CAMPUSplastics | All PBT grades
The international CAMPUS® database offers datasheets of the following grades that are related to the polymer family: PBT.Please click on the grade of interest to generate a datasheet. You also may select a material by choosing an other polymer family or a specific producer. In addition you may select by any part of the grade name using the input box on the left.
| Grade Name | Family | Producer |
|---|---|---|
| ALCOM® PBT 700/1 GF20 PTFE15 | (PBT+PTFE)-GF20 | ALBIS Plastic GmbH |
| ALCOM® PBT 700/1 GF30 PTFE15 | (PBT+PTFE)-GF30 | ALBIS Plastic GmbH |
| ALCOM® PBT 700/1 GF30 PTFE15 Si2 | (PBT+PTFE)-GF... | ALBIS Plastic GmbH |
| ALCOM® PBT 700/1 PTFE20 | (PBT+PTFE) | ALBIS Plastic GmbH |
| ALCOM® PBT 700/1.1 CF20 PTFE15 | (PBT+PTFE)-CF | ALBIS Plastic GmbH |
| ALCOM® PBT 700/1.5 GF15 PTFE15 | (PBT+PTFE)-GF15 | ALBIS Plastic GmbH |
| ALCOM® PBT 700/1.5 GF15 PTFE15 HR | (PBT+PTFE)-GF15 | ALBIS Plastic GmbH |
| ALCOM® PBT 700/2 WT 31-956 LB | PBT | ALBIS Plastic GmbH |
| ALCOM® PBT 700/30.1 TCE10 | PBT... | ALBIS Plastic GmbH |
| ALCOM® PBT 700/30.2 TCD2 | PBT... | ALBIS Plastic GmbH |
| ALCOM® PBT 700/8 GF15 PTFE15 | (PBT+PTFE)-GF15 | ALBIS Plastic GmbH |
| ALTECH PBT A 1000/506 | PBT | ALBIS Plastic GmbH |
| ALTECH PBT A 1000/507 | PBT | ALBIS Plastic GmbH |
| ALTECH PBT A 2020/340 GF20 FR | PBT-GF20 FR | ALBIS Plastic GmbH |
| ALTECH PBT A 2020/510 GF20 IM | PBT-I-GF20 | ALBIS Plastic GmbH |
| ALTECH PBT A 2030/340 GF30 FR | PBT-GF30 FR | ALBIS Plastic GmbH |
| ALTECH PBT A 3030/100 GB30 | PBT-GB30 | ALBIS Plastic GmbH |
| ALTECH PBT+ASA A 2020/510 GF20 | (PBT+ASA)-GF20 | ALBIS Plastic GmbH |
| ALTECH PBT+ASA A 2030/500 GF30 | (PBT+ASA)-GF30 | ALBIS Plastic GmbH |
| Arnite® B434 SE | PBT-GF20 FR(17) | DSM Engineering Plastics |
| Arnite® B436 SE | PBT-GF30 FR(17) | DSM Engineering Plastics |
| Arnite® B437 SE/R | PBT-GF35 FR(17) | DSM Engineering Plastics |
| Arnite® B600 SNF | PBT FR | DSM Engineering Plastics |
| Arnite® B600SE | PBT FR | DSM Engineering Plastics |
| Arnite® B604T | PBT-I | DSM Engineering Plastics |
| Arnite® BM4 240 | (PBT+PET)-MD20 | DSM Engineering Plastics |
| Arnite® T04 200 | PBT | DSM Engineering Plastics |
| Arnite® T06 200 | PBT | DSM Engineering Plastics |
| Arnite® T06 200 (extrusion) | PBT | DSM Engineering Plastics |
| Arnite® T06 200 /D | PBT | DSM Engineering Plastics |
| Arnite® T06 202 | PBT | DSM Engineering Plastics |
| Arnite® T06 202 /A | PBT | DSM Engineering Plastics |
| Arnite® T06 202 XL | PBT | DSM Engineering Plastics |
| Arnite® T06 204 SN | PBT FR(17) | DSM Engineering Plastics |
| Arnite® T06 204 XL | PBT | DSM Engineering Plastics |
| Arnite® T08 200 | PBT | DSM Engineering Plastics |
| Arnite® T08 200 (extrusion) | PBT | DSM Engineering Plastics |
| Arnite® TB6 260 | PBT-GB30 | DSM Engineering Plastics |
| Arnite® TM4 440 | (PBT+PET)-MD20 | DSM Engineering Plastics |
| Arnite® TV4 220 | PBT-GF10 | DSM Engineering Plastics |
| Arnite® TV4 230 | PBT-GF15 | DSM Engineering Plastics |
| Arnite® TV4 230 S | PBT-GF15 FR(17) | DSM Engineering Plastics |
| Arnite® TV4 230 SF | PBT-GF15 FR(17) | DSM Engineering Plastics |
| Arnite® TV4 240 | PBT-GF20 | DSM Engineering Plastics |
| Arnite® TV4 240 S | PBT-GF20 FR(17) | DSM Engineering Plastics |
| Arnite® TV4 241 SL | PBT-GF20 FR(17) | DSM Engineering Plastics |
