GF30 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2030/500 GF30 | PA66-GF30 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2030/507 GF30 | PA66-GF30 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2030/516 GF30 IM | PA66-I-GF30 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2030/588 GF30 | PA66-GF30 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2035/109 GF35 | PA66-GF35 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2035/310 | PA66-I-GF35 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2035/506 GF35 | PA66-I-GF35 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2035/507 GF35 EF | PA66-I-GF35 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2040/100 GF40 | PA66-GF40 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2040/310 GF40 IM | PA66-I-GF40 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2045/220 GF45 UV | PA66-GF45 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2050/100 GF50 | PA66-GF50 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2050/106 GF50 | PA66-GF50 | ALBIS Plastic GmbH |
| ALTECH PA66 A 2050/576 GF50 | PA66-GF50 | ALBIS Plastic GmbH |
| ALTECH PA66 A 3015/100 GB15 | PA66-GB15 | ALBIS Plastic GmbH |
| ALTECH PA66 A 3020/100 GB20 | PA66-GB20 | ALBIS Plastic GmbH |
| ALTECH PA66 A 3030/109 GB30 | PA66-GB30 | ALBIS Plastic GmbH |
| ALTECH PA66 A 3040/100 GB40 | PA66-GB40 | ALBIS Plastic GmbH |
| ALTECH PA66 A 4030/100 MR30 | PA66-MX30 | ALBIS Plastic GmbH |
| ALTECH PA66 A 4040/100 MR40 | PA66-MX40 | ALBIS Plastic GmbH |
| ALTECH PA66 B 1000/109 | PA66 | ALBIS Plastic GmbH |
| ALTECH PA66 B 1000/209 | PA66 | ALBIS Plastic GmbH |
| ALTECH PA66 B 1000/500 | PA66 | ALBIS Plastic GmbH |
| ALTECH PA66 B 2015/506 GF15 | PA66-GF15 | ALBIS Plastic GmbH |
| ALTECH PA66 B 2025/106 GF25 | PA66-GF25 | ALBIS Plastic GmbH |
| ALTECH PA66 B 2030/109 GF30 | PA66-GF30 | ALBIS Plastic GmbH |
| ALTECH PA66 B 2030/209 GF30 | PA66-GF30 | ALBIS Plastic GmbH |
| ALTECH PA66 B 2030/507 GF30 | PA66-GF30 | ALBIS Plastic GmbH |
| ALTECH PA66 B 3020/100 GB20 | PA66-GB20 | ALBIS Plastic GmbH |
| ALTECH PA66 B 3050/100 GB50 | PA66-GB50 | ALBIS Plastic GmbH |
| ALTECH PA66+PA6 A 1000/567 | (PA66+PA6) | ALBIS Plastic GmbH |
| ALTECH PA66+PP A 2030/577 GF30 | (PA66+PP)-GF30 | ALBIS Plastic GmbH |
| ALTECH PA66+PP A 2030/578 | (PA66+PP)-GF30 | ALBIS Plastic GmbH |
| BERGAMID® A70/75/80 | PA66 | PolyOne Engineered Materials Europe |
| BERGAMID® A700/750 | PA66 | PolyOne Engineered Materials Europe |
| BERGAMID® A700G10H | PA66-GF10 | PolyOne Engineered Materials Europe |
| BERGAMID® A700G10U-SO | PA66-GF10 | PolyOne Engineered Materials Europe |
| BERGAMID® A700G15H | PA66-GF15 | PolyOne Engineered Materials Europe |
| BERGAMID® A700G15U-SO | PA66-GF15 | PolyOne Engineered Materials Europe |
| BERGAMID® A700G20H | PA66-GF20 | PolyOne Engineered Materials Europe |
| BERGAMID® A700G20U-SO | PA66-GF20 | PolyOne Engineered Materials Europe |
| BERGAMID® A700G25H | PA66-GF25 | PolyOne Engineered Materials Europe |
| BERGAMID® A700G25U | PA66-GF25 | PolyOne Engineered Materials Europe |
| BERGAMID® A700G25U-SO | PA66-GF25 | PolyOne Engineered Materials Europe |
| BERGAMID® A700G30H | PA66-GF30 | PolyOne Engineered Materials Europe |
| BERGAMID® A700G30U-SO | PA66-GF30 | PolyOne Engineered Materials Europe |
| BERGAMID® A700G35H | PA66-GF35 | PolyOne Engineered Materials Europe |
| BERGAMID® A700G35U-SO | PA66-GF35 | PolyOne Engineered Materials Europe |
| BERGAMID® A700G40H | PA66-GF40 | PolyOne Engineered Materials Europe |
| BERGAMID® A700G45H | PA66-GF45 | PolyOne Engineered Materials Europe |
| BERGAMID® A700G50H | PA66-GF50 | PolyOne Engineered Materials Europe |
