View list of
- All RadiciPlastics grades
- All PA66 grades
- All grades beginning with R
CAMPUS® datasheet | RADILON® A RV250
This datasheet of RADILON® A RV250 from RadiciPlastics is provided by the international plastics database CAMPUS.
You may contact the supplier for more information about this grade.
RADILON® A RV250 | PA66-GF25 | RadiciPlastics
제품 설명서
DESIGNATION:
Thermoplastics ISO1874-PA66,MR,14-090,GF25
BRIEF DESCRIPTION:
PA66 25% Glass fibre reinforced injection moulding grade.
For items with medium stiffness.
Thermoplastics ISO1874-PA66,MR,14-090,GF25
BRIEF DESCRIPTION:
PA66 25% Glass fibre reinforced injection moulding grade.
For items with medium stiffness.
| 기계적 특성 | 건조/응축 | 단위 | 시험규격 |
| 인장탄성률 | 8300 / 6500 | MPa | ISO 527-1/-2 |
| 파단시 강도 | 160 / 110 | MPa | ISO 527-1/-2 |
| 파단시 신율 | 3.6 / 3.8 | % | ISO 527-1/-2 |
| 챠피 충격 강도 , +23°C | 61 / - | kJ/m² | ISO 179/1eU |
| 챠피 충격 강도, -30°C | 57 / - | kJ/m² | ISO 179/1eU |
| 챠피 노치드 충격 강도, +23°C | 12 / - | kJ/m² | ISO 179/1eA |
| 챠피 노치드 충격 강도, -30°C | 9.5 / - | kJ/m² | ISO 179/1eA |
| 열적 특성 | 건조/응축 | 단위 | 시험규격 |
| 녹는점, 10°C/min | 260 / * | °C | ISO 11357-1/-3 |
| 하중하에서의 변형온도, 1.80 MPa | 225 / * | °C | ISO 75-1/-2 |
| 하중하에서의 변형온도, 0.45 MPa | 250 / * | °C | ISO 75-1/-2 |
| 비카트 연화 온도, 50°C/h 50N | 245 / * | °C | ISO 306 |
| 1.5mm 평균두께에서의 난연성 | HB / * | class | IEC 60695-11-10 |
| 테스트 두께 | 1.6 / * | mm | IEC 60695-11-10 |
| UL 승인품의 난연성 | UL / * | - | - |
| 두께 H인 제품의 난연성 | HB / * | class | IEC 60695-11-10 |
| 테스트 두께 | 0.8 / * | mm | IEC 60695-11-10 |
| UL 승인품의 난연성 | UL / * | - | - |
| 물질의 비성질 | 건조/응축 | 단위 | 시험규격 |
| 점도수 | 145 / * | cm³/g | ISO 307, 1157, 1628 |
| 테스트 견본 생산 | 값 | 단위 | 시험규격 |
| ISO에 따른 공정 조건 | 1870 | - | ISO ....-2 |
| 사출성형: 용융수지온도 | 290 | °C | ISO 294 |
| 사출성형: 금형온도 | 80 | °C | ISO 10724 |
도표
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이)
부가물
윤활제
지역별 검색
Disclaimer
This database provides the technical properties of thermoplastics produced and marketed by RADICI NOVACIPS and his subsidiaries companies: RADILON® A Polyamide 66 RADILON® S Polyamide 6 RADILON® CA Copolyamide 66/6 RADILON® CS Copolyamide 6 semiaromatic RADITER® B Poly(butylene terephthalate) RADIFLAM® A Polyamide 66, self-extinguishing RADIFLAM® S Polyamide 6, self-extinguishing RADIFLAM® B Polybutylene terephthalate, self-extinguishing HERAFLEX® A Stirenic Thermoplastic Elastomer SEBS HERAFLEX® E Ether-Ester Thermoplastic Elastomer HERAFLEX® B Stirenic Thermoplastic Elastomer SBS HERAFLEX® P Modified Polypropylene RADILENE® R Polyethylene and Polypropylene The data and graphs contained in this database were carried out by our Research Centers and shall in no event be held to constitute or imply any warranty, undertaking, express or implied commitment from our part.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.