| Arnite® TV4 241 SN | PBT-GF20 FR(17) | DSM Engineering Plastics |
| Arnite® TV4 244 S | PBT-GF20 FR | DSM Engineering Plastics |
| Arnite® TV4 244 SX | PBT-GF20 FR(17) | DSM Engineering Plastics |
| Arnite® TV4 260 S | PBT-GF30 FR(17) | DSM Engineering Plastics |
| Arnite® TV4 260 SN | PBT-GF30 FR(17) | DSM Engineering Plastics |
| Arnite® TV4 260 SXF | PBT-GF30 FR(17) | DSM Engineering Plastics |
| Arnite® TV4 261 | PBT-GF30 | DSM Engineering Plastics |
| Arnite® TV4 261 KL | PBT-GF30 | DSM Engineering Plastics |
| Arnite® TV4 261 SF | PBT-GF30 FR(17) | DSM Engineering Plastics |
| Arnite® TV4 264 SN | PBT-GF30 FR(17) | DSM Engineering Plastics |
| Arnite® TV4 270 | PBT-GF35 | DSM Engineering Plastics |
| Arnite® TV4 290 | PBT-GF50 | DSM Engineering Plastics |
| Arnite® TV4 441 | (PBT+PET)-GF20 | DSM Engineering Plastics |
| Arnite® TV4 460 KL | (PBT+PET)-GF30 | DSM Engineering Plastics |
| Arnite® TV4 461 | (PBT+PET)-GF30 | DSM Engineering Plastics |
| Arnite® TV4 461 KL | (PBT+PET)-GF30 | DSM Engineering Plastics |
| Arnite® TV4 491 | (PBT+PET)-GF50 | DSM Engineering Plastics |
| Arnite® TV4 640 | (PBT+PC)-GF20 | DSM Engineering Plastics |
| Arnite® TV4 660 SN | (PBT+PC)-GF30 FR | DSM Engineering Plastics |
| Arnite® TV6 220 | PBT-GF10 | DSM Engineering Plastics |
| Arnite® TV6 240 | PBT-GF20 | DSM Engineering Plastics |
| Arnite® TV6 241 SN | PBT-GF20 FR(17) | DSM Engineering Plastics |
| Arnite® TV6 241 T | PBT-I-GF20 | DSM Engineering Plastics |
| Arnite® TV6 260 T | PBT-I-GF30 | DSM Engineering Plastics |
| Arnite® TV8 260 | PBT-GF30 | DSM Engineering Plastics |
| Arnite® TZ4 254 S | PBT-(GF+MD)25 FR(17) | DSM Engineering Plastics |
| Arnite® TZ6 280 | PBT-(GF+GB)40 | DSM Engineering Plastics |
| Arnite® TZ6 280 BLK ( NCP-4718/B ) | PBT-(GF+GB)40 | DSM Engineering Plastics |
| Arnite® XG 260 S (T-X07086) | PBT-GF30 FR | DSM Engineering Plastics |
| BERGADUR® PB40/50 | PBT | PolyOne Engineered Materials Europe |
| BERGADUR® PB400G/MI35UBK | PBT-(GF+MD)35 | PolyOne Engineered Materials Europe |
| BERGADUR® PB400G/MI45U | PBT-(GF+MD)45 | PolyOne Engineered Materials Europe |
| BERGADUR® PB400G30U | PBT-GF30 | PolyOne Engineered Materials Europe |
| BERGADUR® PB400G7,5UNATUR | PBT-GF7 | PolyOne Engineered Materials Europe |
| BERGADUR® PB40G/GK30 | PBT-(GF+GB)30 | PolyOne Engineered Materials Europe |
| BERGADUR® PB40G10 | PBT-GF10 | PolyOne Engineered Materials Europe |
| BERGADUR® PB40G20 | PBT-GF20 | PolyOne Engineered Materials Europe |
| BERGADUR® PB40G20U | PBT-GF20 | PolyOne Engineered Materials Europe |
| BERGADUR® PB40G30 | PBT-GF30 | PolyOne Engineered Materials Europe |
| BERGADUR® PB40G30TM-Z | PBT-GF30 | PolyOne Engineered Materials Europe |
| BERGADUR® PB40G30UM | PBT-GF20 | PolyOne Engineered Materials Europe |
| BERGADUR® PB40G40 | PBT-GF40 | PolyOne Engineered Materials Europe |
| BERGADUR® PB40GK30 | PBT-GB30 | PolyOne Engineered Materials Europe |
| BERGADUR® PB40GK30U | PBT-GB30 | PolyOne Engineered Materials Europe |
| BERGADUR® PB40TM-Y | PBT | PolyOne Engineered Materials Europe |
| BERGADUR® PB40TM-Z | PBT | PolyOne Engineered Materials Europe |
| BERGADUR® PB40UM | PBT | PolyOne Engineered Materials Europe |
| BERGADUR® PB450UA | PBT | PolyOne Engineered Materials Europe |
| BERGADUR® PB450UB | PBT | PolyOne Engineered Materials Europe |