| BERGAMID® A700GK25U-SO | PA66-GB25 | PolyOne Engineered Materials Europe |
| BERGAMID® A700MI40 | PA66-MD40 | PolyOne Engineered Materials Europe |
| BERGAMID® A700MOS2 | PA66 | PolyOne Engineered Materials Europe |
| BERGAMID® A700PM-Y | PA66 | PolyOne Engineered Materials Europe |
| BERGAMID® A700TM-YF | PA66 | PolyOne Engineered Materials Europe |
| BERGAMID® A70C10 | PA66-CF10 | PolyOne Engineered Materials Europe |
| BERGAMID® A70C20 | PA66-CF20 | PolyOne Engineered Materials Europe |
| BERGAMID® A70G/GK30 | PA66-(GF+GB)30 | PolyOne Engineered Materials Europe |
| BERGAMID® A70G10 | PA66-GF10 | PolyOne Engineered Materials Europe |
| BERGAMID® A70G15 | PA66-GF15 | PolyOne Engineered Materials Europe |
| BERGAMID® A70G15TM-Z | PA66-GF15 | PolyOne Engineered Materials Europe |
| BERGAMID® A70G15U | PA66-GF15 | PolyOne Engineered Materials Europe |
| BERGAMID® A70G20 | PA66-GF20 | PolyOne Engineered Materials Europe |
| BERGAMID® A70G20/GK10H | PA66-(GF+GB)30 | PolyOne Engineered Materials Europe |
| BERGAMID® A70G25 | PA66-GF25 | PolyOne Engineered Materials Europe |
| BERGAMID® A70G30 | PA66-GF30 | PolyOne Engineered Materials Europe |
| BERGAMID® A70G30MOS2 | PA66-GF30 | PolyOne Engineered Materials Europe |
| BERGAMID® A70G30TF15 | PA66-GF30 | PolyOne Engineered Materials Europe |
| BERGAMID® A70G30TM-Z | PA66-GF30 | PolyOne Engineered Materials Europe |
| BERGAMID® A70G35 | PA66-GF35 | PolyOne Engineered Materials Europe |
| BERGAMID® A70G40 | PA66-GF40 | PolyOne Engineered Materials Europe |
| BERGAMID® A70G45 | PA66-GF45 | PolyOne Engineered Materials Europe |
| BERGAMID® A70G50 | PA66-GF50 | PolyOne Engineered Materials Europe |
| BERGAMID® A70GK15TM-Z | PA66-GB15 | PolyOne Engineered Materials Europe |
| BERGAMID® A70GK20 | PA66-GB20 | PolyOne Engineered Materials Europe |
| BERGAMID® A70GK30 | PA66-GB30 | PolyOne Engineered Materials Europe |
| BERGAMID® A70GK30 MOS2 | PA66-GB30 | PolyOne Engineered Materials Europe |
| BERGAMID® A70GK35 | PA66-GB35 | PolyOne Engineered Materials Europe |
| BERGAMID® A70GK40 | PA66-GB40 | PolyOne Engineered Materials Europe |
| BERGAMID® A70MI20HWTM-X | PA66-MD20 | PolyOne Engineered Materials Europe |
| BERGAMID® A70MI30 | PA66-MD30 | PolyOne Engineered Materials Europe |
| BERGAMID® A70MI40 | PA66-MD40 | PolyOne Engineered Materials Europe |
| BERGAMID® A70MOS2 | PA66 | PolyOne Engineered Materials Europe |
| BERGAMID® A70PM-Z | PA66 | PolyOne Engineered Materials Europe |
| BERGAMID® A70TM-X | PA66 | PolyOne Engineered Materials Europe |
| BERGAMID® A70TM-Y | PA66 | PolyOne Engineered Materials Europe |
| BERGAMID® A70TM-YF | PA66 | PolyOne Engineered Materials Europe |
| BERGAMID® A70TM-Z | PA66 | PolyOne Engineered Materials Europe |
| BERGAMID® A70W25 | PA66 | PolyOne Engineered Materials Europe |
| BERGAMID® A800H | PA66 | PolyOne Engineered Materials Europe |
| CELSTRAN PA66-AF35-02-US | PA66-RF35 | Ticona |
| CELSTRAN PA66-CF40-01-US | PA66-CF40 | Ticona |
| CELSTRAN PA66-GF20-02P11/12 | PA66-GF20 | Ticona |
| CELSTRAN PA66-GF30-02 | PA66-GF30 | Ticona |
| CELSTRAN PA66-GF30-07 | PA66-GF30 | Ticona |
| CELSTRAN PA66-GF40-01 | PA66-GF40 | Ticona |
| CELSTRAN PA66-GF40-02-US | PA66-GF40 | Ticona |
| CELSTRAN PA66-GF40-02P11 | PA66-GF40 | Ticona |
| CELSTRAN PA66-GF40-02P11/15 | PA66-GF40 | Ticona |
| CELSTRAN PA66-GF40-07 | PA66-GF40 | Ticona |
| CELSTRAN PA66-GF40-BV340C P11/3x | PA66-GF40 | Ticona |
| CELSTRAN PA66-GF50-02 AD3007 | PA66-GF50 | Ticona |
| CELSTRAN PA66-GF50-02 P11 | PA66-GF50 | Ticona |
| CELSTRAN PA66-GF50-02 P11/14 | PA66-GF50 | Ticona |
| CELSTRAN PA66-GF50-02 P7 | PA66-GF50 | Ticona |
| CELSTRAN PA66-GF50-02 P7/12 | PA66-GF50 | Ticona |
| CELSTRAN PA66-GF50-02-US | PA66-GF50 | Ticona |
