View list of
CAMPUS® datasheet | Technyl® A 718 V30
This datasheet of Technyl® A 718 V30 from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.
Technyl® A 718 V30 | PA66-GF30 | Rhodia Polyamide Engineering Plastics
제품 설명서
is a polyamide 66 reinforced with glass fiber and thermal stabilized for injection moulding
Color: it is sailed on natural and black color
TECHNYL A 718 V30 features the following properties:
• Good mechanical properties
• Great superficial aspect
• Dimensional stability
• Excellent flow characteristics
This product is indicated for pieces with complex geometries, which need an excellent superficial aspect and good mechanical properties.
| 기계적 특성 | 건조/응축 | 단위 | 시험규격 |
| 인장탄성률 | 9000 / - | MPa | ISO 527-1/-2 |
| 파단시 강도 | 150 / - | MPa | ISO 527-1/-2 |
| 파단시 신율 | 2.5 / - | % | ISO 527-1/-2 |
| 챠피 충격 강도 , +23°C | 35 / * | kJ/m² | ISO 179/1eU |
| 열적 특성 | 건조/응축 | 단위 | 시험규격 |
| 녹는점, 10°C/min | 255 / * | °C | ISO 11357-1/-3 |
| 하중하에서의 변형온도, 1.80 MPa | 250 / * | °C | ISO 75-1/-2 |
Disclaimer
WARRANTY This information is supplied to assist you in your choice of the material best suited to your requirements and does not in any way constitute a product specification. The values given relate to unpigmented materials (natural colour). Pigmentation can alter results. The characteristics supplied are typical values. Our specialists are available to advise you on the values to be used in order to carry out calculations correctly on part dimensions. The information contained in this document is supplied in good faith. However it is given purely as an indication. It shall not be considered in any way as a formal commitment or warranty on our part, notably in respect of the eventual infringement of any rights of third parties who may use our products. We remain at your entire disposal to provide you with any information that you might require.
The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH.
M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors.
Any decision about the application of materials must be double checked with the producer of this material.