| CELANEX 1400A | PBT | Ticona |
| CELANEX 1462Z | PBT-GF30 | Ticona |
| CELANEX 1600A | PBT | Ticona |
| CELANEX 1602Z | PBT | Ticona |
| CELANEX 1632Z | PBT-GF15 | Ticona |
| CELANEX 1642Z | PBT-GF20 | Ticona |
| CELANEX 1662Z | PBT-GF30 | Ticona |
| CELANEX 1700A | PBT | Ticona |
| CELANEX 2000-2 | PBT | Ticona |
| CELANEX 2000-3 | PBT | Ticona |
| CELANEX 2001 | PBT | Ticona |
| CELANEX 2002-2 | PBT | Ticona |
| CELANEX 2002-3 | PBT | Ticona |
| CELANEX 2002UV | PBT | Ticona |
| CELANEX 2003-2 | PBT | Ticona |
| CELANEX 2003-3 | PBT | Ticona |
| CELANEX 2003HR | PBT | Ticona |
| CELANEX 2004-2 | PBT | Ticona |
| CELANEX 2008 | PBT | Ticona |
| CELANEX 2016 | PBT | Ticona |
| CELANEX 2300 GV1/10 | PBT-GF10 | Ticona |
| CELANEX 2300 GV1/20 | PBT-GF20 | Ticona |
| CELANEX 2300 GV1/30 | PBT-GF30 | Ticona |
| CELANEX 2300 GV1/50 | PBT-GF50 | Ticona |
| CELANEX 2300 GV3/20 | PBT-GB20 | Ticona |
| CELANEX 2300 GV3/30 | PBT-GB30 | Ticona |
| CELANEX 2302 GV1/15 | PBT-GF15 | Ticona |
| CELANEX 2302 GV1/20 | PBT-GF20 | Ticona |
| CELANEX 2302 GV1/30 | PBT-GF30 | Ticona |
| CELANEX 2401 MT | PBT | Ticona |
| CELANEX 2402 MT | PBT | Ticona |
| CELANEX 2404 MT | PBT | Ticona |
| CELANEX 2500 | PBT | Ticona |
| CELANEX 3100-2 | PBT-GF7 | Ticona |
| CELANEX 3105H | PBT-GF15 | Ticona |
| CELANEX 3109HR | PBT-GF7 | Ticona |
| CELANEX 3116 | PBT-GF7 | Ticona |
| CELANEX 3200 | PBT-GF15 | Ticona |
| CELANEX 3200-2 | PBT-GF15 | Ticona |
| CELANEX 3200HR | PBT-GF15 | Ticona |
| CELANEX 3201 | PBT-GF15 | Ticona |
| CELANEX 3202-2 | PBT | Ticona |
| CELANEX 3209HR | PBT | Ticona |
| CELANEX 3209HRT | PBT-GF15 | Ticona |
| CELANEX 3216 | PBT-GF15 | Ticona |
| CELANEX 3225HRT | PBT-GF15 | Ticona |
| CELANEX 3226 | PBT | Ticona |
| CELANEX 3300 | PBT-GF30 | Ticona |
| CELANEX 3300-2 | PBT-GF30 | Ticona |
| CELANEX 3300-2LM | PBT | Ticona |
| CELANEX 3300D | PBT-GF30 | Ticona |
| CELANEX 3300HR | PBT-GF30 | Ticona |
| CELANEX 3300LM | PBT-GF30 | Ticona |
| CELANEX 3309HR | PBT-GF30 | Ticona |
| CELANEX 3309HRHF | PBT-GF30 | Ticona |
| CELANEX 3309HRLM | PBT-GF30 | Ticona |
| CELANEX 3309HRT | PBT-GF30 | Ticona |
| CELANEX 3316 | PBT-GF30 | Ticona |
| CELANEX 3316CT | PBT-(GF+MD)50 | Ticona |
| CELANEX 3318 | PBT-GF30 | Ticona |
| CELANEX 3325HRT | PBT-GF30 | Ticona |
| CELANEX 3400-2 | PBT-GF40 | Ticona |
| CELANEX 3409HR | PBT-GF40 | Ticona |
| CELANEX 3425HRT | PBT | Ticona |
| CELANEX 4016 | PBT | Ticona |
| CELANEX 4022 | PBT | Ticona |
| CELANEX 4202 | PBT-GF15 | Ticona |
| CELANEX 4300 | PBT-GF30 | Ticona |
| CELANEX 4300LM | PBT-GF30 | Ticona |
| CELANEX 4302 | PBT-GF30 | Ticona |
| CELANEX 4302HS | PBT-GF30 | Ticona |
| CELANEX 4302LM | PBT-GF30 | Ticona |
| CELANEX 4305 | PBT-GF33 | Ticona |
| CELANEX 4306 | PBT-GF30 | Ticona |
| CELANEX 5200-2 | PBT-GF15 | Ticona |
| CELANEX 5202 | PBT-GF15 | Ticona |
| CELANEX 5202HF | PBT-GF15 | Ticona |
| CELANEX 5205HG | PBT-GF15 | Ticona |
| CELANEX 5214HF | PBT-GF15 | Ticona |
| CELANEX 5300-2 | PBT-GF30 | Ticona |
| CELANEX 5300-2UV | PBT-GF30 | Ticona |
| CELANEX 531HS | PBT | Ticona |
| CELANEX 602AC | PBT | Ticona |
| CELANEX 6035GB20 | PBT-GB20 | Ticona |
| CELANEX 6400-2 | PBT | Ticona |
| CELANEX 6402R | PBT-(GF+MX)40 | Ticona |
| CELANEX 6406 | PBT-(GF+P)40 | Ticona |
| CELANEX 6407 | PBT-(GF+P)30 | Ticona |