| CELSTRAN PA66-GF50-07 | PA66-GF50 | Ticona |
| CELSTRAN PA66-GF50-20 | PA66-GF50 | Ticona |
| CELSTRAN PA66-GF50-20 AD3007 | PA66-GF50 | Ticona |
| CELSTRAN PA66-GF60-02 P11/12 | PA66-GF60 | Ticona |
| CELSTRAN PA66-GF60-02 P11/14 | PA66-GF60 | Ticona |
| CELSTRAN PA66-GF60-02-US | PA66-GF60 | Ticona |
| CELSTRAN PA66-SF10-02 | PA66-MF(x)10 | Ticona |
| CELSTRAN PA66-SF50-02 AF3001 | PA66-MF(x)50 | Ticona |
| CELSTRAN PA66-SF6-02 | PA66-MF(x)6 | Ticona |
| Durethan® A 30 | PA66 | LANXESS Deutschland GmbH |
| Durethan® A 30 H2.0 | PA66 | LANXESS Deutschland GmbH |
| Durethan® A 30 H3.0 | PA66 | LANXESS Deutschland GmbH |
| Durethan® A 30 S | PA66 | LANXESS Deutschland GmbH |
| Durethan® A 30 S FN31 | PA66 FR | LANXESS Deutschland GmbH |
| Durethan® AC 30 DUS027 | PA66 | LANXESS Deutschland GmbH |
| Durethan® AC 30 H3.0 | PA66 | LANXESS Deutschland GmbH |
| Durethan® AKV 15 | PA66-GF15 | LANXESS Deutschland GmbH |
| Durethan® AKV 15 H2.0 | PA66-GF15 | LANXESS Deutschland GmbH |
| Durethan® AKV 15 H3.0 | PA66-GF15 | LANXESS Deutschland GmbH |
| Durethan® AKV 25 F30 | PA66-GF25 FR | LANXESS Deutschland GmbH |
| Durethan® AKV 30 | PA66-GF30 | LANXESS Deutschland GmbH |
| Durethan® AKV 30 G H2.0 SR1 | PA66-GF30 | LANXESS Deutschland GmbH |
| Durethan® AKV 30 G HR DUS023 | PA66-GF30 | LANXESS Deutschland GmbH |
| Durethan® AKV 30 GIT H2.0 | PA66-GF30 | LANXESS Deutschland GmbH |
| Durethan® AKV 30 H2.0 | PA66-GF30 | LANXESS Deutschland GmbH |
| Durethan® AKV 30 H3.0 | PA66-GF30 | LANXESS Deutschland GmbH |
| Durethan® AKV 30 HR H2.0 | PA66-GF30 | LANXESS Deutschland GmbH |
| Durethan® AKV 325 H2.0 | PA66-GF25 | LANXESS Deutschland GmbH |
| Durethan® AKV 35 CX H2.0 | PA66-GF35 | LANXESS Deutschland GmbH |
| Durethan® AKV 35 H2.0 | PA66-GF35 | LANXESS Deutschland GmbH |
| Durethan® AKV 35 H3.0 | PA66-GF35 | LANXESS Deutschland GmbH |
| Durethan® AKV 40 H3.0 | PA66-GF40 | LANXESS Deutschland GmbH |
| Durethan® AKV 50 H2.0 | PA66-GF50 | LANXESS Deutschland GmbH |
| Durethan® AKV 50 H3.0 | PA66-GF50 | LANXESS Deutschland GmbH |
| Durethan® AM 40 X H2.0 | PA66-(GF+MD)40 | LANXESS Deutschland GmbH |
| Durethan® C 38 F | PA66 | LANXESS Deutschland GmbH |
| Durethan® C 38 FKS | PA66 | LANXESS Deutschland GmbH |
| Durethan® DP 2-2224/30 H2.0 | PA66-(MD+GF)30 | LANXESS Deutschland GmbH |
| Durethan® DP 2-2240/15 H2.0 | PA66-GF15 | LANXESS Deutschland GmbH |
| Durethan® DP 2325 H3.0 | PA66 | LANXESS Deutschland GmbH |
| Durethan® DP 2801 | PA66 FR | LANXESS Deutschland GmbH |
| Durethan® DP 2802/30 | PA66-GF30 FR | LANXESS Deutschland GmbH |
| Durethan® DP A 30 S FN30 | PA66 | LANXESS Deutschland GmbH |
| Durethan® DP A 32 | PA66 | LANXESS Deutschland GmbH |
| Durethan® DP AKV 30 FN00 | PA66-GF30 FR | LANXESS Deutschland GmbH |
| Durethan® DP AKV 30 HR EF | PA66-GF30 | LANXESS Deutschland GmbH |
| Durethan® DP AKV 30 X HR EF | PA66-GF30 | LANXESS Deutschland GmbH |
| Durethan® DP AKV 35 LT H2.0 | PA66-GF35 | LANXESS Deutschland GmbH |
| Durethan® DP AKV 50 H2.0 EF | PA66-GF50 | LANXESS Deutschland GmbH |
| Durethan® DP AKV 50 HR H2.0 | PA66-GF50 | LANXESS Deutschland GmbH |
| Grilon AG-25 HM | PA66-GF25 | EMS-GRIVORY - a unit of EMS-CHEMIE AG |
| Grilon AG-30 | PA66-GF30 | EMS-GRIVORY - a unit of EMS-CHEMIE AG |
| Grilon AG-30 H | PA66 | EMS-GRIVORY - a unit of EMS-CHEMIE AG |
| Grilon AG-30 LF 15 | PA66-(GF+Z)45 | EMS-GRIVORY - a unit of EMS-CHEMIE AG |
| Grilon AG-35 | PA66-GF35 | EMS-GRIVORY - a unit of EMS-CHEMIE AG |
| Grilon AS LF 20 | PA66-Z20 | EMS-GRIVORY - a unit of EMS-CHEMIE AG |
| Grilon AS V0 | PA66 | EMS-GRIVORY - a unit of EMS-CHEMIE AG |
| Grilon AS/2 | PA66 | EMS-GRIVORY - a unit of EMS-CHEMIE AG |
| Grilon AZ 3 | PA66 | EMS-GRIVORY - a unit of EMS-CHEMIE AG |
