View list of
  • All Ticona grades
  • All PBT grades
  • All grades beginning with C

CAMPUS® datasheet | CELANEX 4302LM


This datasheet of CELANEX 4302LM from Ticona is provided by the international plastics database CAMPUS.

You may contact the supplier for more information about this grade.

This datasheet includes:

  CELANEX 4302LM | PBT-GF30 | Ticona
제품 설명서
Celanex 4302 is a 30% glass reinforced PBT designed for improved mold
flow, warp resistance and surface appearance, that is also enhanced for
improved laser marking graphics.
기계적 특성단위시험규격
파단시 강도 120 MPa ISO 527-1/-2
파단시 신율 2.8 % ISO 527-1/-2
열적 특성단위시험규격
녹는점, 10°C/min 225 °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 173 °C ISO 75-1/-2
기타 특성단위시험규격
밀도 1490 kg/m³ ISO 1183
테스트 견본 생산단위시험규격
ISO에 따른 공정 조건 7790 - ISO ....-2
사출성형: 용융수지온도 260 °C ISO 294
사출성형: 금형온도 82 °C ISO 10724
사출성형: 사출속도 300 mm/s ISO 294
사출성형: 유지압력 48 MPa ISO 294
Disclaimer
NOTICE TO USERS: Values shown are based on testing
of laboratory test specimens and represent data that fall
within the standard range of properties for natural material.
These values alone do not represent a sufficient basis for
any part design and are not intended for use in
establishing maximum, minimum, or ranges of values for
specification purposes. Colorants or other additives may
cause significant variations in data values.

Properties of molded parts can be influenced by a wide
variety of factors including, but not limited to, material
selection, additives, part design, processing conditions and
environmental exposure. Any determination of the
suitability of a particular material and part design for any
use contemplated by the users and the manner of such
use is the sole responsibility of the users, who must assure
themselves that the material as subsequently processed
meets the needs of their particular product or use.

To the best of our knowledge, the information contained in
this publication is accurate; however, we do not assume
any liability whatsoever for the accuracy and completeness
of such information. The information contained in this
publication should not be construed as a promise or
guarantee of specific properties of our products. It is the
sole responsibility of the users to investigate whether any
existing patents are infringed by the use of the materials
mentioned in this publication.

Moreover, there is a need to reduce human exposure to
many materials to the lowest practical limits in view of
possible adverse effects. To the extent that any hazards
may have been mentioned in this publication, we neither
suggest nor guarantee that such hazards are the only ones
which exist. We recommend that persons intending to rely
on any recommendation or to use any equipment,
processing technique, or material mentioned in this
publication should satisfy themselves that they can meet
all applicable safety and health standards.

We strongly recommend that users seek and adhere to the
manufacturer's current instructions for handling each
material they use, and to entrust the handling of such
material to adequately trained personnel only. Please call
the telephone numbers listed for additional technical
information. Call Customer Services for the appropriate
Materials Safety Data Sheets (MSDS) before attempting to
process our products.

The products mentioned herein are not intended for use in
medical or dental implants.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012