| CELANEX 6407HR | PBT-(GF+P)30 | Ticona |
| CELANEX 6500 | PBT-(GF+P)30 | Ticona |
| CELANEX 6500HF | PBT | Ticona |
| CELANEX 6500HR | PBT | Ticona |
| CELANEX 6500LM | PBT-(GF+P)30 | Ticona |
| CELANEX 7316 | PBT-(GF+P)35 | Ticona |
| CELANEX 733LD | PBT | Ticona |
| CELANEX 7407 | PBT-GF40 | Ticona |
| CELANEX 7714 | PBT | Ticona |
| CELANEX 7716 | PBT-(GF+P)35 | Ticona |
| CELANEX D3200LC | PBT | Ticona |
| CELANEX J235 | PBT | Ticona |
| CELANEX J600 | PBT-(GF+P)40 | Ticona |
| CELANEX LW2333R | PBT-(GB+GF)50 | Ticona |
| CELANEX LW2547W | PBT-(GF+MX)30 | Ticona |
| CELANEX XFR 4840 | PBT | Ticona |
| CELANEX XFR 4840 10/0242 Black | PBT | Ticona |
| CELANEX XFR 6842 GF10 | PBT-GF30 | Ticona |
| CELANEX XFR 6842 GF15 | PBT-GF30 | Ticona |
| CELANEX XFR 6842 GF20 | PBT-GF30 | Ticona |
| CELANEX XFR 6842 GF30 | PBT-GF30 | Ticona |
| CELSTRAN PBT-CF40-08 | PBT-CF40 | Ticona |
| CELSTRAN PBT-GF30-08 | PBT-GF30 | Ticona |
| CELSTRAN PBT-GF40-08 | PBT-GF40 | Ticona |
| CELSTRAN PBT-GF50-08 | PBT-GF50 | Ticona |
| Crastin® 6129 NC010 | PBT | DuPont Engineering Polymers |
| Crastin® 6130 NC010 | PBT | DuPont Engineering Polymers |
| Crastin® 6131 NC010 | PBT | DuPont Engineering Polymers |
| Crastin® 6134 NC010 | PBT | DuPont Engineering Polymers |
| Crastin® BM6450XD BK560 | PBT | DuPont Engineering Polymers |
| Crastin® CE15315 NC010 | PBT-GF15 FR(17) | DuPont Engineering Polymers |
| Crastin® CE15330 NC010 | PBT-GF30 FR(17) | DuPont Engineering Polymers |
| Crastin® CE2055 NC010 | PBT | DuPont Engineering Polymers |
| Crastin® CE2255 BK580 | PBT | DuPont Engineering Polymers |
| Crastin® FG6129 NC010 | PBT | DuPont Engineering Polymers |
| Crastin® FG6130 NC010 | PBT | DuPont Engineering Polymers |
| Crastin® FGS600F40 NC010 | PBT | DuPont Engineering Polymers |
| Crastin® HR5315HF NC010 | PBT-I-GF15 | DuPont Engineering Polymers |
| Crastin® HR5330HF NC010 | PBT-I-GF30 | DuPont Engineering Polymers |
| Crastin® LW9020 NC010 | (PBT+ASA)-GF20 | DuPont Engineering Polymers |
| Crastin® LW9020FR NC010 | (PBT+ASA)-GF20 FR(17) | DuPont Engineering Polymers |
| Crastin® LW9030 NC010 | (PBT+ASA)-GF30 | DuPont Engineering Polymers |
| Crastin® LW9030FR NC010 | (PBT+ASA)-GF30 FR(17) | DuPont Engineering Polymers |
| Crastin® LW9320 NC010 | (PBT+SAN)-I-GF20 | DuPont Engineering Polymers |
| Crastin® LW9320LM BK591 | (PBT+SAN)-I-GF20 | DuPont Engineering Polymers |
| Crastin® LW9330 NC010 | (PBT+SAN)-I-GF30 | DuPont Engineering Polymers |
| Crastin® S600F10 NC010 | PBT | DuPont Engineering Polymers |
| Crastin® S600F20 NC010 | PBT | DuPont Engineering Polymers |
| Crastin® S600F40 NC010 | PBT | DuPont Engineering Polymers |
| Crastin® S610SF NC010 | PBT | DuPont Engineering Polymers |
| Crastin® S620F20 NC010 | PBT | DuPont Engineering Polymers |
| Crastin® S650FR NC010 | PBT FR(17) | DuPont Engineering Polymers |
| Crastin® SC164 NC010 | PBT | DuPont Engineering Polymers |
| Crastin® SC193 NC010 | (PBT+ASA)-GF30 | DuPont Engineering Polymers |
| Crastin® SK601 NC010 | PBT-GF10 | DuPont Engineering Polymers |
| Crastin® SK602 NC010 | PBT-GF15 | DuPont Engineering Polymers |
| Crastin® SK603 NC010 | PBT-GF20 | DuPont Engineering Polymers |
| Crastin® SK605 NC010 | PBT-GF30 | DuPont Engineering Polymers |
| Crastin® SK608 BK509 | PBT-GF45 | DuPont Engineering Polymers |