| Grilon AZ 3/2 | PA66 | EMS-GRIVORY - a unit of EMS-CHEMIE AG |
| Minlon® 10B140 BK061 | PA66-MD40 | DuPont Engineering Polymers |
| Minlon® 10B40 NC010 | PA66-MD40 | DuPont Engineering Polymers |
| Minlon® 10B40HS1 BK061 | PA66-MD40 | DuPont Engineering Polymers |
| Minlon® 11C140 NC010 | PA66-I-MD40 | DuPont Engineering Polymers |
| Minlon® 11C40 NC010 | PA66-I-MD40 | DuPont Engineering Polymers |
| Minlon® 12T NC010 | PA66-I-MD36 | DuPont Engineering Polymers |
| Minlon® 12TA BKB124 | PA66-I-MD32 | DuPont Engineering Polymers |
| Minlon® 22C NC010 | PA66-(MD+GF)38 | DuPont Engineering Polymers |
| Minlon® EFE6053 BK413 | PA66-(MD+GF)40 | DuPont Engineering Polymers |
| Minlon® EFE6096 GY090A | PA66-I-MD15 | DuPont Engineering Polymers |
| Minlon® FE6190 BK086 | PA66-(MD+GF)36 | DuPont Engineering Polymers |
| Minlon® IG38C1 BK434 | PA66-(MD+GF)38 | DuPont Engineering Polymers |
| Novamid® 3010SR | PA66 | DSM Engineering Plastics |
| Orgalloy® RS 6600 | PA66... | ARKEMA |
| Orgalloy® RS 6620 | PA66-GF20... | ARKEMA |
| Orgalloy® RS 6630 | PA66-GF30... | ARKEMA |
| Orgalloy® RS 6635 A | PA66-GF35... | ARKEMA |
| RADIFLAM® A AE | PA66 FR | RadiciPlastics |
| RADIFLAM® A FR | PA66 FR | RadiciPlastics |
| RADIFLAM® A RV250AF | PA66-GF25 FR | RadiciPlastics |
| RADIFLAM® A RV250FR | PA66-GF25 FR | RadiciPlastics |
| RADIFLAM® A RV300AE | PA66-GF30 FR | RadiciPlastics |
| RADIFLAM® A RV300AF | PA66-GF30 FR | RadiciPlastics |
| RADIFLAM® A RV350AF | PA66-GF35 FR | RadiciPlastics |
| RADILON® A 35E 990 | PA66 | RadiciPlastics |
| RADILON® A 38 | PA66 | RadiciPlastics |
| RADILON® A 42 | PA66 | RadiciPlastics |
| RADILON® A CF350 | PA66-CF35 | RadiciPlastics |
| RADILON® A CP300K | PA66-MX30 | RadiciPlastics |
| RADILON® A CP400 | PA66-MX40 | RadiciPlastics |
| RADILON® A CV300LK | PA66-GB30 | RadiciPlastics |
| RADILON® A ECP3808 | PA66-I-MX30 | RadiciPlastics |
| RADILON® A ERV1906LK | PA66-I-GF13 | RadiciPlastics |
| RADILON® A ERV3012 | PA66-I-GF18 | RadiciPlastics |
| RADILON® A ESL128 | PA66-I | RadiciPlastics |
| RADILON® A HS | PA66 | RadiciPlastics |
| RADILON® A HSK | PA66 | RadiciPlastics |
| RADILON® A HSX | PA66-I | RadiciPlastics |
| RADILON® A HSX88 | PA66-I | RadiciPlastics |
| RADILON® A LX14080 | PA66 | RadiciPlastics |
| RADILON® A RCF3505 | PA66-(CF+GF)35 | RadiciPlastics |
| RADILON® A RV150 | PA66-GF15 | RadiciPlastics |
| RADILON® A RV200 | PA66-GF20 | RadiciPlastics |
| RADILON® A RV250 | PA66-GF25 | RadiciPlastics |
| RADILON® A RV300 | PA66-GF30 | RadiciPlastics |
| RADILON® A RV300 990 | PA66-GF30 | RadiciPlastics |
| RADILON® A RV300R | PA66-GF30 | RadiciPlastics |
| RADILON® A RV300RKC | PA66-GF30 | RadiciPlastics |
| RADILON® A RV330 | PA66-GF33 | RadiciPlastics |
| RADILON® A RV350 | PA66-GF35 | RadiciPlastics |
| RADILON® A RV400 | PA66-GF40 | RadiciPlastics |
| RADILON® A RV500 | PA66-GF50 | RadiciPlastics |
| RADILON® A USX200 | PA66-I | RadiciPlastics |
| RADILON® A USZ200 | PA66-I | RadiciPlastics |
| SCHULAMID® 66 CF 20 H | PA66-CF20 | A. Schulman GmbH |
| SCHULAMID® 66 GB 30 H | PA66-GB30 | A. Schulman GmbH |
| SCHULAMID® 66 GBF 3020 | PA66-(GB+GF)30 | A. Schulman GmbH |
| SCHULAMID® 66 GBF 3020 FR 4 | PA66-(GB+GF)30 FR | A. Schulman GmbH |
| SCHULAMID® 66 GF 15 H | PA66-GF15 | A. Schulman GmbH |
| SCHULAMID® 66 GF 15 HI H | PA66-I-GF15 | A. Schulman GmbH |
| SCHULAMID® 66 GF 15 HI K2034 | PA66-I-GF15 | A. Schulman GmbH |
| SCHULAMID® 66 GF 25 FR 5 A | PA66-GF25 FR | A. Schulman GmbH |
| SCHULAMID® 66 GF 25 H | PA66-GF25 | A. Schulman GmbH |
| SCHULAMID® 66 GF 30 FR 2 | PA66-GF30 FR | A. Schulman GmbH |
| SCHULAMID® 66 GF 30 GID | PA66-GF30 | A. Schulman GmbH |
