This datasheet of Technyl® C 246SI V11 from Rhodia Polyamide Engineering Plastics is provided by the international plastics database CAMPUS.

This datasheet includes:

  Technyl® C 246SI V11 | PA6-GF11 | Rhodia Polyamide Engineering Plastics
제품 설명서
 Polyamide 6, reinforced with 11 % of glass fibre, with high impact resistance, for injection moulding.

 

TECHNYL®C 246SI V11 has good mechanical properties and impact strength at low temperature.

 

This grade is widely used for 

 - Ski boot part

 

This product is available in natural color and colors in request.

열적 특성건조/응축단위시험규격
녹는점, 10°C/min 222 / * °C ISO 11357-1/-3
두께 H인 제품의 난연성 HB / * class IEC 60695-11-10
테스트 두께 3.2 / * mm IEC 60695-11-10
UL 승인품의 난연성 UL / * - -
기타 특성건조/응축단위시험규격
밀도 1170 / - kg/m³ ISO 1183
물질의 비성질건조/응축단위시험규격
점도수 205 / * cm³/g ISO 307, 1157, 1628
특징
생산 공정
사출 성형
지역별 검색
Disclaimer
WARRANTY

 This information is supplied to assist you in your choice of the
 material best suited to your requirements and does not in any way
 constitute a product specification.

 The values given relate to unpigmented materials (natural colour).
 Pigmentation can alter results. The characteristics supplied are
 typical values. Our specialists are available to advise you on the
 values to be used in order to carry out calculations correctly on
 part dimensions.

 The information contained in this document is supplied in good
 faith. However it is given purely as an indication. It shall not be
 considered in any way as a formal commitment or warranty on our part,
 notably in respect of the eventual infringement of any rights of
 third parties who may use our products. We remain at your entire
 disposal to provide you with any information that you might require.


The CAMPUS internet database is hosted by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

CAMPUS® is a registered trademark of CWFG mbH, Frankfurt am Main, 2012