| Crastin® SK609 NC010 | PBT-GF50 | DuPont Engineering Polymers |
| Crastin® SK612SF NC010 | PBT-GF15 | DuPont Engineering Polymers |
| Crastin® SK615SF NC010 | PBT-GF30 | DuPont Engineering Polymers |
| Crastin® SK641FR NC010 | PBT-GF10 FR(17) | DuPont Engineering Polymers |
| Crastin® SK642FR NC010 | PBT-GF15 FR(17) | DuPont Engineering Polymers |
| Crastin® SK643FR NC010 | PBT-GF20 FR(17) | DuPont Engineering Polymers |
| Crastin® SK645FR NC010 | PBT-GF30 FR(17) | DuPont Engineering Polymers |
| Crastin® SO653 NC010 | PBT-GB20 | DuPont Engineering Polymers |
| Crastin® ST820 NC010 | PBT-I | DuPont Engineering Polymers |
| Crastin® ST830FRUV NC010 | PBT-I FR(17) | DuPont Engineering Polymers |
| Hytrel® DYM250S BK472 | (TPC+PBT)-CD | DuPont Engineering Polymers |
| Hytrel® DYM350BK | (TPC+PBT) | DuPont Engineering Polymers |
| Makroblend® KU2-7609 | (PC+PBT)-I-MD20 | Bayer MaterialScience |
| Makroblend® KU2-7912/4 | (PC+PBT)-I | Bayer MaterialScience |
| Makroblend® KU2-7915 | (PC+PBT)-I | Bayer MaterialScience |
| Makroblend® S7916 | (PBT+PC)-I | Bayer MaterialScience |
| Makroblend® UT1018 | (PC+PBT) | Bayer MaterialScience |
| Makroblend® UT3905 | (PC+PBT)-I | Bayer MaterialScience |
| Makroblend® UT3907 | (PC+PBT)-I | Bayer MaterialScience |
| Makroblend® UT4045 G | (PC+PBT)-GF20 | Bayer MaterialScience |
| Makroblend® UT408 | (PC+PBT) | Bayer MaterialScience |
| Makroblend® UT6005 | (PC+PBT)-I | Bayer MaterialScience |
| Makroblend® UT6007 | (PC+PBT)-I | Bayer MaterialScience |
| Pocan® A 3131 | (PBT+ASA)-GF30 | LANXESS Deutschland GmbH |
| Pocan® B 1100 | PBT | LANXESS Deutschland GmbH |
| Pocan® B 1300 | PBT | LANXESS Deutschland GmbH |
| Pocan® B 1305 | PBT | LANXESS Deutschland GmbH |
| Pocan® B 1501 | PBT | LANXESS Deutschland GmbH |
| Pocan® B 1505 | PBT | LANXESS Deutschland GmbH |
| Pocan® B 1505 Z | PBT | LANXESS Deutschland GmbH |
| Pocan® B 1600 | PBT | LANXESS Deutschland GmbH |
| Pocan® B 1700 | PBT | LANXESS Deutschland GmbH |
| Pocan® B 1701 | PBT | LANXESS Deutschland GmbH |
| Pocan® B 2505 | PBT FR | LANXESS Deutschland GmbH |
| Pocan® B 3215 | PBT-GF10 | LANXESS Deutschland GmbH |
| Pocan® B 3215 XF | PBT-I-GF10 | LANXESS Deutschland GmbH |
| Pocan® B 3215 Z | PBT-GF10 | LANXESS Deutschland GmbH |
| Pocan® B 3217 XF | PBT-I-GF16 | LANXESS Deutschland GmbH |
| Pocan® B 3225 | PBT-GF20 | LANXESS Deutschland GmbH |
| Pocan® B 3225 XF | PBT-GF20 | LANXESS Deutschland GmbH |
| Pocan® B 3225 Z | PBT-GF20 | LANXESS Deutschland GmbH |
| Pocan® B 3233 HR | PBT-GF30 | LANXESS Deutschland GmbH |
| Pocan® B 3235 | PBT-GF30 | LANXESS Deutschland GmbH |
| Pocan® B 3235 XF | PBT-GF30 | LANXESS Deutschland GmbH |
| Pocan® B 4215 | PBT-GF12 FR | LANXESS Deutschland GmbH |
| Pocan® B 4225 | PBT-GF20 FR | LANXESS Deutschland GmbH |
| Pocan® B 4235 | PBT-GF30 FR | LANXESS Deutschland GmbH |
| Pocan® B 4235 Z | PBT-GF30 FR | LANXESS Deutschland GmbH |
| Pocan® B 4239 | PBT-GF30 FR | LANXESS Deutschland GmbH |
| Pocan® B 5220 XF | PBT-I-GB20 | LANXESS Deutschland GmbH |
| Pocan® B 700 | PBT | LANXESS Deutschland GmbH |
| Pocan® B 7375 | PBT-X25 | LANXESS Deutschland GmbH |
| Pocan® B 7425 | PBT-GB20 | LANXESS Deutschland GmbH |
| Pocan® B 7616 | (PBT+PC)-GF15 | LANXESS Deutschland GmbH |
| Pocan® BF 4130 XF | PBT-GF30 FR | LANXESS Deutschland GmbH |