| SCHULAMID® 66 GF 30 GID K1802 | PA66-GF30 | A. Schulman GmbH |
| SCHULAMID® 66 GF 30 H | PA66-GF30 | A. Schulman GmbH |
| SCHULAMID® 66 GF 30 H BLACK REC | PA66-GF30 | A. Schulman GmbH |
| SCHULAMID® 66 GF 30 HE LW | PA66-GF30 | A. Schulman GmbH |
| SCHULAMID® 66 GF 30 HI | PA66-I-GF30 | A. Schulman GmbH |
| SCHULAMID® 66 GF 30 HR | PA66-GF30 | A. Schulman GmbH |
| SCHULAMID® 66 GF 35 H | PA66-GF35 | A. Schulman GmbH |
| SCHULAMID® 66 GF 35 H BLACK REC | PA66-GF35 | A. Schulman GmbH |
| SCHULAMID® 66 GF 35 HE GREY 967826 | PA66-GF35 | A. Schulman GmbH |
| SCHULAMID® 66 GF 50 H | PA66-GF50 | A. Schulman GmbH |
| SCHULAMID® 66 GRF 2318 H | PA66-(GF+CD)23 | A. Schulman GmbH |
| SCHULAMID® 66 MK 30 HI H K1357 | PA66-I-MX30 | A. Schulman GmbH |
| SCHULAMID® 66 MKF 4015 | PA66-(GF+MD)40 | A. Schulman GmbH |
| SCHULAMID® 66 MNF 2510 H | PA66-(MX+GF)25 | A. Schulman GmbH |
| SCHULAMID® 66 MV 2 | PA66 | A. Schulman GmbH |
| SCHULAMID® 66 MV HI | PA66-I | A. Schulman GmbH |
| SCHULAMID® 66 MV HI H K1416 | PA66-I | A. Schulman GmbH |
| SCHULAMID® 66 MV HI HH K2300 | PA66-I | A. Schulman GmbH |
| SCHULAMID® 66 MV HI K1416 | PA66-I | A. Schulman GmbH |
| SCHULAMID® 66 MV HI TST | PA66-I | A. Schulman GmbH |
| SCHULAMID® 66 MW 30 FR 4 | PA66-MD30 FR | A. Schulman GmbH |
| SCHULAMID® 66 MW 30 FR 4 K2031 | PA66-MX30 FR | A. Schulman GmbH |
| SCHULAMID® 66 MW 30 FR 4 K2230 | PA66-MX30 FR | A. Schulman GmbH |
| SCHULAMID® 66 SK 1000 | PA66-I | A. Schulman GmbH |
| SCHULAMID® 66/6 MT 20 K1849 | (PA6+PA66)-T20 | A. Schulman GmbH |
| Technyl® 2710IR | PA66-I | Rhodia Polyamide Engineering Plastics |
| Technyl® A 20 V25 | PA66-GF25 FR | Rhodia Polyamide Engineering Plastics |
| Technyl® A 20 V35 | PA66-GF35 FR | Rhodia Polyamide Engineering Plastics |
| Technyl® A 205F | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 208F | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 21 T3 V25 | PA66-GF25 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 216 | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 216 NAT FA | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 216 S30 | PA66-GB30 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 216 S40 | PA66-GB40 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 216 V20 | PA66-GF20 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 216 V30 | PA66-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 216 V30 Natural FA | PA66-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 216 V33 | PA66-GF33 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 216T V33 BLACK 1N | PA66-GF33 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 217 | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 MZ15 V25 | PA66-(GF+MF)40 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 S30 | PA66-GB30 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 S40 | PA66-GB40 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 V15 | PA66-GF15 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 V20 | PA66-GF20 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 V25 | PA66-GF25 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 V25 black 21NHFE | PA66-GF25 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 V25 Nat BA | PA66-GF25 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 V25 Natural B | PA66-GF25 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 V30 | PA66-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 V30 Black 21 NHFE | PA66-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 V30 black 34NG | PA66-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 V30 Black 34NG-K | PA66-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 V35 | PA66-GF35 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 V35 black 