CAMPUS® datasheet | RITEFLEX 663


This datasheet of RITEFLEX 663 from Ticona is provided by the international plastics database CAMPUS.

You may contact the supplier for more information about this grade.

This datasheet includes:

  RITEFLEX 663 | TPC | Ticona
제품 설명서
Riteflex 663 is a nominal 63 Shore D thermoplastic polyester elastomer
with medium modulus.
기계적 특성단위시험규격
인장탄성률 360 MPa ISO 527-1/-2
항복강도 22 MPa ISO 527-1/-2
항복변형률 44 % ISO 527-1/-2
파단시 평균신율 >50 % ISO 527-1/-2
챠피 노치드 충격 강도, -30°C 22 kJ/m² ISO 179/1eA
열적 특성단위시험규격
녹는점, 10°C/min 210 °C ISO 11357-1/-3
하중하에서의 변형온도, 0.45 MPa 114 °C ISO 75-1/-2
선형 열팽창 계수, 평행 180 E-6/K ISO 11359-1/-2
두께 H인 제품의 난연성 HB class IEC 60695-11-10
테스트 두께 1.5 mm IEC 60695-11-10
전기적 특성단위시험규격
상대 유전뮬, 1MHz 4 - IEC 60250
소산 인자, 1MHz 400 E-4 IEC 60250
부피 저항 >1E13 Ohm*m IEC 60093
전기 압력 14 kV/mm IEC 60243-1
CTI 600 - IEC 60112
기타 특성단위시험규격
밀도 1240 kg/m³ ISO 1183
Disclaimer
NOTICE TO USERS: Values shown are based on testing
of laboratory test specimens and represent data that fall
within the standard range of properties for natural material.
These values alone do not represent a sufficient basis for
any part design and are not intended for use in
establishing maximum, minimum, or ranges of values for
specification purposes. Colorants or other additives may
cause significant variations in data values.

Properties of molded parts can be influenced by a wide
variety of factors including, but not limited to, material
selection, additives, part design, processing conditions and
environmental exposure. Any determination of the
suitability of a particular material and part design for any
use contemplated by the users and the manner of such
use is the sole responsibility of the users, who must assure
themselves that the material as subsequently processed
meets the needs of their particular product or use.

To the best of our knowledge, the information contained in
this publication is accurate; however, we do not assume
any liability whatsoever for the accuracy and completeness
of such information. The information contained in this
publication should not be construed as a promise or
guarantee of specific properties of our products. It is the
sole responsibility of the users to investigate whether any
existing patents are infringed by the use of the materials
mentioned in this publication.

Moreover, there is a need to reduce human exposure to
many materials to the lowest practical limits in view of
possible adverse effects. To the extent that any hazards
may have been mentioned in this publication, we neither
suggest nor guarantee that such hazards are the only ones
which exist. We recommend that persons intending to rely
on any recommendation or to use any equipment,
processing technique, or material mentioned in this
publication should satisfy themselves that they can meet
all applicable safety and health standards.

We strongly recommend that users seek and adhere to the
manufacturer's current instructions for handling each
material they use, and to entrust the handling of such
material to adequately trained personnel only. Please call
the telephone numbers listed for additional technical
information. Call Customer Services for the appropriate
Materials Safety Data Sheets (MSDS) before attempting to
process our products.

The products mentioned herein are not intended for use in
medical or dental implants.

The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012