| Pocan® BF 4215 | PBT-GF12 FR | LANXESS Deutschland GmbH |
| Pocan® BF 4225 | PBT-GF20 FR | LANXESS Deutschland GmbH |
| Pocan® BF 4235 | PBT-GF30 FR | LANXESS Deutschland GmbH |
| Pocan® BF 4409 | PBT-GF7 FR | LANXESS Deutschland GmbH |
| Pocan® BF 8230 | PBT-(GF+GB)30 FR | LANXESS Deutschland GmbH |
| Pocan® C 1202 | (PBT+PC)-I | LANXESS Deutschland GmbH |
| Pocan® C 3230 XF | (PBT+PC)-GF30 | LANXESS Deutschland GmbH |
| Pocan® DP 1105 | PBT | LANXESS Deutschland GmbH |
| Pocan® DP 2004 | PBT FR | LANXESS Deutschland GmbH |
| Pocan® DP 4035 | (PBT+PET)-GF30 FR | LANXESS Deutschland GmbH |
| Pocan® DP 7102 | PBT-MD30 | LANXESS Deutschland GmbH |
| Pocan® DP 7244 | PBT-GF30 FR | LANXESS Deutschland GmbH |
| Pocan® DP BF 4232 | PBT-GF30 FR | LANXESS Deutschland GmbH |
| Pocan® DP C 1502 | (PBT+PC)-I | LANXESS Deutschland GmbH |
| Pocan® DP CF 2200 | (PBT+PC) FR | LANXESS Deutschland GmbH |
| Pocan® DP T7140 LDS | (PET+PBT)-(MD+GF)44 | LANXESS Deutschland GmbH |
| Pocan® ECO T 3220 | (PBT+PET)-GF20 | LANXESS Deutschland GmbH |
| Pocan® ECO T 3230 | (PBT+PET)-GF30 | LANXESS Deutschland GmbH |
| Pocan® ECO T 3240 | (PBT+PET)-GF45 | LANXESS Deutschland GmbH |
| Pocan® KL 1-7033 | PBT-GF30 | LANXESS Deutschland GmbH |
| Pocan® KL 1-7265 | PBT-GF15 | LANXESS Deutschland GmbH |
| Pocan® KU 1-7301 | PBT | LANXESS Deutschland GmbH |
| Pocan® KU 1-7313 | (PBT+PET)-GF15 | LANXESS Deutschland GmbH |
| Pocan® KU 1-7625 | (PBT+PC)-GF20 | LANXESS Deutschland GmbH |
| Pocan® KU 1-7635 | (PBT+PC)-GF30 | LANXESS Deutschland GmbH |
| Pocan® KU 1-7635 POS151 | (PBT+PC)-GF30 | LANXESS Deutschland GmbH |
| Pocan® KU 2-7003 | PBT | LANXESS Deutschland GmbH |
| Pocan® KU 2-7018 | PBT | LANXESS Deutschland GmbH |
| Pocan® KU 2-7205 | PBT FR | LANXESS Deutschland GmbH |
| Pocan® KU 2-7209 Z | PBT-GF15 FR | LANXESS Deutschland GmbH |
| Pocan® KU 2-7317 | PBT-I-Z17 | LANXESS Deutschland GmbH |
| Pocan® KU 2-7503/1 | PBT FR | LANXESS Deutschland GmbH |
| Pocan® KU 2-7604 | (PBT+PC) FR | LANXESS Deutschland GmbH |
| Pocan® S 1506 | PBT | LANXESS Deutschland GmbH |
| Pocan® S 1517 | PBT | LANXESS Deutschland GmbH |
| Pocan® S 7020 | PBT FR | LANXESS Deutschland GmbH |
| Pocan® S 7926 | PBT FR | LANXESS Deutschland GmbH |
| Pocan® T 3150 XF | (PBT+PET)-GF55 | LANXESS Deutschland GmbH |
| Pocan® T 7323 | (PBT+PET)-GF20 | LANXESS Deutschland GmbH |
| Pocan® T 7323 POS151 | (PBT+PET)-GF20 | LANXESS Deutschland GmbH |
| Pocan® T 7331 | (PBT+PET)-GF30 | LANXESS Deutschland GmbH |
| Pocan® T 7331 POS151 | (PBT+PET)-GF30 | LANXESS Deutschland GmbH |
| Pocan® T 7391 | (PBT+PET)-GF45 | LANXESS Deutschland GmbH |
| Pocan® T 7391 POS151 | (PBT+PET)-GF45 | LANXESS Deutschland GmbH |
| Pocan® TS 3220 | (PBT+PET)-I-GF20 | LANXESS Deutschland GmbH |
| RADIFLAM® B N100AE | PBT FR | RadiciPlastics |
| RADIFLAM® B RV250AE | PBT-GF25 FR | RadiciPlastics |
| RADITER® B N100 | PBT | RadiciPlastics |
| RADITER® B RV150 | PBT-GF15 | RadiciPlastics |
| RADITER® B RV200 | PBT-GF20 | RadiciPlastics |
| RADITER® B RV300 | PBT-GF30 | RadiciPlastics |
| RADITER® B RVA100 | (PBT+ASA)-GF10 | RadiciPlastics |
| RADITER® B RVA200 | (PBT+ASA)-GF20 | RadiciPlastics |
| RADITER® B RVA300 | (PBT+ASA)-GF30 | RadiciPlastics |
| SCHULABLEND® M/MX 50 | (PBT+PC)... | A. Schulman GmbH |
| SCHULADUR® A BS 40 HI | PBT-I-Z40 | A. Schulman GmbH |