21NHFE | PA66-GF35 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 V35 black 34NG | PA66-GF35 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 V40 | PA66-GF40 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 V40 black 21NHFE | PA66-GF40 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218 V50 | PA66-GF50 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218C V10 | PA66-GF10 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218G V30 | PA66-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218G V33 BLACK 34N | PA66-GF33 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218G1 V25 BLACK 34N | PA66-GF25 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218G1 V30 BLACK 34N | PA66-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218G2 V30 BLACK 34N | PA66-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218HP V30 black 21N | PA66-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218HP V35 black 21N | PA66-GF35 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218HP V50 black 21N | PA66-GF50 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218W V30 | PA66-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218W V30 black FA | PA66-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 218W V33 Natural T | PA66-GF33 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 221 | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 221 Natural FA | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 222 | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 225F | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 230 | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 238 | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 238 V13 | PA66-GF13 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 246M | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 248 V33 | PA66-GF33 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 258 P1 Black 2N | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 30G1 | PA66 FR | Rhodia Polyamide Engineering Plastics |
| Technyl® A 30H1 V25 | PA66-GF25 FR | Rhodia Polyamide Engineering Plastics |
| Technyl® A 30H1 V30 | PA66-GF30 FR | Rhodia Polyamide Engineering Plastics |
| Technyl® A 32G1 | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 402 | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 402 H1 | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 402 Natural FA | PA66 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 50H1 | PA66 FR | Rhodia Polyamide Engineering Plastics |
| Technyl® A 52 G1 MX 20 | PA66-MF | Rhodia Polyamide Engineering Plastics |
| Technyl® A 548B2 V15 Black 23N | PA66-GF15 | Rhodia Polyamide Engineering Plastics |
| Technyl® A 60 G1 V25 | PA66-GF25 FR | Rhodia Polyamide Engineering Plastics |
| Technyl® A 60 G2 V30 | PA66-GF30 FR | Rhodia Polyamide Engineering Plastics |
| Technyl® A 60G1 V30 | PA66-GF30 FR | Rhodia Polyamide Engineering Plastics |
| Technyl® A 718 V30 | PA66-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® AFX 218 V50 | PA66-GF50 | Rhodia Polyamide Engineering Plastics |
| Technyl® AFX 218 V60 | PA66-GF60 | Rhodia Polyamide Engineering Plastics |
| Technyl® AR 130/GF BLACK | PA66-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® AR 218 V30 Black | PA66-GF30 | Rhodia Polyamide Engineering Plastics |
| Technyl® D 247F | (PA66+PA610)-I | Rhodia Polyamide Engineering Plastics |
| TROGAMID® BX9724 blk (sw) | (PANDT/INDT+PA66)-GF40 | Evonik Industries AG |
| Ultramid® 1000-11 NF2001 | PA66 | BASF |
| Ultramid® 1000-2 NF2001 | PA66 | BASF |
| Ultramid® 1003-2 NF2002 | PA66 | BASF |
| Ultramid® 1310-11 NF2001 | PA66 | BASF |
| Ultramid® 1403-2 BK ND3007 | PA66-GF13 | BASF |
| Ultramid® 1403-2 NF3001 | PA66-GF13 | BASF |
| Ultramid® 1503-2 BK ND3007 | PA66-GF33 | BASF |
| Ultramid® 1503-2 NF2004 | PA66-GF33 | BASF |
| Ultramid® 1603-2 BK ND3007 | PA66-GF43 | BASF |
| Ultramid® 1603-2 NF2004 | PA66-GF43 | BASF |
| Ultramid® 1703-2 BK ND3007 | PA66-GF25 | BASF |
| Ultramid® 7423-2 NF3001 | PA66-GF13 | BASF |
| Ultramid® 7523-2AM BK ND3007 | PA66-GF33 | BASF |
| Ultramid® A3EG10 | PA66-GF50 | BASF |
| Ultramid® A3EG5 | PA66-GF25 | BASF |
| Ultramid® A3EG6 | PA66-GF30 | BASF |
| Ultramid® A3EG7 | PA66-GF35 | BASF |
| Ultramid® A3HG5 | PA66-GF25 | BASF |
| Ultramid® A3HG6 HR bk 23591 | PA66-GF30 | BASF |
| Ultramid® A3HG6 WIT bk20560 | (PA66+PA6/6T)-(GF+GB)30 | BASF |
| Ultramid® A3HG7 | PA66-GF35 | BASF |
| Ultramid® A3K | PA66 | BASF |
| Ultramid® A3L HP | PA66 | BASF |
| Ultramid® A3U40G5 | PA66-GF25 FR | BASF |
| Ultramid® A3UG5 | PA66-GF25 FR | BASF |
| Ultramid® A3W | PA66 | BASF |
| Ultramid® A3W2G10 bk20560 | PA66-GF50 | BASF |
| Ultramid® A3WG10 | PA66-GF50 | BASF |
| Ultramid® A3WG3 | PA66-GF15 | BASF |
| Ultramid® A3WG5 | PA66-GF25 | BASF |
| Ultramid® A3WG6 | PA66-GF30 | BASF |
| Ultramid® A3WG6 HRX bk 23591 | PA66-GF30 | BASF |
| Ultramid® A3WG7 | PA66-GF35 | BASF |
| Ultramid® A3WG8 bk20560 | PA66-GF40 | BASF |
| Ultramid® A3WGM53 bk 20560 | PA66-(GF+MD)40 | BASF |
| Ultramid® A3X2G10 | PA66-GF50 FR | BASF |
| Ultramid® A3X2G5 | PA66-GF25 FR | BASF |
| Ultramid® A3X2G7 | PA66-GF35 FR | BASF |
| Ultramid® A3XZG5 | PA66-I-GF25 FR(52) | BASF |
| Ultramid® A3Z | PA66-I | BASF |
| Ultramid® A3Z HP | PA66 | BASF |
| Ultramid® A3ZG6 bk 20591 | PA66-I-GF30 | BASF |
| Ultramid® A4H | PA66 | BASF |
| Ultramid® N-265 NF3001 | PA66-MF40 | BASF |
| Ultramid® N-276 NF3001 | PA66-(GF+MF)40 | BASF |
| Ultramid® N-333 NF3001 | PA66-GF33 | BASF |
| Ultramid® NBX-0025 NF2001 | PA66 | BASF |
| Ultramid® NFX-0102 NF2004 | PA66-GF30 | BASF |
| Zytel® 101 NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® 101F NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® 101L NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® 103FHS NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® 103FHSA NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® 103HSL NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® 105F BK010 | PA66 | DuPont Engineering Polymers |
| Zytel® 132F NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® 135F NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® 42A NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® 444AHS BK152 | PA66-I | DuPont Engineering Polymers |
| Zytel® 45HSB NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® 70G13HS1L NC010 | PA66-GF13 | DuPont Engineering Polymers |
| Zytel® 70G13L NC010 | PA66-GF13 | DuPont Engineering Polymers |
| Zytel® 70G20HSL NC010 | PA66-GF20 | DuPont Engineering Polymers |
| Zytel® 70G25HSL NC010 | PA66-GF25 | DuPont Engineering Polymers |
| Zytel® 70G25HSLR NC010 | PA66-GF25 | DuPont Engineering Polymers |
| Zytel® 70G30HSL BK039B | PA66-GF30 | DuPont Engineering Polymers |
| Zytel® 70G30HSLR NC010 | PA66-GF30 | DuPont Engineering Polymers |
| Zytel® 70G30L NC010 | PA66-GF30 | DuPont Engineering Polymers |
| Zytel® 70G33HS1L NC010 | PA66-GF33 | DuPont Engineering Polymers |
| Zytel® 70G33HSL BK083 | PA66-GF33 | DuPont Engineering Polymers |
| Zytel® 70G33L NC010 | PA66-GF33 | DuPont Engineering Polymers |
| Zytel® 70G35EF NC010 | PA66-GF35 | DuPont Engineering Polymers |
| Zytel® 70G35HSL NC010 | PA66-GF35 | DuPont Engineering Polymers |
| Zytel® 70G35HSLRA4 BK267 | PA66-GF35 | DuPont Engineering Polymers |
| Zytel® 70G35HSLX BK357 | PA66-GF35 | DuPont Engineering Polymers |
| Zytel® 70G35HSRX BK099 | PA66-GF35 | DuPont Engineering Polymers |