| SCHULADUR® A GB 20 | PBT-GB20 | A. Schulman GmbH |
| SCHULADUR® A GB 30 SCHWARZ | PBT-GB30 | A. Schulman GmbH |
| SCHULADUR® A GF 10 | PBT-GF10 | A. Schulman GmbH |
| SCHULADUR® A GF 15 HF FR 1 | PBT-GF15 FR | A. Schulman GmbH |
| SCHULADUR® A GF 15 HI | PBT-I-GF15 | A. Schulman GmbH |
| SCHULADUR® A GF 20 | PBT-GF20 | A. Schulman GmbH |
| SCHULADUR® A GF 20 HF FR 1 | PBT-GF30 FR | A. Schulman GmbH |
| SCHULADUR® A GF 30 | PBT-GF30 | A. Schulman GmbH |
| SCHULADUR® A GF 30 HF FR 1 | PBT-GF30 FR | A. Schulman GmbH |
| SCHULADUR® A GF 30 HF2 FR1 | PBT-GF30 FR | A. Schulman GmbH |
| SCHULADUR® A GF 30 HI | PBT-I-GF30 | A. Schulman GmbH |
| SCHULADUR® A GF 30 HIR SCHWARZ | PBT-GF30 | A. Schulman GmbH |
| SCHULADUR® A GF 30 TOP SPEED | PBT-GF30 | A. Schulman GmbH |
| SCHULADUR® A MV 14 | PBT | A. Schulman GmbH |
| SCHULADUR® A MV 14 FR 1 | PBT FR | A. Schulman GmbH |
| SCHULADUR® A MV 14 SHI FR 1 | PBT-I FR | A. Schulman GmbH |
| SCHULADUR® A NV 12 | PBT | A. Schulman GmbH |
| SCHULADUR® A NV 12 SHI | PBT-I | A. Schulman GmbH |
| SCHULADUR® A1 GF 30 HF FR 1 | PBT-GF15 FR | A. Schulman GmbH |
| SCHULADUR® A1 GF 30 LW | (PBT+PET)-GF30... | A. Schulman GmbH |
| SCHULADUR® A1 GF 50 | (PBT+PET)-GF50 | A. Schulman GmbH |
| SCHULADUR® A3 GF 10 | (PBT+ASA)-GF10 | A. Schulman GmbH |
| SCHULADUR® A3 GF 20 | (ASA+PBT)-GF30... | A. Schulman GmbH |
| SCHULADUR® A3 GF 30 | (ASA+PBT)-GF30... | A. Schulman GmbH |
| SCHULADUR® A3 GF 30 FR 1 | (ASA+PBT)-GF30 FR... | A. Schulman GmbH |
| SCHULADUR® A3 GF 30 TS SCHWARZ | (PBT+ASA)-GF30 | A. Schulman GmbH |
| SCHULADUR® PCR GF 15 K1947 | (PBT+PET)-GF15 | A. Schulman GmbH |
| SCHULADUR® PCR GF 20 | (PBT+PET)-GF20... | A. Schulman GmbH |
| SCHULADUR® PCR GF 30 | (PBT+PET)-GF30... | A. Schulman GmbH |
| SCHULADUR® PCR GF 45 | (PBT+PET)-GF45... | A. Schulman GmbH |
| SCHULATEC® TinCo 50 | PBT-(MF(x)+Z)85 | A. Schulman GmbH |
| Ultradur® B 2550 | PBT | BASF |
| Ultradur® B 2550 FC | PBT | BASF |
| Ultradur® B 4040 G10 | (PBT+PET)-GF50 | BASF |
| Ultradur® B 4040 G4 | (PBT+PET)-GF20 | BASF |
| Ultradur® B 4040 G6 | (PBT+PET)-GF30 | BASF |
| Ultradur® B 4040 G6 High Speed | (PBT+PET)-GF30 | BASF |
| Ultradur® B 4300 G10 | PBT-GF50 | BASF |
| Ultradur® B 4300 G2 | PBT-GF10 | BASF |
| Ultradur® B 4300 G2 FC | PBT-GF10 | BASF |
| Ultradur® B 4300 G2 High Speed | PBT-GF10 | BASF |
| Ultradur® B 4300 G3 High Speed | PBT-GF15 | BASF |
| Ultradur® B 4300 G4 | PBT-GF20 | BASF |
| Ultradur® B 4300 G4 FC | PBT-GF20 | BASF |
| Ultradur® B 4300 G4 High Speed | PBT-GF20 | BASF |
| Ultradur® B 4300 G6 | PBT-GF30 | BASF |
| Ultradur® B 4300 G6 FC Aqua UN | PBT-GF30 | BASF |
| Ultradur® B 4300 G6 High Speed | PBT-GF30 | BASF |
| Ultradur® B 4300 G6 HR | PBT-GF30 | BASF |
| Ultradur® B 4300 GM42 | PBT-(GF+MF)30 | BASF |
| Ultradur® B 4300 K4 | PBT-GB20 | BASF |
| Ultradur® B 4300 K6 | PBT-GB30 | BASF |
| Ultradur® B 4300 M5 | PBT-MF25 | BASF |
| Ultradur® B 4330 G6 HR | PBT-I-GF30 | BASF |
| Ultradur® B 4406 | PBT FR | BASF |
| Ultradur® B 4406 G2 | PBT-GF10 FR | BASF |
| Ultradur® B 4406 G4 | PBT-GF20 FR | BASF |
| Ultradur® B 4406 G6 | PBT-GF30 FR | BASF |
| Ultradur® B 4500 | PBT | BASF |
| Ultradur® B 4500 FC | PBT | BASF |
| Ultradur® B 4520 | PBT | BASF |
| Ultradur® B 4520 High Speed | PBT | BASF |
| Ultradur® B 4520 PRO | PBT | BASF |
| Ultradur® B 4560 | PBT | BASF |
| Ultradur® B 6550 | PBT | BASF |
| Ultradur® B 6550 FC | PBT | BASF |
| Ultradur® B 6550 L | PBT | BASF |
| Ultradur® B 6550 LN | PBT | BASF |
| Ultradur® S 4090 G2 | (PBT+ASA)-GF10 | BASF |
| Ultradur® S 4090 G4 | (PBT+ASA)-GF20 | BASF |
| Ultradur® S 4090 G4 High Speed | (PBT+ASA)-GF20 | BASF |
| Ultradur® S 4090 G6 | (PBT+ASA)-GF30 | BASF |
| Ultradur® S 4090 G6X | (PBT+ASA)-GF30 | BASF |
| Ultradur® S 4090 G6X High Speed | (PBT+ASA)-GF30 | BASF |
| Ultradur® S 4090 GX | (PBT+ASA)-GF14 | BASF |
| Ultradur® S 4090 GX LS High Speed | (PBT+ASA)-GF14 | BASF |
| VANDAR 2100 | PBT | Ticona |
| VANDAR 2100UV | PBT | Ticona |
| VANDAR 2122 | PBT-P10 | Ticona |
| VANDAR 2500 | PBT | Ticona |
| VANDAR 4602Z | PBT | Ticona |
| VANDAR 4602ZHR | PBT | Ticona |
| VANDAR 4612R | PBT-GF7 | Ticona |
| VANDAR 4632Z | PBT-GF15 | Ticona |
| VANDAR 4662Z | PBT-GF30 | Ticona |
| VANDAR 6000 | PBT | Ticona |
| VANDAR 8000 | PBT | Ticona |
| VESTODUR® 1000 nc (nf) | PBT | Evonik Industries AG |
| VESTODUR® 1003 nc (nf) | PBT | Evonik Industries AG |
| VESTODUR® 1003-FR3 nc (nf) | PBT FR(17) | Evonik Industries AG |
| VESTODUR® 2000 nc (nf) | PBT | Evonik Industries AG |
| VESTODUR® 2002-FR3 nc (nf) | PBT FR(17) | Evonik Industries AG |
| VESTODUR® 2003 nc (nf) | PBT | Evonik Industries AG |
| VESTODUR® 3000 nc (nf) | PBT | Evonik Industries AG |
| VESTODUR® 3001 nc (nf) | PBT | Evonik Industries AG |
| VESTODUR® 3013 nc (nf) | PBT | Evonik Industries AG |
| VESTODUR® 3030 nc (nf) | PBT | Evonik Industries AG |
| VESTODUR® GF10 nc (nf) | PBT-GF10 | Evonik Industries AG |
| VESTODUR® GF12-FR3 nc (nf) | PBT-GF12 FR(17) | Evonik Industries AG |
| VESTODUR® GF20 nc (nf) | PBT-GF20 | Evonik Industries AG |
| VESTODUR® GF20-FR3 nc (nf) | PBT-GF20 FR(17) | Evonik Industries AG |
| VESTODUR® GF30 nc (nf) | PBT-GF30 | Evonik Industries AG |
| VESTODUR® GF30-FR3 nc (nf) | PBT-GF30 FR(17) | Evonik Industries AG |
| VESTODUR® GK20 nc (nf) | PBT-GB20 | Evonik Industries AG |
| VESTODUR® GK30 nc (nf) | PBT-GB20 | Evonik Industries AG |
| VESTODUR® HI19 nc (nf) | PBT-I | Evonik Industries AG |
| VESTODUR® HI19-S3 nc (nf) | PBT | Evonik Industries AG |
| VESTODUR® X4621 | PBT | Evonik Industries AG |
| VESTODUR® X4877 nc (nf) | PBT-I-GF30 | Evonik Industries AG |
| VESTODUR® X7061 nc (nf) | PBT | Evonik Industries AG |
| VESTODUR® X7062 | PBT | Evonik Industries AG |
| VESTODUR® X7065 nc (nf) | PBT | Evonik Industries AG |
| VESTODUR® X7085 nc (nf) | PBT-GF45 | Evonik Industries AG |
| VESTODUR® X7095 nc (nf) | PBT-GF | Evonik Industries AG |
| VESTODUR® X7190 nc (nf) | PBT | Evonik Industries AG |
| VESTODUR® X7212 nc (nf) | PBT-GF45 FR(17) | Evonik Industries AG |
| VESTODUR® X7329 nc (nf) | PBT-GF30 FR(17) | Evonik Industries AG |
| VESTODUR® X7390 nc (nf) | PBT | Evonik Industries AG |
| VESTODUR® X7396 nc (nf) | PBT | Evonik Industries AG |
| VESTODUR® X9400 nc (nf) | PBT-GF10 | Evonik Industries AG |
| VESTODUR® X9402 blk (sw) E70127 | PBT-GF30 | Evonik Industries AG |
| VESTODUR® X9403 nc (nf) | PBT FR(30) | Evonik Industries AG |
| VESTODUR® X9405 nc (nf) | PBT-GF30 FR(17) | Evonik Industries AG |
| VESTODUR® X9417 blk (sw) E70286 | PBT-GF15 | Evonik Industries AG |
| VESTODUR® X9419 nc (nf) | PBT | Evonik Industries AG |
| VESTODUR® X9420 | PBT | Evonik Industries AG |