| Zytel® 70G43HSLA BK099 | PA66-GF43 | DuPont Engineering Polymers |
| Zytel® 70G43L NC010 | PA66-GF43 | DuPont Engineering Polymers |
| Zytel® 70G50HSLA BK039B | PA66-GF50 | DuPont Engineering Polymers |
| Zytel® 70GB30HSL NC010 | PA66-GB30 | DuPont Engineering Polymers |
| Zytel® 70K20HSL NC010 | PA66-RF20 | DuPont Engineering Polymers |
| Zytel® 74G33J NC010 | (PA66+PA6)-GF33 | DuPont Engineering Polymers |
| Zytel® 74G33W BK196 | (PA66+PA6)-GF33 | DuPont Engineering Polymers |
| Zytel® 79G13HSL NC010 | PA66-I-GF13 | DuPont Engineering Polymers |
| Zytel® 79G13L NC010 | PA66-I-GF13 | DuPont Engineering Polymers |
| Zytel® 8018HS NC010 | PA66-I-GF14 | DuPont Engineering Polymers |
| Zytel® 80G14A NC010A | PA66-I-GF14 | DuPont Engineering Polymers |
| Zytel® 80G14AHS NC010 | PA66-I-GF14 | DuPont Engineering Polymers |
| Zytel® 80G33HS1L NC010 | PA66-I-GF33 | DuPont Engineering Polymers |
| Zytel® 80G33L NC010 | PA66-I-GF33 | DuPont Engineering Polymers |
| Zytel® 80G43HS1L BK104 | PA66-I-GF43 | DuPont Engineering Polymers |
| Zytel® 84G33 BKB031 | (PA66+PA6)-I-GF33 | DuPont Engineering Polymers |
| Zytel® BM70G15HSLR BK537 | PA66-I-GF15 | DuPont Engineering Polymers |
| Zytel® BM70G20HSLX BK537 | PA66-I-GF20 | DuPont Engineering Polymers |
| Zytel® E41HSB NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® E42A NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® E51HSB NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® E53 NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® EFE1068 NC010T | PA66 | DuPont Engineering Polymers |
| Zytel® EFE8089B BK416 | PA66-I-GF33 | DuPont Engineering Polymers |
| Zytel® FE270038 BK267 | PA66-(GF+MD)40 | DuPont Engineering Polymers |
| Zytel® FE270046 BK267 | (PA66+PA6T/XT)-GF30 | DuPont Engineering Polymers |
| Zytel® FE270050 BK099 | PA66-(GF+MD)30 | DuPont Engineering Polymers |
| Zytel® FE3071 NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® FE4200 BK136 | PA66-I | DuPont Engineering Polymers |
| Zytel® FG101L NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® FG133F1 NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® FG408L NC010 | PA66-I | DuPont Engineering Polymers |
| Zytel® FG42A NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® FG42L NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® FG50 NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® FG53 NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® FG70G30HSLR NC010 | PA66-GF30 | DuPont Engineering Polymers |
| Zytel® FGFE5171 NC010 | PA66-GF33 | DuPont Engineering Polymers |
| Zytel® FN714 NC010A | PA66... | DuPont Engineering Polymers |
| Zytel® FN718 NC010A | PA66... | DuPont Engineering Polymers |
| Zytel® FR50 NC010A | PA66-GF25 FR(17) | DuPont Engineering Polymers |
| Zytel® FR7025V0F NC010 | PA66 FR(30) | DuPont Engineering Polymers |
| Zytel® FR7026V0F NC010 | PA66 FR(30) | DuPont Engineering Polymers |
| Zytel® FR70G25V0 NC010 | PA66-GF25 FR(17) | DuPont Engineering Polymers |
| Zytel® FR70M30V0 NC010 | PA66-MD30 FR(17) | DuPont Engineering Polymers |
| Zytel® LM70G35HSLX BK314 | PA66-GF35 | DuPont Engineering Polymers |
| Zytel® MT409AHS NC010 | PA66-I | DuPont Engineering Polymers |
| Zytel® PC310 NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® PLS90G30DR BK099 | PA66-GF30 | DuPont Engineering Polymers |
| Zytel® SC310 NC010 | PA66 | DuPont Engineering Polymers |
| Zytel® ST800HSL BK152 | PA66-I | DuPont Engineering Polymers |
| Zytel® ST801 BK010A | PA66-I | DuPont Engineering Polymers |
| Zytel® ST801A NC010A | PA66-I | DuPont Engineering Polymers |
| Zytel® ST801AHS NC010 | PA66-I | DuPont Engineering Polymers |
| Zytel® ST801AW NC010 | PA66-I | DuPont Engineering Polymers |